Effects of annealing process on magnetic properties and structures of Nd–Pr–Ce–Fe–B melt-spun powders

2016 ◽  
Vol 406 ◽  
pp. 239-243 ◽  
Author(s):  
Kun Pei ◽  
Min Lin ◽  
Aru Yan ◽  
Xing Zhang
2012 ◽  
Vol 186 ◽  
pp. 206-211
Author(s):  
Daniela Derewnicka ◽  
Piotr Dłużewski ◽  
Marzena Spyra ◽  
Hanna Krztoń

This study investigated alloys with the composition Nd9Fe77B14 and Nd9Fe73Ti4B14 (at.%). Materials were melt spun in the form of a partially amorphous ribbon, which was subsequently annealed at 953K in order to obtain the optimum magnetic properties. The highest properties were obtained for annealing lasting 20 minutes (JHC = 913kA/m, Jr = 0,84T, BHmax = 107kJ/m3). Annealing at 953K results in simultaneous crystallisation in the whole mass of the alloy. The growth of grains is controlled by the duration of the annealing process. The objective of this work was to study the mechanisms of crystallisation and the reasons for a finer structure resulting from the presence of titanium. The phase composition was evaluated by X-ray diffraction. The microstructure was studied using a high-resolution transmission electron microscope. Detailed analysis of titanium distribution in the grains and in the grain boundaries was examined by x-ray spectrometry.


2015 ◽  
Vol 644 ◽  
pp. 7-12 ◽  
Author(s):  
Mithun Palit ◽  
J. Arout Chelvane ◽  
Himalay Basumatary ◽  
D. Aravindha Babu ◽  
S.V. Kamat

2015 ◽  
Vol 618 ◽  
pp. 258-262 ◽  
Author(s):  
A. Wisniewski ◽  
R. Puzniak ◽  
Z. Śniadecki ◽  
A. Musiał ◽  
M. Jarek ◽  
...  

2002 ◽  
Vol 91 (11) ◽  
pp. 9267-9271 ◽  
Author(s):  
Z. G. Sun ◽  
W. Löser ◽  
J. Eckert ◽  
K.-H. Müller ◽  
L. Schultz

2009 ◽  
Vol 479 (1-2) ◽  
pp. 78-81 ◽  
Author(s):  
L.Y. Li ◽  
A. Yan ◽  
J.H. Yi ◽  
G.T. Zhang ◽  
W. Xie ◽  
...  

2016 ◽  
Vol 483 ◽  
pp. 69-74 ◽  
Author(s):  
M. Hussain ◽  
L.Z. Zhao ◽  
C. Zhang ◽  
D.L. Jiao ◽  
X.C. Zhong ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document