Hot cracking resistance of welded joints in austenitic steels produced by high-speed laser welding

1997 ◽  
Vol 11 (2) ◽  
pp. 149-151
Author(s):  
A N Grezev ◽  
A F Baskov ◽  
V L Luk'yanenko
2015 ◽  
Vol 60 (3) ◽  
pp. 1807-1812
Author(s):  
M. Stolecki ◽  
H. Bijok ◽  
Ł. Kowal ◽  
J. Adamiec

Abstract This paper describes the technology of welding of finned tubes made of the X5CrNi1810 (1.4301) austenitic steel, developed at Energoinstal SA, allowing one to get high quality joints that meet the requirements of the classification societies (PN-EN 15614), and at the same time to significantly reduce the manufacturing costs. The authors described an automatic technological line equipped with a Trumph disc laser and a tube production technological process. To assess the quality of the joints, one performed metallographic examinations, hardness measurements and a technological attempt to rupture the fin. Analysis of the results proved that the laser-welded finned tubes were performed correctly and that the welded joints had shown no imperfections.


2021 ◽  
Vol 313 ◽  
pp. 94-105
Author(s):  
A. Bernatskyi ◽  
V. Sydorets ◽  
O.M. Berdnikova ◽  
I. Krivtsun ◽  
O. Kushnarova

Extending the lifetime of energy facilities is extremely important today. This is especially true of nuclear power plants, the closure (or modernization) of which poses enormous financial and environmental problems. High-quality repair of reactors can significantly extend their service life. One of the critical parts is heat exchangers, the tubes of which quite often fail. Sealing, as a type of repair of heat exchanger tubes by the plugs, is promising provided that the joint quality is high. Practical experience in the use of welding to solve this problem has shown the need to search technological solutions associated with increasing the depth of penetration and reducing the area of thermal effect. The aim of the work was to develop a highly efficient technology for repair and extension of service life of heat exchangers of nuclear power plants based on the results of studying the technological features of laser welding of joints of dissimilar austenitic steels AISI 321 and AISI 316Ti in the vertical spatial position. Based on the results of the analysis of mechanical test data, visual and radiographic control, impermeability tests and metallographic studies of welded joints, the appropriate modes of laser welding of plugs have been determined. The principal causes of defects during laser welding of annular welded joints of dissimilar stainless steels are determined and techniques for their elimination and prevention of their formation are proposed. Based on the results of the research, technological recommendations for laser welding of plugs in the heat exchange tube of the collector are formulated, which significantly improves the technology of repair of steam generators of nuclear power plants and extends the service life of reactors.


1998 ◽  
Vol 12 (5) ◽  
pp. 390-393
Author(s):  
E L Makarov ◽  
A V Konovalov ◽  
B F Ya Kushin ◽  
A A Pshennikov

1993 ◽  
Vol 7 (2) ◽  
pp. 147-149
Author(s):  
A V Surkov ◽  
A S Zupchenko ◽  
P N Kipiani ◽  
L E Balandina ◽  
A I Savchenko ◽  
...  

2021 ◽  
Vol 93 (1) ◽  
pp. 15-23
Author(s):  
Piotr Śliwiński ◽  
Maciej Piotrowski

Contemporary grades of structural steels are produced using a very advanced thermo-mechanical treatment processes, so their properties strongly depend on the obtained structure. Corrosion-resistant austenitic steels have a high hot cracking tendency. Therefore, it is advantageous to use welding technologies, such as laser welding, that limit the size of the joint and its heat-affected zones and thus the deformations caused by the welding process. Laser welding is also characterized by small amount of heat transferred into the material  during the process which limits the hot cracking tendency. During the tests, 8 samples made of S960QL steel and S304 steel, were prepared using a Trumpf TruDisk 3302 laser welding device. The produced samples were subjected to macro- and microscopy metallographic tests. Static tensile test and bend test were also performed as well as a hardness  Vickers test under a load of 100N. Good quality joints were obtained, characterized by a small number of welding imperfections, small size of the weld and heat affected zone, as well as satisfactory mechanical properties.


Alloy Digest ◽  
2002 ◽  
Vol 51 (5) ◽  

Abstract NIROSTA 4305 is an austenitic alloy with a high sulfur content. The alloy is typically used for machined parts. As with other austenitic steels, it is necessary to machine with good-quality high-speed steel or tungsten carbide tools. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-854. Producer or source: ThyssenKrupp Nirosta GmbH.


Sign in / Sign up

Export Citation Format

Share Document