Influence of Mo addition on microstructure and mechanical properties of Ti(C,N)-based cermets fabricated by in-situ carbothermal reduction of TiO2

Vacuum ◽  
2021 ◽  
Vol 184 ◽  
pp. 109912
Author(s):  
Zhengkai Yang ◽  
Yong Zheng ◽  
Xiangyu Xu ◽  
Guotao Zhang ◽  
Zheng Ke ◽  
...  
2021 ◽  
Vol 212 ◽  
pp. 108681
Author(s):  
Diqiang Liu ◽  
Aijun Zhang ◽  
Jiangang Jia ◽  
Jiesheng Han ◽  
Junyan Zhang ◽  
...  

Crystals ◽  
2021 ◽  
Vol 11 (4) ◽  
pp. 422
Author(s):  
Kuai Zhang ◽  
Yungang Li ◽  
Hongyan Yan ◽  
Chuang Wang ◽  
Hui Li ◽  
...  

An Fe/FeAl2O4 composite was prepared with Fe-Fe2O3-Al2O3 powder by a hot press sintering method. The mass ratio was 6:1:2, sintering pressure was 30 MPa, and holding time was 120 min. The raw materials for the powder particles were respectively 1 µm (Fe), 0.5 µm (Fe2O3), and 1 µm (Al2O3) in diameter. The effect of sintering temperature on the microstructure and mechanical properties of Fe/FeAl2O4 composite was studied. The results showed that Fe/FeAl2O4 composite was formed by in situ reaction at 1300 °C–1500 °C. With the increased sintering temperature, the microstructure and mechanical properties of the Fe/FeAl2O4 composite showed a change law that initially became better and then became worse. The best microstructure and optimal mechanical properties were obtained at 1400 °C. At this temperature, the grain size of Fe and FeAl2O4 phases in Fe/FeAl2O4 composite was uniform, the relative density was 96.7%, and the Vickers hardness and bending strength were 1.88 GPa and 280.0 MPa, respectively. The wettability between Fe and FeAl2O4 was enhanced with increased sintering temperature. And then the densification process was accelerated. Finally, the microstructure and mechanical properties of the Fe/FeAl2O4 composite were improved.