Microwave dielectric high-entropy ceramic Li(Gd0.2Ho0.2Er0.2Yb0.2Lu0.2)GeO4 with stable temperature coefficient for low-temperature cofired ceramic technologies

Author(s):  
Huaicheng Xiang ◽  
Lei Yao ◽  
Junqi Chen ◽  
Aihong Yang ◽  
Haitao Yang ◽  
...  
2012 ◽  
Vol 535-537 ◽  
pp. 832-835
Author(s):  
Hui Xiong ◽  
Gang Xiong ◽  
Cui Hua She

The effects of B2O3 on the sinterability and microwave dielectric properties of Ca[(Li1/3Nb2/3)0.95Zr0.05]O3−δ−0.04TiO2 (CLNZ−0.04TiO2) ceramics were investigated . B2O3 doping can effectively reduce sintering temperatue by 150~200°C. The temperature coefficient of resonator frequency τf increased with an increase of B2O3 content and sintering temperatue. When B2O3 of 2wt% were added, the optimum microwave dielectric properties: εr =31.8,Qf =17240GHz and τf = − 5.9×10−6/°C were obtained at the sintering temperature of 950°C.


2010 ◽  
Vol 25 (12) ◽  
pp. 2380-2383 ◽  
Author(s):  
Yi Zeng ◽  
Hong Wang ◽  
Huanfu Zhou

The effect of BaCu(B2O5) (BCB) on the sintering temperature and microwave dielectric properties of Ba(Nd0.8Bi0.2)2Ti4O12 (BNBT) ceramics was investigated. The sintering temperature of the BNBT ceramics was significantly reduced from 1300 to 900 °C. Due to adding BCB into Ba(Nd1–xBix)2Ti4O12, the temperature coefficient of resonant frequency can be adjusted to zero with BCB content increasing. Good microwave dielectric properties of quality factor (Q×f) = 2600 GHz, εr = 75, and τf = 5 ppm/°C were obtained for BNBT with 7 wt% BCB sintered at 925 °C for 2 h, which make it a potential candidate for low temperature cofired ceramics applications.


Alloy Digest ◽  
1960 ◽  
Vol 9 (4) ◽  

Abstract EVANOHM is a nickel-base alloy having low temperature coefficient of resistance and high electrical resistivity. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on joining. Filing Code: Ni-57. Producer or source: Wilbur B. Driver Company.


Alloy Digest ◽  
1957 ◽  
Vol 6 (8) ◽  

Abstract ISO-ELASTIC is an iron-nickel alloy having low temperature coefficient of the modulus of elasticity. It is suitable for precision instrument springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Fe-14. Producer or source: John Chatillon & Sons.


2020 ◽  
Vol 26 (S2) ◽  
pp. 2916-2917
Author(s):  
Luis Laguna Zubia ◽  
C.G. Garay-Reyes ◽  
M.A. Ruiz-Esparza-Rodriguez ◽  
J.M. Mendoza-Duarte ◽  
Ivanovich Estrada ◽  
...  

Metals ◽  
2021 ◽  
Vol 11 (5) ◽  
pp. 742
Author(s):  
Motomichi Koyama ◽  
Takeaki Gondo ◽  
Kaneaki Tsuzaki

The effects of ausforming in an Fe30Mn10Cr10Co high-entropy alloy on the microstructure, hardness, and plastic anisotropy were investigated. The alloy showed a dual-phase microstructure consisting of face-centered cubic (FCC) austenite and hexagonal close-packed (HCP) martensite in the as-solution-treated condition, and the finish temperature for the reverse transformation was below 200 °C. Therefore, low-temperature ausforming at 200 °C was achieved, which resulted in microstructure refinement and significantly increased the hardness. Furthermore, plasticity anisotropy, a common problem in HCP structures, was suppressed by the ausforming treatment. This, in turn, reduced the scatter of the hardness.