scholarly journals Shear Bond Strength of Enamel-Composite Resin-Zirconia Joints

Author(s):  
H. Serdar Çötert ◽  
◽  
Gökhan Aksoy ◽  
Niler Özdemir ◽  
◽  
...  
2014 ◽  
Vol 30 ◽  
pp. e38-e39
Author(s):  
M.A. Basílio ◽  
K.V. Cardoso ◽  
G.M.R.M. De Souza ◽  
E.M. Mariscal ◽  
J.N. Arioli-Filho

2018 ◽  
Vol 32 (4) ◽  
pp. 163
Author(s):  
Fábio Herrmann Coelho-de-Souza ◽  
Guilherme Fossá ◽  
Flávia Ávila Pereira ◽  
Celso Afonso Klein-Júnior ◽  
Maria Carolina Guilherme Erhardt ◽  
...  

OBJECTIVE: This study evaluated in vitro the shear bond strength of experimentally fractured human tooth fragments reattached with different adhesive materials and retentive techniques.METHODS: Forty-eight sound mandibular incisors were randomly divided into 6 groups (n=8). Their incisal edges were cut off in 5 groups, representing an enamel-dentin fracture. Intact teeth were used as control (Group 1). The fragment edges were reattached with adhesive system (Scotch Bond Multipurpose – 3M ESPE) (Group 2), adhesive system and composite resin (ICE – SDI) (Group 3), adhesive system and composite resin with circumferential bevel (Group 4), adhesive system and composite resin with internal dentin groove (Group 5), and adhesive system and composite resin with the circumferential bevel and internal dentin groove (Group 6). Shear bond strength was determined in a universal testing machine. Fracture modes were identified by light microscope. Kruskal-Wallis was used to analysis resistance to fracture and fracture patterns.RESULTS: The results showed statistically significant differences (p<0.05) among groups. The intact teeth (Group 1) showed higher fracture resistance than the other groups. Groups 2 and 6 did not differ and were statistically superior to other techniques. Group 4 presented statistically higher than in Group 5, which in turn was more resistant than Group 3.CONCLUSIONS: None of the fragment reattachment techniques was able to achieve the strength of sound teeth. Fragments reattached only with adhesive system or with adhesive system and composite resin with the circumferential bevel and internal dentin groove showed the best performance for resistance to fracture.


2002 ◽  
Vol 27 (6) ◽  
pp. 569 ◽  
Author(s):  
Soo-young Choi ◽  
Sun-Wa Jeong ◽  
Yun-Chan Hwang ◽  
Sun-Ho Kim ◽  
Chang Yun ◽  
...  

Author(s):  
Hoseinali Mahgoli ◽  
Mahnaz Arshad ◽  
Kamran Rasouli ◽  
Ali Akbar Sobati ◽  
Ahmad Reza Shamshiri

  Objectives: This study aimed to assess the effect of application of two types of zirconia primers on repair bond strength of composite to zirconia ceramic. Materials and Methods: In this in vitro, experimental study, 60 zirconia blocks were divided into five groups and subjected to the application of Z-Prime Plus (ZPP), Monobond Plus (MBP), Porcelain Bonding Resin (PBR), ZPP followed by PBR (ZPP+PBR) and MBP followed by PBR (MBP+PBR). They were then bonded to Z100 composite. The samples were then immersed in water at 37°C for 24 hours, thermocycled for 1000 cycles between 5-55°C and subjected to shear bond strength (SBS) test. The mode of failure was determined under a stereomicroscope and a scanning electron microscope (SEM). Results: The mean bond strength was the highest in ZPP+PBR group followed by MBP+PBR, ZPP, PBR and MBP group (22.29±8.86, 15.75±2.81, 12.02±3.24, 3.60±2.92 and 2.92±1.78 MPa, respectively). The effects of type of zirconia primer and use/no use of PBR on SBS were significant (P<0.05). The frequency of adhesive failure in MBP and PBR groups was significantly higher than that in MBP+PBR and ZPP+PBR groups (P<0.05). The cohesive failure was significantly more frequent in ZPP+PBR group than in ZPP, MBP and PBR groups (P<0.05). Conclusion: Simultaneous application of zirconia primer and PBR is the most efficient technique for repair of all-ceramic zirconia restorations with composite resin.


2014 ◽  
Vol 25 (6) ◽  
pp. 519-523 ◽  
Author(s):  
Erica Moreno Zanconato-Carvalho ◽  
João Felipe Bruniera ◽  
Natália Spadini de Faria ◽  
Vivian Colucci ◽  
Danielle Cristine Messias

Surface treatment of dentin before the bleaching procedure may affect its permeability and influence the bond strength of restorative materials. This study evaluated the influence of surface treatment before the bleaching on shear bond strength (SBT) of restorative materials to intracoronal dentin. Dentin slabs were subjected to surface treatment: no bleaching (control - CON), no surface treatment + bleaching (HP), 37% phosphoric acid + bleaching (PA) and Er:YAG laser + bleaching (L). After the bleaching procedure, specimens (n=10) were restored with: microhybrid composite resin (MH), flowable composite resin (F), and resin-modified glass-ionomer cement (RMGIC). The shear test was carried out. ANOVA and Tukey's test (α=0.05) showed significant difference for surface treatment and restorative materials (p<0.05). CON presented higher STB and was statistically different from HP (p<0.05). PA and L showed intermediate values and were statistically similar to CON and HP (p>0.05). STB for MH and F were higher than RMGIC (p<0.05), and did not differ from each other (p>0.05). The surface treatments with phosphoric acid and Er:YAG laser before the bleaching procedure provided shear bond strength at the same level of unbleached dentin and the composite resins presented superior bond strength to the intracoronal dentin.