Evaluation of Mechanical Properties of Glass Fiber Reinforced Epoxy Polymer Composites with Alumina, Titanium dioxide and Silicon Carbide Fillers

2018 ◽  
Vol 5 (10) ◽  
pp. 22355-22361 ◽  
Author(s):  
M.D. Kiran ◽  
H.K. Govindaraju ◽  
T. Jayaraju
2000 ◽  
Vol 21 (5) ◽  
pp. 739-744 ◽  
Author(s):  
M. Alagar ◽  
T. V. Thanikai Velan ◽  
A. Ashok Kumar

2022 ◽  
Vol 58 (4) ◽  
pp. 28-36
Author(s):  
Velmurugan Natarajan ◽  
Ravi Samraj ◽  
Jayabalakrishnan Duraivelu ◽  
Prabhu Paulraj

This study aims to reveal the consequence of thickness reinforcement on Fiber Laminates (Polyester Resin, Glass Fiber, Aluminum, and Bentonite) and to see if it can enhance the mechanical properties and resistance of laminates. Glass fiber reinforced polymer composites have recently been used in automotive, aerospace, and structural applications where they will be safe for the application s unique shape. Hand layup was used to fabricate three different combinations, including Aluminium /Glass fiber reinforced polyester composites (A/GFRP), Bentonite/Glass fiber reinforced polyester composites (B/GFRP), and Aluminium&Bentonie/Glass fiber reinforced polyester composites (AB/GFRP). Results revealed that AB/GFRP had better tensile strength, flexural strength, and hardness than GFRP and A/GFRP. Under normal atmospheric conditions and after exposure to boiling water, hybrid Aluminium&Bentonite and glass fiber-reinforced nanocomposites have improved mechanical properties than other hybrid composites. After exposure to temperature, the flexural strength, tensile strength and stiffness of AB/GFRP Composites are 40 % higher than A/GFRP and 17.44% higher than B/GFRP Composites.


2020 ◽  
Vol 60 (4) ◽  
pp. 740-751 ◽  
Author(s):  
Bruno Ribeiro ◽  
Jefersson Alexander Rojas Corredor ◽  
Michelle Leali Costa ◽  
Edson Cocchieri Botelho ◽  
Mirabel Cerqueira Rezende