Photostabilization of wood using low molecular weight phenol formaldehyde resin and hindered amine light stabilizer

2013 ◽  
Vol 98 (1) ◽  
pp. 158-168 ◽  
Author(s):  
Philip D. Evans ◽  
Sara Kraushaar Gibson ◽  
Ian Cullis ◽  
Chunling Liu ◽  
Gilles Sèbe
1995 ◽  
Vol 68 (5) ◽  
pp. 717-727 ◽  
Author(s):  
Martin van Duin ◽  
Aniko Souphanthong

Abstract The application of phenol-formaldehyde resins as crosslinking agents is increasing in importance due to the good high temperature properties of the corresponding vulcanizate and the use in thermoplastic vulcanizates. With respect to the chemistry of phenol-formaldehyde cure (reaction mechanism and structure of crosslink) there are still problems that have to be resolved. The reaction products of the phenol-formaldehyde resin curing of EPDM, contain 2-ethylidene norbornene (ENB) as the third monomer, have been studied. Since such an investigation is rather difficult to perform for the polymer system, a low molecular weight model for EPDM was used: 2-ethylidene norbornane (ENBH). Reaction of ENBH and a resole results in scission of the dimethylene ether bridges, i.e. in degradation of the resole into mono-, bis- and terisooctylphenol units. These are consequently converted into products, consisting of two ENBH molecules linked by mono-, bis- and terisooctylphenol units. The solid resole seems to be a technological solution for storing phenol in combination with formaldehyde. These results support the use of 2-hydroxymethylphenol (HMP) as a low molecular weight model for the resole. At low temperatures and/or short reaction times HMP oligomers (= resoles) and HMP oligomers linked to one ENBH molecule are formed, which are converted into ENBH/HMP (1:1) condensation products. The reaction products of ENBH with both the resole and HMP are shown to contain methylene linked structures, as demonstrated by the formation of monisooctylphenol crosslinks and the presence of residual unsaturation and hydroxyl groups, besides chroman linked structures. This is the first experimental evidence that during phenol-formaldehyde resin cure of rubber, formation of methylene bridges occurs.


2017 ◽  
Vol 19 (3) ◽  
pp. 1-11 ◽  
Author(s):  
G. Aizat ◽  
A. Zaidon ◽  
S. H. Lee ◽  
S. B. Edi ◽  
B. Paiman

In order to improve the inherently poor properties of oil palm wood (OPW), this study examines the effects of resin molecular weight, diffusion time and compression ratio on the properties of laminated compreg OPW. Treating solutions used were medium molecular weight phenol formaldehyde (MmwPF) and low molecular weight phenol formaldehyde (LmwPF). OPW strips were soaked in the treating solutions for 24 h before wrapping in a plastic bag and leaving them for diffusion for 2, 4 and 6 days, respectively. Then, three-layer laminated compreg OPW were fabricated and compressed in hot press at 150°C for 20 minutes to achieve compression ratios of 55%, 70% and 80%. Results indicated that dimensional stability and mechanical properties of the phenolic resin treated laminated compreg OPW were significantly better than the untreated laminates. MmwPF-treated laminates exhibited inferior properties in comparison to that of LmwPF-treated laminates. Nevertheless, MmwPF-treated laminated compreg OPW emitted significantly lesser formaldehyde.


Forests ◽  
2020 ◽  
Vol 11 (1) ◽  
pp. 84 ◽  
Author(s):  
Susanne Bollmus ◽  
Cara Beeretz ◽  
Holger Militz

This study deals with the influence of chemical modification on elasto-mechanical properties of Scots pine (Pinus sylvestris L.). The elasto-mechanical properties examined were impact bending strength, determined by impact bending test; tensile strength; and work to maximum load in traction, determined by tensile tests. The modification agents used were one melamine-formaldehyde resin (MF), one low molecular weight phenol-formaldehyde resin, one higher molecular weight phenol-formaldehyde resin, and a dimethylol dihydroxyethyleneurea (DMDHEU). Special attention was paid to the influence of the solution concentration (0.5%, 5%, and 20%). With an increase in the concentration of each modification agent, the elasto-mechanical properties decreased as compared to the control specimens. Especially impact bending strength decreased greatly by modifications with the 0.5% solutions of each agent (by 37% to 47%). Modification with DMDHEU resulted in the highest overall reduction of the elasto-mechanical properties examined (up to 81% in work to maximum load in traction at 20% solution concentration). The results indicate that embrittlement is not primarily related to the degree of modification depended on used solution concentration. It is therefore assumed that molecular size and the resulting ability to penetrate into the cell wall could be crucial. The results show that, in the application of chemically modified wood, impact and tensile loads should be avoided even after treatment with low concentrations.