A new type of graft copolymer, sulfonated humic acid-acrylic acid resin (SHA), was synthesized and developed as dispersant for highly-loaded coal water slurry (CWS) from Chinese Binchang coal. In this study, The formulation, stability and rheology of the slurry with SHA were investigated. The experimental results show that SHA can reduce effectively CWS viscosity at low dosage, and that the CWS with SHA has excellent stability within 48 h and exhibits shear-thinning apparent viscosity/shear rate behavior. Based on the above, SHA is a promising dispersant for highly-loaded CWS in the practical use in industry.


2010 ◽  
Vol 24 (2) ◽  
pp. 1260-1268 ◽  
Author(s):  
Debadutta Das ◽  
Uma Dash ◽  
Amalendu Nayak ◽  
Pramila K. Misra

1989 ◽  
Vol 7 (0) ◽  
pp. 43-49
Author(s):  
Hayami Itoh ◽  
Shuhei Tatsumi ◽  
Yoshihiro Kajibata ◽  
Shoichi Takao ◽  
Hironori Ozaki ◽  
...  

Processes ◽  
2019 ◽  
Vol 7 (8) ◽  
pp. 500 ◽  
Author(s):  
Shen ◽  
Min ◽  
Liu ◽  
Xue ◽  
Zhu

Low-rank coal is difficult to upgrade using conventional flotation methods due to its high hydrophilic properties. Thus, it is necessary to explore new methods for upgrading and utilizing low-rank coal. In this investigation, a gaseous dodecane pretreatment method was used to enhance the flotation performance of low-rank coal. Pore distribution analysis, FTIR (Fourier Transform Infrared Spectroscopy), and contact angle measurements were used to study the surface properties of the coal sample. Size distribution and float-sink test results indicated that the coal sample contained a lot of clean coal with low ash content, which could be used as a high quality raw material for making coal water slurry. FTIR, pore distribution analysis, and contact angle results showed that the coal was very hydrophilic due to the high concentration of -OH group and the large number of pores and cracks on the coal surface. The hydrophobicity of the coal sample was significantly improved by the gaseous dodecane pretreatment method. Clean coal with 67.2% combustible matter recovery and 10.5% ash content was obtained by gaseous dodecane pretreatment flotation method. Coal water slurry with 60% concentration was prepared using the flotation clean coal.


2015 ◽  
Vol 37 (4) ◽  
pp. 472-478 ◽  
Author(s):  
Xueqing Qiu ◽  
Weimei Zeng ◽  
Wanshan Liang ◽  
Yuyuan Xue ◽  
Nanlong Hong ◽  
...  

2005 ◽  
Vol 25 (4) ◽  
pp. 193-210 ◽  
Author(s):  
Ryo Moriyama ◽  
Shohei Takeda ◽  
Masaki Onozaki ◽  
Yukuo Katayama

Sign in / Sign up

Export Citation Format

Share Document