Analysis of hydrogen diffusion coefficient during hydrogen permeation through niobium and its alloys

2009 ◽  
Vol 476 (1-2) ◽  
pp. 102-106 ◽  
Author(s):  
H. Yukawa ◽  
G.X. Zhang ◽  
N. Watanabe ◽  
M. Morinaga ◽  
T. Nambu ◽  
...  
2009 ◽  
Vol 283-286 ◽  
pp. 225-230 ◽  
Author(s):  
Hiroshi Yukawa ◽  
G.X. Zhang ◽  
N. Watanabe ◽  
Masahiko Morinaga ◽  
T. Nambu ◽  
...  

The hydrogen diffusion coefficients are investigated during the hydrogen permeation through Nb-based hydrogen permeable membranes at high temperature. It is found that the hydrogen diffusion coefficient for pure niobium under practical conditions is much lower than the reported values measured for dilute hydrogen solid solutions. Surprisingly, the hydrogen diffusion is found to be faster in Pd-Ag alloy with fcc crystal structure than in pure niobium with bcc crystal structure at 773K during the hydrogen permeation. It is also found that the addition of Ru or W into niobium increases the hydrogen diffusion coefficient under the practical conditions.


Hydrogen ◽  
2021 ◽  
Vol 2 (4) ◽  
pp. 414-427
Author(s):  
Atif Imdad ◽  
Alfredo Zafra ◽  
Victor Arniella ◽  
Javier Belzunce

It is well known that the presence of hydrogen decreases the mechanical properties of ferritic steels, giving rise to the phenomenon known as hydrogen embrittlement (HE). The sensitivity to HE increases with the strength of the steel due to the increase of its microstructural defects (hydrogen traps), which eventually increase hydrogen solubility and decrease hydrogen diffusivity in the steel. The aim of this work is to study hydrogen diffusivity in a 42CrMo4 steel submitted to different heat treatments—annealing, normalizing and quench and tempering—to obtain different microstructures, with a broad range of hardness levels. Electrochemical hydrogen permeation tests were performed in a modified Devanathan and Stachursky double-cell. The build-up transient methodology allowed the determination of the apparent hydrogen diffusion coefficient, Dapp, and assessment of its evolution during the progressive filling of the microstructural hydrogen traps. Consequently, the lattice hydrogen diffusion coefficient, DL, was determined. Optical and scanning electron microscopy (SEM) were employed to examine the steel microstructures in order to understand their interaction with hydrogen atoms. In general, the results show that the permeation parameters are strongly related to the steel hardness, being less affected by the type of microstructure.


2010 ◽  
Vol 297-301 ◽  
pp. 1091-1096 ◽  
Author(s):  
Hiroshi Yukawa ◽  
G.X. Zhang ◽  
Masahiko Morinaga ◽  
T. Nambu ◽  
Yoshihisa Matsumoto

The hydrogen solubility and the hydrogen permeability have been measured for Nb-based alloys in order to investigate the alloying effects on the hydrogen diffusivity during hydrogen permeation. The hydrogen diffusion coefficient during hydrogen permeation is estimated from a linear relationship between the normalized hydrogen flux, , and the difference of hydrogen concentration, C, between the inlet and the outlet sides of the membrane. It is found that the hydrogen diffusion coefficient during the hydrogen permeation is increased by alloying ruthenium or tungsten into niobium. On the other hand, the activation energy for hydrogen diffusion in pure niobium under the practical permeation condition is much higher than the reported values measured for dilute hydrogen solid solutions. It is interesting that the activation energy for hydrogen diffusion decreases by the addition of ruthenium or tungsten into niobium.


2008 ◽  
Vol 33 (16) ◽  
pp. 4419-4423 ◽  
Author(s):  
G ZHANG ◽  
H YUKAWA ◽  
N WATANABE ◽  
Y SAITO ◽  
H FUKAYA ◽  
...  

2010 ◽  
Vol 638-642 ◽  
pp. 1131-1136
Author(s):  
Wei Liang Wang ◽  
Kazuhiro Ishikawa ◽  
Kiyoshi Aoki

In general, hydrogen permeabilityΦ of the alloy membrane is expressed as the product of the hydrogen diffusion coefficient D and the hydrogen solution coefficient K. Therefore, to improve the hydrogen permeability efficiently, the values of K and D should be separately considered. In the present study, hydrogen absorption and permeation behaviors of the Nb19Ti40Ni41 alloy consisting of the eutectic phase are investigated by measuring pressure-composition-isotherm (PCI) and by the hydrogen flow method and compared with those of palladium. The hydrogen absorption in the Nb19Ti40Ni41 alloy does not obey the Sieverts’ law in the pressure region of 0-1.0MPa at 523K, but it shows linear relationship between the difference in the square root of hydrogen pressure and hydrogen content between 0.1 and 0.4MPa. Although the value of D for the Nb19Ti40Ni41 alloy is considerably lower than that of palladium, its high K value enhances the hydrogen permeability Φ. It is suggested that the enhancement of D by microstructural control for Nb19Ti40Ni41 alloy is effective for improvement of Φ.


2021 ◽  
Vol ahead-of-print (ahead-of-print) ◽  
Author(s):  
Xiang Qiu ◽  
Kun Zhang ◽  
Qin Kang ◽  
Yicheng Fan ◽  
Hongyu San ◽  
...  

Purpose This paper aims to study the mechanism of hydrogen embrittlement in 12Cr2Mo1R(H) steel, which will help to provide valuable information for the subsequent hydrogen embrittlement research of this kind of steel, so as to optimize the processing technology and take more appropriate measures to prevent hydrogen damage. Design/methodology/approach The hydrogen diffusion coefficient of 12Cr2Mo1R(H) steel was measured by the hydrogen permeation technique of double electrolytic cells. Moreover, the influence of hydrogen traps in the material and experimental temperature on hydrogen diffusion behavior was discussed. The first-principles calculations based on density functional theory were used to study the occupancy of H atoms in the bcc-Fe cell, the diffusion path and the interaction with vacancy defects. Findings The results revealed that the logarithm of the hydrogen diffusion coefficient of the material has a linear relationship with the reciprocal of temperature and the activation energy of hydrogen atom diffusion in 12Cr2Mo1R(H) steel is 23.47 kJ/mol. H atoms stably exist in the nearly octahedral interstices in the crystal cell with vacancies. In addition, the solution of Cr/Mo alloy atom does not change the lowest energy path of H atom, but increases the diffusion activation energy of hydrogen atom, thus hindering the diffusion of hydrogen atom. Cr/Mo and vacancy have a synergistic effect on inhibiting the diffusion of H atoms in α-Fe. Originality/value This article combines experiments with first-principles calculations to explore the diffusion behavior of hydrogen in 12Cr2Mo1R(H) steel from the macroscopic and microscopic perspectives, which will help to establish a calculation model with complex defects in the future.