Research on the Microstructure Characteristic and Tensile Property of Laser-MIG Hybrid Welded Joint for 5A06 Aluminum Alloy

2019 ◽  
Vol 26 (3) ◽  
pp. 346-359 ◽  
Author(s):  
Yanqiu Zhao ◽  
Xiaohong Zhan ◽  
Qiyu Gao ◽  
Shuai Chen ◽  
Yue Kang
2012 ◽  
Vol 724 ◽  
pp. 182-185 ◽  
Author(s):  
Shan Gao ◽  
Zhi Sheng Wu ◽  
Peng Fei Jin ◽  
Jun Jie Wang ◽  
Peng Shuai

5A06 aluminum alloy welding was obtained by using SAlMg-3 as welding wire with MIG (metal inert gas arc welding). The welded joint with deep cryogenic treatment at liquid nitrogen temperature (-155) for 4h, 8h, 10h were analyzed by metallographic and XRD examination. The results have shown that a lot of subgrain appears in the microstructure of the welded joint resulting in the refined grain after cryogenic treatment. The obvious increasing in content of β-phase (Mg2Al3) is distributed and dispersed evenly, contributed to dispersion strengthening of the welded joint. Meanwhile, orientation phenomena is obtained for some grain after deep cryogenic treatment. As a result, the microstructure of the joint can be modified by the deep cryogenic treatment.


2011 ◽  
Vol 314-316 ◽  
pp. 927-931 ◽  
Author(s):  
Shan Gao ◽  
Zhi Sheng Wu ◽  
Peng Fei Jin ◽  
Jun Jie Wang

In this paper, some deep cryogenic treatment experiments are first applied to 5A06 aluminum alloy welded joint at liquid nitrogen temperature (-155°C )for 4h, 8h, 10h respectively. 5A06 alloy welded joints before and after deep cryogenic treatment are observed by X-ray diffraction and scanning electrical microscopy. The experimental results have shown that the deep cryogenic treatment causesβphase of alloy to disperse and makes the grain smaller than that of joint before deep cryogenic treatment. Therefore, the mechanical properties of 5A06 alloy welded joints after deep cryogenic treatment are greatly improved.


2020 ◽  
Vol 2020 (12) ◽  
pp. 13-17
Author(s):  
Nikolay Proskuryakov ◽  
Uliana Putilova ◽  
Rasul Mamadaliev ◽  
Oleg Teploukhov

The comparative investigation results of AD33 aluminum alloy welded joint quality dependence upon changes in a laser beam motion rate for conditions of hand and automatic laser welding are shown. A micro-structure of a welded joint at the hand and automatic laser welding of the AD33 alloy is investigated.


2010 ◽  
Vol 146-147 ◽  
pp. 1402-1405 ◽  
Author(s):  
Che Lah Nur Azida ◽  
Azman Jalar ◽  
Norinsan Kamil Othman ◽  
Nasrizal Mohd Rashdi ◽  
Md Zaukah Ibel

AA6061 Aluminum alloy welded joint using two different filler metals were studied by using X-ray CT-Scan. The filler metals ER 4043 and ER 5356 were used in this present work in order to investigate the effect of using different filler metals on the welded joint quality of AA 6061 aluminum alloy in welded zone microstructure. Gas metal arc welding (GMAW) technique and V grove butt joint with four layers and five passes welded joint were performed. From this investigation, it is found that AA6061 with ER 4043 showed less distribution of porosity compared to AA6061 with ER 5356 welded joint confirmed by X-ray Ct-Scan. The decreasing of porosities and presence of very fine grains in weld region area with ER 5356 compared to ER 4043 will be discussed in term of microstructure analysis.


1996 ◽  
Vol 46 (10) ◽  
pp. 500-504 ◽  
Author(s):  
Hiizu OCHI ◽  
Koichi OGAWA ◽  
Yoshiaki YAMAMOTO ◽  
Shigeki HASHINAGA ◽  
Yasuo SUGA ◽  
...  