scholarly journals Orthodontic bonding to silicate ceramics: impact of different pretreatment methods on shear bond strength between ceramic restorations and ceramic brackets

Author(s):  
Rebecca Jungbauer ◽  
Christian Kirschneck ◽  
Christian M. Hammer ◽  
Peter Proff ◽  
Daniel Edelhoff ◽  
...  

Abstract Objective The study aims to investigate the shear bond strength (SBS) between silicate ceramic restorations and ceramic brackets after different pretreatments and aging methods. Material and methods Leucite (LEU) and lithium disilicate (LiSi) specimens were pretreated with (i) 4% hydrofluoric acid + silane (HF), (ii) Monobond Etch&Prime (MEP), (iii) silicatization + silane (CoJet), and (iv) SiC grinder + silane (SiC). Molars etched (phosphoric acid) and conditioned acted as comparison group. SBS was measured after 24 h (distilled water, 37 °C), 500 × thermocycling (5/55 °C), and 90 days (distilled water, 37 °C). Data was analyzed using Shapiro–Wilk, Kruskal–Wallis with Dunn’s post hoc test and Bonferroni correction, Mann–Whitney U, and Chi2 test (p < 0.05). The adhesive remnant index (ARI) was determined. Results LEU pretreated with MEP showed lower SBS than pretreated with HF, CoJet, or SiC. LiSi pretreated with MEP resulted in lower initial SBS than pretreated with HF or SiC. After thermocycling, pretreatment using MEP led to lower SBS than with CoJet. Within LiSi group, after 90 days, the pretreatment using SiC resulted in lowest SBS values. After HF and MEP pretreatment, LEU showed lower initial SBS than LiSi. After 90 days of water storage, within specimens pretreated using CoJet or SiC showed LEU higher SBS than LiSi. Enamel presented higher or comparable SBS values to LEU and LiSi. With exception of MEP pretreatment, ARI 3 was predominantly observed, regardless the substrate, pretreatment, and aging level. Conclusions MEP pretreatment presented the lowest SBS values, regardless the silicate ceramic and aging level. Further research is necessary. Clinical relevance There is no need for intraoral application of HF for orthodontic treatment.

2017 ◽  
Vol 15 (2) ◽  
pp. 176
Author(s):  
Patricia de Fátima Fraga ◽  
Ana Paula Terossi de Godoi ◽  
Ana Rosa Costa ◽  
Lourenço Correr-Sobrinho ◽  
Mario Vedovello Filho ◽  
...  

Aim: This in vitro study investigated the effect of the application of an adhesive, silane and thermal cycling (TC) on the shear bond strength (SBS) of ceramic brackets to feldspathic ceramic. Methods: 16 cylinders of feldspathic ceramic were etched with hydrofluoric acid and divided into four groups (n=4): G1 - silane, without TC; G2 – silane, with TC; G3 - adhesive, without TC; G4 - adhesive, with TC. One layer of silane was applied on the surface of cylinders in G1 and G2 e one layer of photo-activated adhesive Single Bond Universal was used in G3 and G4. Ceramic brackets were bonded using Transbond XT. The SBS data were subjected to two-way ANOVA and Tukey’s post hoc test (α=0.05). The Adhesive Remnant Index (ARI) was evaluated at 40× magnification. Results: Silane was more effective than adhesive on the SBS of the brackets to ceramic (p<0.05). TC decreased significantly the SBS values compared with the groups without TC (p<0.05). The ARI results showed predominance of score 0. Conclusions: Groups with silane showed higher SBS than groups with adhesive. TC influence significantly on the bond strength. Regarding ARI, score 0 predominated in all groups.


2016 ◽  
Vol 27 (6) ◽  
pp. 734-738 ◽  
Author(s):  
Natália Regina Santos de Matos ◽  
Ana Rosa Costa ◽  
Heloísa Cristina Valdrighi ◽  
Américo Bortolazzo Correr ◽  
Silvia Amélia Vedovello ◽  
...  

Abstract The aim of this study was to evaluate the effect of silanes, thermal cycling and acid etching on the shear bond strength (SBS) of metallic brackets to feldspathic ceramic. Feldspathic ceramic cylinders (Groups 1, 2, 5 and 6) were etched for 60 s with 10% hydrofluoric acid and Groups 3, 4, 7 and 8, without acid etching. Two layers of silane Clearfil Ceramic Primer (CCP, Groups 1 to 4) and two layers of RelyX Ceramic Primer (RCP, groups 5 to 8) were applied and dried for 60 s. Brackets were bonded to the cylinders with Transbond XT and light-activated for 40 s with Bluephase G2. All specimens were stored in deionized water at 37 °C for 24 h, and the specimens of groups 1, 3, 5 and 7 were submitted to 7,000 thermal cycles (5 °C/55 °C). After storage, the SBS test was performed at a crosshead speed of 1 mm/min. Data were subjected to three-way ANOVA and Tukey's post hoc test (α=0.05). The adhesive remnant index (ARI) was evaluated at 8x magnification. The SBS of CCP was significantly greater than of RCP (p<0.05), with or without thermal cycling. Thermal cycling significantly reduced the SBS (p<0.05). The groups submitted to acid etching showed significantly higher SBS than those without acid etching (p<0.05). In conclusion, thermal cycling reduced SBS for all groups. The best ceramic surface treatment for bracket bonding was achieved by acid etching and CCP silane. The ARI results showed predominance of score 0 for all groups.


