Effect of oxidation heat treatment on the bond strength between a ceramic and cast and milled cobalt-chromium alloys

2015 ◽  
Vol 123 (4) ◽  
pp. 297-304 ◽  
Author(s):  
Jieyin Li ◽  
Xiuhua Ye ◽  
Bohua Li ◽  
Juankun Liao ◽  
Peilin Zhuang ◽  
...  
2021 ◽  
Vol 24 (6) ◽  
Author(s):  
Michelli Menezes Sobreiro ◽  
Ana Paula Macedo ◽  
Osvaldo Luiz Bezzon ◽  
Valéria Oliveira Pagnano

2014 ◽  
Vol 2 (1) ◽  
pp. 16 ◽  
Author(s):  
Flávia Trindade ◽  
Lilian Anami ◽  
Júlia da Costa Lima ◽  
Luis Gustavo de Vasconcellos ◽  
Ivan Balducci ◽  
...  

2014 ◽  
Vol 112 (3) ◽  
pp. 600-605 ◽  
Author(s):  
Josep Serra-Prat ◽  
Jordi Cano-Batalla ◽  
Josep Cabratosa-Termes ◽  
Oscar Figueras-Àlvarez

2006 ◽  
Vol 17 (1) ◽  
pp. 24-28 ◽  
Author(s):  
Alfredo Julio Fernandes Neto ◽  
Heitor Panzeri ◽  
Flavio Domingues Neves ◽  
Ricardo Alves do Prado ◽  
Gustavo Mendonça

Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cylinder specimens (15 mm in height; 6 mm in diameter) were obtained for each alloy, in away that 10 specimens of each alloy were tested with each porcelain. Bond strength was measured with an Emic screw-driven mechanical testing machine by applying parallel shear forces to the specimens until fracture. Kruskal-Wallis and Mann-Whitney U tests were used for statistical analysis of the alloy/ceramic combinations (p<0.05). Resistal P/Duceram had significantly higher bond strength (44.38±9.12 MPa) (p<0.05) than the other combinations, except for Co-Cr-Ti alloy/Vita VMK 88 (38.41±12.64 MPa). The association of the experimental Co-Cr-Ti alloy with Williams porcelain had significantly higher bond strength (28.20±3.86 MPa) than the combination of other alloys with the same porcelain (p<0.05). Based of these results and within the limitations of an in vitro study, it may be concluded that the bond strength of the three ceramic systems to the Ni-Cr and Co-Cr-Ti alloys varied significantly, indicating that metal/ceramic compatibility was very important to the bond strength.


2007 ◽  
Vol 64 (4) ◽  
pp. 241-245 ◽  
Author(s):  
Nemanja Mirkovic

Background/Aim. Metal-ceramic bond strength and alloys' elastic modulus clearly determine the potential of alloy application, because the ceramic integrity during mastication depends on these two characteristics. The aim of this study was to evaluate metal-ceramic bond strength and elastic modulus of cobalt-chromium alloys in making porcelainfused- to-metal restorations, regarding the application of the most frequent nickel-chromium alloy. Methods. The research was performed as an experimental study. Six metalceramic samples were made from nickel-chromium alloy (Wiron 99) and cobalt-chromium alloy (Wirobond C), according to the manufactures manuals and instructions from ISO 9693: 1996. Three-point bending test was performed up to the ceramic fracture. The fracture load was measured on an universal testing machine (Zwick, type 1464), with cross-head speed of 0,05mm/min. Results. The results of this study confirmed the significant differences between the metal-ceramic bond strength (p < 0.01) and elastic modulus (p < 0.001) of nickel-chromium and cobalt-chromium alloys, where cobalt-chromium alloys showed higher values for both tested parameters. Conclusion. Cobalt-chromium metal-ceramic alloys can successfully replace nickel-chromium alloys, especially for fabrication of long-span metal-ceramic bridges due to the great flexural strength.


2021 ◽  
Vol 43 ◽  
pp. 2629-2634
Author(s):  
Wanwilai Vittayakorn ◽  
Phieraya Poolphol ◽  
Kantapon Aimprakod ◽  
Tosapol Maluangnont