Improvements in morphology, mechanical and thermal properties of films produced by reactive blending of poly(lactic acid)/natural rubber latex with dicumyl peroxide

2017 ◽  
Vol 26 (8) ◽  
pp. 615-628 ◽  
Author(s):  
Chutimar Deetuam ◽  
Chavakorn Samthong ◽  
Parichat Pratumpol ◽  
Anongnat Somwangthanaroj
2011 ◽  
Vol 410 ◽  
pp. 59-62 ◽  
Author(s):  
Punmanee Juntuek ◽  
Chaiwat Ruksakulpiwat ◽  
Pranee Chumsamrong ◽  
Yupaporn Ruksakulpiwat

From our previous study, natural rubber (NR) was used to improve toughness of poly (lactic acid) (PLA). Impact strength and elongation at break of PLA was increased when adding NR. Moreover, by using NR-g-GMA as compatibilizer for PLA and NR blend, impact strength and elongation at break was improved. However, tensile strength and modulus of PLA/NR blend with and without NR-g-GMA were decreased. In this study, calcium carbonate (CaCO3) and vetiver grass fiber were used as fillers in PLA/NR blend. With the addition of CaCO3 into PLA/NR blend with NR-g-GMA, impact strength and modulus of the composite were further increased with a loss in tensile strength. In contrast, the addition of vetiver grass fiber into PLA/NR blend with NR-g-GMA led to an increase in tensile strength and modulus and a decrease in impact strength and elongation at break. The onset degradation temperatures of PLA composites were lower than that of PLA and PLA/NR blend.


Author(s):  
Li Zhang ◽  
Lusheng Liao ◽  
Jing Chen ◽  
Lin Ma ◽  
Fuquan Zhang ◽  
...  

2015 ◽  
Vol 1125 ◽  
pp. 222-226 ◽  
Author(s):  
Mohd Shaiful Zaidi Mat Desa ◽  
Azman Hassan ◽  
Agus Arsad ◽  
Nor Nisa Balqis Mohammad

The effect of rubber toughening on mechanical and thermal properties of poly (lactic acid) (PLA) was investigated by using three types of rubbers; natural rubber (NR), epoxidized natural rubber (ENR) and core-shell rubber (CSR). The PLA/rubber blends were prepared by melt blending in a counter-rotating twin-screw extruder, where the rubber content for all blends was kept at 5 wt%. It was found that the addition of the rubbers increased the impact strength for all blends as compared to pure PLA. On the other hand, all PLA/rubber blends showed notable decrease of Young’s modulus especially for PLA/NR blend which decreased by 72% than pure PLA. Similarly, significant decrease of tensile strength was also observed for all PLA/rubber blends. PLA/ENR blend showed a morebalance mechanical properties with fairly significant improvement of impact strength and moderate decrease of tensile strength, Young’s modulus and elongation at break. In general, PLA/NR blend showed the highest overall impact strength, while the PLA/CSR showed the highest tensile strength and Young’s modulus among the blends. Thermal analysis revealed that the Tg of PLA decreased with incorporation of the three types of rubbers with NR showing the largest decrease. This study indicates that NR, ENR and CSR are effective in enhancing toughness of PLA


Polymers ◽  
2021 ◽  
Vol 13 (15) ◽  
pp. 2429
Author(s):  
Krittameth Kiatiporntipthak ◽  
Nanthicha Thajai ◽  
Thidarat Kanthiya ◽  
Pornchai Rachtanapun ◽  
Noppol Leksawasdi ◽  
...  

Polylactic acid (PLA) was melt-blended with epoxy resin to study the effects of the reaction on the mechanical and thermal properties of the PLA. The addition of 0.5% (wt/wt) epoxy to PLA increased the maximum tensile strength of PLA (57.5 MPa) to 67 MPa, whereas the 20% epoxy improved the elongation at break to 12%, due to crosslinking caused by the epoxy reaction. The morphology of the PLA/epoxy blends showed epoxy nanoparticle dispersion in the PLA matrix that presented a smooth fracture surface with a high epoxy content. The glass transition temperature of PLA decreased with an increasing epoxy content owing to the partial miscibility between PLA and the epoxy resin. The Vicat softening temperature of the PLA was 59 °C and increased to 64.6 °C for 0.5% epoxy. NMR confirmed the reaction between the -COOH groups of PLA and the epoxy groups of the epoxy resin. This reaction, and partial miscibility of the PLA/epoxy blend, improved the interfacial crosslinking, morphology, thermal properties, and mechanical properties of the blends.


2021 ◽  
Vol 904 ◽  
pp. 441-446
Author(s):  
Nuchnapa Tangboriboon ◽  
Sarun Muntongkaw ◽  
Sompratthana Pianklang

Adding 0, 20, and 50 wt% natural-rubber latex compound into the plaster ceiling matrix affected to increase the physical-mechanical-thermal performance properties of plaster ceiling composites. Adding 50 wt% natural rubber latex compound into plaster composites can increase the superior adhesion of the nail-tensile resistance equal to 57.54 N and decrease thermal conductivity equal to 0.0634 W/m.K. In addition, adding natural rubber latex compounds into plaster composites can reduce water solubility, brittleness, impact, and cost of energy consumption due to the exterior temperature. Adequate thermal insulation for roofing, ceiling, and wall systems also reduces radiative losses that chill occupants in cold weather, and reduce interior surface temperatures in the summer, thereby optimizing the comfort of building occupants. The mechanical and thermal properties of plaster composites were investigated by using a Universal Testing Machine (UTM) and heat flow meter, respectively, measured according to TIS 1211-50, TIS 219-2522, and ASTM C518.