Study on Cleanliness of Ultra-Low Carbon Steel First Slab
By means of Oxygen and Nitrogen Analyzer, Metallographic Examination, SLIME, SEM, EDS, etc, the cleanliness of ultra-low carbon steel first slab produced by LD-RH-CC, and the comparative analysis with the cleanliness of normal slab is studied. The results show that T[O] and [N] are obviously decreasing with the increasing of casting length. The micro-inclusions and large-inclusions are generally decreasing with the increasing of casting length. The micro-inclusions of the first slab are mainly from deoxidization products and reoxidation of liquid steel. And the sources of large-sized inclusions mainly are reoxidation of liquid steel, slag entrapment in mould or tundish and stuffing sand. The cleanliness of ultra-low carbon steel first slab is closed to those normal slabs at the length of 3.5m.