The bearing capacity of a threaded pair made of spatially reinforced carbon-carbon composite materials (CCCM) with a 4DL reinforcement scheme in the temperature range from 20 to 2500 °C is experimentally determined. Recommendations are given for the design of CCCM threaded joints for operation at high temperatures.
Keywords: carbon-carbon composite material, threaded joint, limit load, bearing capacity, threaded pair, high temperature.