Cement-based grouts for masonry consolidation with high content of limestone filler, metakaolin, glass powder and ceramic waste

2021 ◽  
Vol 306 ◽  
pp. 124947
Author(s):  
Miguel C.S. Nepomuceno ◽  
Luís F.A. Bernardo ◽  
Luiz A. Pereira-de-Oliveira ◽  
Rúben O. Timóteo
2002 ◽  
Vol 713 ◽  
Author(s):  
Roman V. Bogdanov ◽  
Yuri F. Batrakov ◽  
Elena V. Puchkova ◽  
Andrey S. Sergeev ◽  
Boris E. Burakov

ABSTRACTAt present, crystalline ceramic based on titanate pyrochlore, (Ca,Gd,Hf,Pu,U)2Ti2O7, is considered as the US candidate waste form for the immobilization of weapons grade plutonium. Naturally occuring U-bearing minerals with pyrochlore-type structure: hatchettolite, betafite, and ellsworthite, were studied in orders to understand long-term radiation damage effects in Pu ceramic waste forms. Chemical shifts (δ) of U(Lδ1)– and U(Lβ1) – X-ray emission lines were measured by X-ray spectrometry. Calculations were performed on the basis of a two-dimensional δLá1- and δLδ1- correlation diagram. It was shown that 100% of uranium in hatchettolite and, probably, 95-100% of uranium in betafite are in the form of (UO2)2+. formal calculation shows that in ellsworthite only 20% of uranium is in the form of U4+ and 80% of the rest is in the forms of U5+ and U6+. The conversion of the initial U4+ ion originally occurring in the pyrochlore structure of natural minerals to (UO2)2+ due to metamict decay causes a significant increase in uranium mobility.


1982 ◽  
Vol 14 (4-5) ◽  
pp. 281-290
Author(s):  
Ph Vilaginès ◽  
B Sarrette ◽  
C Danglot ◽  
R Vilaginès

The aim of this work is to describe a new and inexpensive glass powder apparatus allowing virus concentration from 500 1 sample of water (10). Its efficiency was determined by analysis of drinking and surface waters preinoculated by Poliovirus. The detection of viruses from river water is compared when 500 1 (new apparatus) or 10 1 (preceeding apparatus) (7) are processed. The proposed new 500 1 apparatus allowed the recuperation of viruses in 100 % of the analysed samples the 10 1 one allowing their recuperation in only 50 % samples. This method was applied to the virus determination in the surface and drinking waters of the Paris area.


2018 ◽  
Vol 102 (7) ◽  
pp. 4314-4324 ◽  
Author(s):  
Mingyang Zhao ◽  
Yun Xu ◽  
Lindsay Shuller‐Nickles ◽  
Jake Amoroso ◽  
Anatoly I. Frenkel ◽  
...  

Materials ◽  
2021 ◽  
Vol 14 (4) ◽  
pp. 869
Author(s):  
Minghua Wei ◽  
Shaopeng Wu ◽  
Haiqin Xu ◽  
Hechuan Li ◽  
Chao Yang

Steel slag is the by-product of the steelmaking industry, the negative influences of which prompt more investigation into the recycling methods of steel slag. The purpose of this study is to characterize steel slag filler and study its feasibility of replacing limestone filler in asphalt concrete by evaluating the resistance of asphalt mastic under various aging methods. Firstly, steel slag filler, limestone filler, virgin asphalt, steel slag filler asphalt mastic and limestone filler asphalt mastic were prepared. Subsequently, particle size distribution, surface characterization and pore characterization of the fillers were evaluated. Finally, rheological property, self-healing property and chemical functional groups of the asphalt mastics with various aging methods were tested via dynamic shear rheometer and Fourier transform infrared spectrometer. The results show that there are similar particle size distributions, however, different surface characterization and pore characterization in the fillers. The analysis to asphalt mastics demonstrates how the addition of steel slag filler contributes to the resistance of asphalt mastic under the environment of acid and alkaline but is harmful under UV radiation especially. In addition, the pore structure in steel slag filler should be a potential explanation for the changing resistance of the asphalt mastics. In conclusion, steel slag filler is suggested to replace limestone filler under the environment of acid and alkaline, and environmental factor should be taken into consideration when steel slag filler is applied to replace natural fillers in asphalt mastic.


Sign in / Sign up

Export Citation Format

Share Document