This investigation describes the design, fabrication, and testing of woven glass fiber reinforced epoxy matrix laminates with aligned CNT sheets integrated between plies in order to improve the matrix dominated through thickness properties such as the interlaminar fracture toughness at ply interfaces. Using aligned CNT sheets allows for a concentration of millimeter long CNTs at the most likely point of laminate failure. Mode I and Mode II interlaminar fracture toughness of various CNT modified samples were investigated using double cantilever beam (DCB) and end notched flexure (ENF) experiments, respectively. Short beam strength (SBS) and in-plane tensile properties of the CNT modified samples were also investigated. Moderate improvement was observed in Mode I and Mode II fracture toughness at crack initiation when aligned CNT sheets with a basis weight of 0.354 g/m2were used to modify the ply interface. No compromise in the in-plane mechanical properties of the laminate was observed and very little improvement was observed in the shear related short beam strength of the CNT modified laminates as compared to the control samples. Integration of aligned CNT sheets into the composite laminate imparted in-plane and through thickness electrical properties into the nonconductive glass fiber reinforced epoxy composite laminates.


2011 ◽  
Vol 194-196 ◽  
pp. 1697-1702
Author(s):  
Li Liang ◽  
Pu Rong Jia ◽  
Gui Qiong Jiao

Delamination is one of the important damage modes in the fiber-reinforced composite laminates. The interlaminar fracture toughness is the key parameter in delamination failure analysis of composites. The stress analysis by a finite element modeling has shown that the shear stress is very large near the ply splicing area. So the delamination failure is mainly dependent on the mode II fracture toughness. A new way of loading in tensile testing is proposed for the measurement of mode II fracture toughness. Specific specimen with splicing plies has been designed and used for the experiment. Testing study on the carbon-fiber-reinforced laminate with ply splicing was performed. Steady crack propagation has been seen by the tensile testing of the specimen. Mode II fracture toughness GIIC of the laminate has been determined by the experiment data analysis. The experiment and numerical analysis shows that the tensile testing for the measurement of mode II interlaminar fracture toughness is feasible.


Materials ◽  
2021 ◽  
Vol 14 (9) ◽  
pp. 2103
Author(s):  
Christophe Floreani ◽  
Colin Robert ◽  
Parvez Alam ◽  
Peter Davies ◽  
Conchúr M. Ó. Brádaigh

Powder epoxy composites have several advantages for the processing of large composite structures, including low exotherm, viscosity and material cost, as well as the ability to carry out separate melting and curing operations. This work studies the mode I and mixed-mode toughness, as well as the in-plane mechanical properties of unidirectional stitched glass and carbon fibre reinforced powder epoxy composites. The interlaminar fracture toughness is studied in pure mode I by performing Double Cantilever Beam tests and at 25% mode II, 50% mode II and 75% mode II by performing Mixed Mode Bending testing according to the ASTM D5528-13 test standard. The tensile and compressive properties are comparable to that of standard epoxy composites but both the mode I and mixed-mode toughness are shown to be significantly higher than that of other epoxy composites, even when comparing to toughened epoxies. The mixed-mode critical strain energy release rate as a function of the delamination mode ratio is also provided. This paper highlights the potential for powder epoxy composites in the manufacturing of structures where there is a risk of delamination.


2018 ◽  
Vol 1 (2) ◽  
Author(s):  
Mohamad Alsaadi 1,2 ◽  
Ahmet Erkliğ 2

In this study, the influence of sewage sludge ash (SSA) waste particle contents on the mechanical properties and interlaminar fracture toughness for mode I and mode II delamination of S-glass fiber reinforced epoxy composites were investigated. Composite laminate specimens for tensile, flexural double-cantilever beam (DCB) and end-notched flexure (ENF) tests were prepared and tested according to ASTM standards with 5, 10, 15 and 20 wt% SSA filled S-glass/epoxy composites. Properties improvement reasons was explained based on optical and scanning electron microscopy. The highest improvement in tensile and flexural strength was obtained with 10 wt% content of SSA. The highest mode I and mode II interlaminar fracture toughness’s were obtained with 15 wt% content of SSA. The mode I and mode II interlaminar fracture toughness’s improved by 33 and 63.6%, respectively, compared to the composite without SSA.