2020 ◽  
Vol 25 (3) ◽  
pp. 31-38
Author(s):  
Gonzalo Andrés Garcés ◽  
Victor Hugo Rojas ◽  
Cristian Bravo ◽  
Camila S. Sampaio

ABSTRACT Introduction: Orthodontic treatment for adults is currently increasing, and therefore the need to bond brackets to restorations and temporary crowns. The use of CAD/CAM PMMA provisional restorations for orthodontic purposes have not yet been described, and there is currently insufficient information regarding the strength of bracket adhesion. Objective: This study aimed at evaluating the effects of thermocycling (TC) and surface treatment on shear bond strength (SBS) of brackets to different provisional materials. Methods: Forty specimens were made from each material [PMMA (Telio Lab), bis-acryl (Telio CS C&B), and PMMA CAD/CAM (Telio CAD)], sandpapered, and divided according to surface treatment (pumiced or sandblasted) and TC (half of the samples = 1,000 cycles, 5°C/55°C water baths) (n = 10/group). Stainless-steel brackets were bonded to the specimens (using Transbond XT), and SBS testing was performed. Data were analyzed by three-way ANOVA and LSD post-hoc tests (α = 0.05). Failure types were classified with adhesive remnant index (ARI) scores. Results: SBS values ranged from 1.5 to 14.9 MPa. Sandblasted bis-acryl and sandblasted auto-curing PMMA groups presented similar values (p> 0.05), higher than the CAD/CAM material (p< 0.05), with or without TC. When thermocycled, pumiced bis-acryl showed higher SBS than pumiced acrylic (p= 0.005) and CAD/CAM materials (p= 0.000), with statistical difference (p= 0.009). TC showed negative effect (p< 0.05) for sandblasted bis-acryl and pumiced acrylic groups. ARI predominant score was mostly zero (0) for CAD/CAM, 1 and 2 for bis-acryl, and 1 for acrylic groups. Conclusion: In general, bis-acryl material showed the highest SBS values, followed by acrylic and CAD/CAM materials, which showed SBS values lower than an optimum strength for bonding brackets.


2013 ◽  
Vol 18 (2) ◽  
pp. 76-80 ◽  
Author(s):  
Aisha de Souza Gomes Stumpf ◽  
Carlos Bergmann ◽  
José Renato Prietsch ◽  
Juliane Vicenzi

OBJECTIVE: To determine the shear bond strength of orthodontic brackets using color change adhesives that are supposed to aid in removing excess of bonding material and compare them to a traditional adhesive. METHODS: Ninety metallic and ninety ceramic brackets were bonded to bovine incisors using two color change adhesives and a regular one. A tensile stress was applied by a universal testing machine. The teeth were observed in a microscope after debonding in order to determine the Adhesive Remnant Index (ARI). RESULTS: The statistical analysis (ANOVA, Tukey, and Kruskall-Wallis tests) demonstrated that the mean bond strength presented no difference when metallic and ceramic brackets were compared but the bond resistance values were significantly different for the three adhesives used. The most common ARI outcome was the entire adhesive remaining on the enamel. CONCLUSIONS: The bond strength was similar for metallic and ceramic brackets when the same adhesive system was used. ARI scores demonstrated that bonding with these adhesives is safe even when ceramic brackets were used. On the other hand, bond strength was too low for orthodontic purposes when Ortho Lite Cure was used.


2014 ◽  
Vol 2014 ◽  
pp. 1-5 ◽  
Author(s):  
Ahmad Sheibaninia ◽  
Sepehr Sepasi ◽  
Mohammad Ali Saghiri ◽  
Setareh Sepasi

Aim.This study aims to evaluate the effect of acidic food simulant and (acetic acid 3%) on the shear bond strength (SBS) and adhesive remnant index (ARI) scores of one conventional and three different self-ligating brackets with different base designs.Materials and Methods.Freshly extracted first maxillary premolars(n=160)were embedded in resin blocks. A conventional stainless steel bracket, Equilibrium 2, and three types of self-ligating brackets, Speed, In-Ovation R, and Damon 3MX, were bonded to teeth and exposed to distilled water (groups 1, 3, 5, and 7) or acetic acid 3% (groups 2, 4, 6, 8) for 12 weeks. SBS and ARI were calculated and statistical analysis was performed with the analysis of variance (SBS) orχ2test (ARI) to compare values between the different groups.Results.Equilibrium 2 and In-Ovation R showed a significantly lower SBS in the acidic environment than in distilled water. Significant differences in ARI scores were found for Equilibrium 2 after immersion in an acidic environment, shifting from 0 in distilled water to 2 in an acidic environment.Conclusions.Equilibrium 2 and In-Ovation R brackets showed a significant decrease in SBS after a 12-week immersion in acetic acid 3%, although all groups showed clinically acceptable SBS. Equilibrium 2 showed significant differences in ARI scores when exposed to acetic acid 3%.


