The Microstructure Evolution of a Nickel-Base Single Crystal Superalloy after Long-Term Aging

2015 ◽  
Vol 1088 ◽  
pp. 217-220 ◽  
Author(s):  
Yu Xian Jia

Microstructure evolution of a nickel-base single crystal superalloy during thermal exposure at 982°C was investigated. The SEM studies revealed that the size of γ' phase increased and some of which linked together with the elongation of the exposure time. There is acicular phase precipitation after the long-term ageing treatment. The TCP phase is not increased by the increment of ageing time after reaching a certain amount. There are skeleton shape carbides precipitate after 100h and 300h. The amount of precipitated carbides decreases by the elongation of ageing time.

2011 ◽  
Vol 418-420 ◽  
pp. 265-269
Author(s):  
Yu Xian Jia ◽  
Tao Jin ◽  
Jin Lai Liu

Microstructure evolution of a nickel-base single crystal superalloy on the [001], [011] and [111] orientation during thermal exposure at 1000°C was investigated. The SEM studies revealed that the size of γ' phase increased and some of which linked together with the elongation of the exposure time. After 1100h the cubic γ' phase hardly is observed, and the rafting structure becomes perfect. With growing and linking of γ' phase the γ matrix channel is widening gradually, and the direction of γ' rafts is not along one define orientation. The TCP phase is not found in the three oriented samples during the thermal exposure.


2016 ◽  
Vol 849 ◽  
pp. 482-487 ◽  
Author(s):  
Xin Zhou ◽  
Jie Xiao ◽  
Yan Ling Pei ◽  
Shu Suo Li ◽  
Sheng Kai Gong

The coarsening behavior of γ' phase and precipitation behavior of TCP phase in a Ni3Al based single crystal superalloy were investigated by experimental and calculation. The Re-containing and Mo-rich single crystal superalloy used in this study exhibit good high-temperature strength and oxidation resistance. After fully heat-treated, the experimental superalloys were aged at 1050°C and 1150°C for different time periods from 50h to 1000h. The microstructure after thermal exposure was examined by field emission-scanning electron microscopy (FE-SEM). The results indicated that the coarsening behavior of γ' phase agrees well with the typical Lifshitz-Slyozov-Wagner (LSW) theory. After thermal exposure, both the size and the volume fraction of the TCP phase changed perceptibly.


China Foundry ◽  
2021 ◽  
Vol 18 (3) ◽  
pp. 185-191
Author(s):  
Xu-dong Wang ◽  
Zhong Yang ◽  
Qiang Gao ◽  
Li-rong Liu

2005 ◽  
Vol 69 (8) ◽  
pp. 743-746 ◽  
Author(s):  
Yutaka Koizumi ◽  
Hiroshi Harada ◽  
Toshiharu Kobayashi ◽  
Tadaharu Yokokawa

2011 ◽  
Vol 528 (6) ◽  
pp. 2620-2634 ◽  
Author(s):  
J.-B. le Graverend ◽  
J. Cormier ◽  
P. Caron ◽  
S. Kruch ◽  
F. Gallerneau ◽  
...  

2019 ◽  
Vol 33 (5) ◽  
pp. 731-740
Author(s):  
Zihao Tan ◽  
Lin Yang ◽  
Xinguang Wang ◽  
Yunling Du ◽  
Lihua Ye ◽  
...  