In this work, non-equiatomic W10Mo27Cr21Ti22Al20 refractory high-entropy alloy (RHEA) was produced using mechanical alloying followed by spark plasma sintering. The phase formation, microstructure, and compressive mechanical properties of the alloy were studied. During mechanical alloying, a Body-centered cubic (BCC) solid solution phase with a particle size of less than 1 µm was obtained after 18 h ball milling. The microstructure of the sintered sample exhibits three distinct phases consisting of two solid solution phases BCC1 and BCC2 as well as fine TiCxOy precipitates distributed in them. The volume fractions of each phase were about 79%, 8%, and 13%, respectively. The sintered W10Mo27Cr21Ti22Al20 showed yield strengths of 2465, 1506, 405, and 290 MPa at room temperature 600, 1000, and 1200°C, respectively, which are about twice that of the same refractory high-entropy alloy produced by vacuum arc melting. At 1000 and 1200°C, the strength after yielding gradually increased to 970 and 718 MPa at a compressive strain of 60%. The studied refractory high-entropy alloy can have good potential in high-temperature applications due to its high specific strength at elevated temperatures compared to conventional Ni-based superalloys and most as-reported refractory high-entropy alloys.

Entropy ◽  
2019 ◽  
Vol 21 (2) ◽  
pp. 122 ◽  
Author(s):  
Yuchen Sun ◽  
Boren Ke ◽  
Yulin Li ◽  
Kai Yang ◽  
Mingqi Yang ◽  
...  

In the study, an equiatomic CoCrNiCuZn high-entropy alloy (HEA) was prepared by mechanical alloying (MA) and the phases, microstructures, and thermal properties of the alloy powder were explored. The results suggest that a solid solution with body-centered cubic (BCC) phase and a crystalline size of 10 nm formed after 60 h of milling. Subsequently, the alloy powder was consolidated by spark plasma sintering (SPS) at different temperatures (600 °C, 700 °C, 800 °C, and 900 °C). Two kinds of face-centered cubic (FCC) phases co-existed in the as-sintered samples. Besides, Vickers hardness and compressive strength of the consolidated alloy sintered at 900 °C were respectively 615 HV and 2121 MPa, indicating excellent mechanical properties.


Sign in / Sign up

Export Citation Format

Share Document