2012 ◽  
Vol 2012 ◽  
pp. 1-5 ◽  
Author(s):  
Isabell Immerz ◽  
Peter Proff ◽  
Piero Roemer ◽  
Claudia Reicheneder ◽  
Andreas Faltermeier

The aim of the study was to investigate the effect of bleaching on the colouration of tooth enamel and shear bond strength of orthodontic ceramic brackets based upon current whitening practice. The bleaching and bonding techniques were performed on extracted bovine teeth for the investigation of their colorimetric spectrum and the adhesive bond strength on surface enamel. One group was designated as the control group with no pre-treatment. Another group was treated with a 45% hydrogen peroxide solution prior to bonding. The difference in colour was expressed as the Euclidian distance ΔE. The resulting shear bond strength was analyzed and evaluated by scores of Adhesion Remnant Index. Statistical analysis was performed using the Kruskall-Wallis and post-hoc test. The colorimetric analysis revealed statistically significant differences between original and bleached as well as bleached and debonded teeth setting off a blue colour shift. Furthermore, statistically there was no significant difference noted in bonding strength between non-treated surfaces and those treated with peroxide. It can be concluded that peroxide pre-treatment does result in colour differences of teeth. Bonding and debonding procedures seem to have no statistically significant influence on the enamel colour using current materials.


2012 ◽  
Vol 83 (1) ◽  
pp. 152-157 ◽  
Author(s):  
Erika L. Silva-Benítez ◽  
Veronica Zavala-Alonso ◽  
Gabriel A. Martinez-Castanon ◽  
Juan P. Loyola-Rodriguez ◽  
Nuria Patiño-Marin ◽  
...  

Abstract Objective: To study the shear bond strength (SBS), sites of failure, and micromorphology of bonded molar tubes used on teeth affected by dental fluorosis. Materials and Methods: This in vitro study included 140 first molars classified according to Dean's index for dental fluorosis. Samples were divided into seven groups: (1) healthy teeth etched for 15 seconds, (2) teeth with moderate fluorosis (MOF) etched for 15 seconds, (3) teeth with MOF etched for 150 seconds, (4) teeth with MOF microabrasion etched for 15 seconds, (5) teeth with severe fluorosis (SEF) etched for 15 seconds, (6) teeth with SEF etched for 150 seconds, and (7) teeth with SEF microabrasion etched for 15 seconds. All samples were incubated and were then submitted to the SBS test and evaluated with the modified adhesive remnant index (ARI) and analyzed by using a scanning electronic microscope. Results: The SBS mean value for healthy enamel was 20 ± 10.2 MPa. For the group with MOF, the etched 150-second mean value was the highest (19 ± 7.6 MPa); for the group with SEF treated with microabrasion and etched for 15 seconds, the mean value was (13 ± 4.1 MPa). Significant differences (P ≤ .05) were found in the ARI between healthy and fluorosed groups. Conclusions: Fluorotic enamel affects the adhesion of bonded molar tubes. The use of overetching in cases of MOF and the combination of microabrasion and etching in SEF provides a suitable adhesion for fixed appliance therapy.


2014 ◽  
Vol 2014 ◽  
pp. 1-7 ◽  
Author(s):  
Ahmed Mohammed Hassan ◽  
Ahmed Ali Goda ◽  
Kusai Baroudi

Objective. The aim of this study was to evaluate the effect of different disinfectant agents on bond strength of two types of resin composite materials.Methods. A total of 80 sound posterior teeth were used. They were divided into four groups(n=20)according to the dentin surface pretreatment (no treatment, chlorhexidine gluconate 2%, sodium hypochlorite 4%, and EDTA 19%). Each group was divided into two subgroups according to the type of adhesive (prime and bond 2.1 and Adper easy one). Each subgroup was further divided into two subgroups according to the type of resin composite (TPH spectrum and Tetric EvoCeram). Shear bond strength between dentin and resin composite was measured using Universal Testing Machine. Data collected were statistically analyzed byt-test and one-way ANOVA followed by Tukey’spost hoctest.Results. It was found that dentin treated with EDTA recorded the highest shear bond strength values followed by sodium hypochlorite and then chlorhexidine groups while the control group showed the lowest shear bond strength.Conclusions. The surface treatment of dentin before bonding application has a great effect on shear bond strength between resin composite and dentin surface.


Sign in / Sign up

Export Citation Format

Share Document