6xxx Series Al Alloy Sheets with High Formability Produced by Twin-roll Strip Casting and Asymmetric Rolling

2012 ◽  
Vol 50 (7) ◽  
pp. 503-509 ◽  
Author(s):  
Jae-Chul Lee ◽  
Hong-Kyu Kim ◽  
Jae-Hyung Cho ◽  
Hyoung-Wook Kim
2015 ◽  
Vol 772 ◽  
pp. 250-256 ◽  
Author(s):  
Hideto Harada ◽  
Shin Ichi Nishida ◽  
Mayumi Suzuki ◽  
Hisaki Watari ◽  
T. Haga

This paper describes direct cladding of magnesium (Mg) and aluminum (Al) alloys using a tandem horizontal twin roll caster that has three pairs of upper and lower rolls. Manufacturing conditions that are appropriate for fabricating Al/Mg and Al/Mg/Al cladded material were investigated. The surface condition of the cladded cast strip was examined. An electron probe micro analyzer was used to observe the interface between Al alloy and Mg alloy. The thickness of the mixed layer of Al and Mg alloy was 15μm, and how the materials were connected was clarified. Microscopic observation and backscattered electron analysis were used to investigate the cladding mechanisms of the Al and Mg alloy layers. Average hardness was determined using the Vickers hardness test at the Al layer and at the diffused layer between Mg and Al alloys. Cladding of Al/Mg alloy and A/Mg/Al alloy was possible using a tandem twin-roll caster. In addition, Al3Mg2 and Al12Mg17 phase precipitation at the interface of the Al and Mg alloys was confirmed during direct cladding from molten metals.


Author(s):  
Zhi-Qiang Xu ◽  
Zhe-Ru Meng ◽  
Shun-Hui Xue ◽  
De-Quan Zhang ◽  
Feng-Shan Du

2017 ◽  
Vol 898 ◽  
pp. 1276-1282
Author(s):  
Wen Li Hu ◽  
Yuan Xiang Zhang ◽  
Guo Yuan ◽  
Guo Dong Wang

High silicon steel was fabricated by twin-roll strip casting. The cracks on the surfaces of the processed strips were obtained and analyzed by digital camera after series of surface treatment. Optical microscopy (OM) and scanning electron microscopy (SEM) were used to observe and characterize the microstructure nearby crack and fracture surface along the normal direction, respectively, and the crack formation mechanism was further analyzed in conjunction with processing parameters utilized during twin-roll strip casting process. The results indicated that morelongitudinal cracks along the rolling direction were observed in comparison with transverse cracks along the transverse direction on the strip surfaces. Trans granular and intergranular fracture modes both worked during the formations of longitudinal and transverse cracks on the processed strips. The dominant factor causing the formation of crack on the surface of the processed strips was the inhomogeneous transfer of heat during casting and rolling. The inhomogeneous transfer of heat induced by gas gap during casting resulted in variations of dendrite length and secondary dendrite spacing (SDAS). Meanwhile, the casting velocity influenced the formation of gas gap, which further influenced the thermal contraction. So the control of velocity of casting above a certain level proved beneficial to enhancing the performance of strip casting and to improving the quality of strip products.


2019 ◽  
Vol 29 (5) ◽  
pp. 1017-1025 ◽  
Author(s):  
Mang XU ◽  
Guo-huai LIU ◽  
Tian-rui LI ◽  
Bing-xing WANG ◽  
Zhao-dong WANG

2018 ◽  
Vol 773 ◽  
pp. 171-178
Author(s):  
Toshio Haga ◽  
Kentaro Okamura ◽  
Hisaki Warari ◽  
Shinichi Nishida

This paper shows improvements made to a vertical type tandem twin roll caster and the appropriate casting conditions necessary to cast three-layer clad strips, the base strip of which has a lower solidification temperature than the overlay strip. In experiments, 4045 aluminum alloy was used for the base strip and 3003 aluminum alloy was used for the overlay strips. The roll speed was 30 m/min. By connecting the overlay strips to the base strip one at a time and cooling the base strip to between 450 and 530°C after applying the first overlay strip, a sound three-layer clad strip – defined as one in which the interfaces between strips are clear and do not separate during bending-to-failure tests – could be cast. The tensile shear testing between the base and second overlay strip was improved as the base-strip temperature was increased to 450-530°C range.


2007 ◽  
Vol 187-188 ◽  
pp. 339-343 ◽  
Author(s):  
X.M. Zhang ◽  
Z.Y. Jiang ◽  
L.M. Yang ◽  
X.H. Liu ◽  
G.D. Wang ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document