Multiphase Model for Predicting the Elimination of Inclusions inside a Liquid-Steel Ladle

2011 ◽  
Vol 13 (7) ◽  
pp. 538-542 ◽  
Author(s):  
Pascal Gardin ◽  
Ségolène Gauthier ◽  
Marie Simonnet ◽  
Jean Lehmann
Author(s):  
Adán Ramirez-Lopez ◽  
Omar Davila-Maldonado ◽  
Alfronso Nájera-Bastida ◽  
Rodolfo Morales ◽  
Jafeth Rodríguez-Ávila ◽  
...  

Steel is one of the essential materials in the world's civilization. It is essential to produce many products such as pipelines, mechanical elements in machines, vehicles, profiles, and beam sections for buildings in many industries. Until the '50s of the 20th century, steel products required a complex process known as ingot casting; for years, steelmakers focused on developing and simplifying this process. The result was the con-tinuous casting process (CCP); it is the most productive method to produce steel. The CCP allows producing significant volumes of steel sections without interruption and is more productive than the formal ingot casting process. The CCP begins by transferring the liquid steel from the steel-ladle to a tundish. This tundish or vessel distributes the liquid steel, by flowing through its volume, to one or more strands having wa-ter-cooled copper molds. The mold is the primary cooling system, PCS, solidifying a steel shell to withstand a liquid core and its friction forces with the mold wall. Further down the mold, the rolls drive the steel section in the SCS. Here the steel section is cooled, solidifying the remaining liquid core, by sprays placed in every cooling segment all around the billet and along the curved section of the machine. Finally, the steel strand goes towards a horizontal-straight free-spray zone, losing heat by radiation mechanism, where the billet cools down further to total solidification. A moving torch cutting-scissor splits the billet to the desired length at the end of this heat-radiant zone.


Author(s):  
M. K. Isaev ◽  
V. A. Bigeev ◽  
A. B. Sychkov ◽  
A. M/ Stolyarov

Metal processing in ladle by calcium-containing cored wires is one of the most spread methods of ladle treatment and modifying. Results of analysis of efficiency induces of existing cored wires application depending on their diameter, wall thickness and filling coefficient presented. It was shown that the basic efficiency index of a cored wire application – recovery coefficient – depending on wire quality (homogeneity of filling by calcium along the wire length), wire grade, conditions of its injection into liquid steel and other parameters can vary within a range from 50 to 95%. Reasons of unsatisfactory calcium recovery at usage of calcium-containing wires of 14–15 mm diameter with steel shell 0.4 mm thick and filling of mechanical mixture of steel shots and metallic calcium in various proportions was considered. Advantages of the modern calcium-containing cored wire with thicker wall were highlighted, including their higher wire rigidity and stability of its supply by a wire feeder into liquid steel. It was established that calcium content in a cored wire at the level of 100 g/m was the most effective composition. It was noted that increase of speed of cored wire feeding into steel will result in an increase of calcium recovery and in a decrease of probability of metal splashing out the steel ladle.


2011 ◽  
Vol 13 (7) ◽  
pp. 543-549 ◽  
Author(s):  
Ismael Lis Alves Daoud ◽  
Nicolas Rimbert ◽  
Alain Jardy ◽  
Benoît Oesterlé ◽  
Stéphane Hans ◽  
...  

2015 ◽  
Vol 60 (1) ◽  
pp. 257-262 ◽  
Author(s):  
M. Bielnicki ◽  
J. Jowsa ◽  
A. Cwudziński

AbstractThe paper reports the results of numerical simulation of the flow of liquid steel with the use of a multiphase model. The facility under study was a mould designed for continuous casting of steel slabs. The geometry of the facility, along with the computational grid, was generated within the program Ansys-MeshingR. Numerical computations were performed in the programs: COMSOL Multiphysics¯ and Ansys-Fluent¯. The use of the multiphase model enabled the determination of the behavior of the liquid slag layer on the metal bath surface. From the performed computer simulations, the fields of liquid steel motion and liquid steel turbulence kinetic energy distribution in the mould's symmetry plane have been presented. Based on the values recorded at selected measurement points located on the slag surface, a diagram illustrating the variation of the slag layer position during continuous steel casting has been plotted.