Structural Features of Welded Joint of Medium-Carbon Chromium Steel Containing Metastable Austenite

2020 ◽  
Vol 11 (1) ◽  
pp. 132-139
Author(s):  
Yu. S. Korobov ◽  
O. V. Pimenova ◽  
M. A. Filippov ◽  
M. S. Khadyev ◽  
N. N. Ozerets ◽  
...  
Author(s):  
A. S. Atamashkin ◽  
E. Yu. Priymak ◽  
N. V. Firsova

The paper presents an analysis of the mechanical behavior of friction samples of welded joints from steels 30G2 (36 Mn 5) and 40 KhN (40Ni Cr 6), made by rotary friction welding (RFW). The influence of various temperature conditions of postweld tempering on the mechanical properties and deformation behavior during uniaxial tensile testing is analyzed. Vulnerabilities where crack nucleation and propagation occurred in specimens with a welded joint were identified. It was found that with this combination of steels, postweld tempering of the welded joint contributes to a decrease in the integral strength characteristics under conditions of static tension along with a significant decrease in the relative longitudinal deformation of the tested samples.


Author(s):  
Kiyoshi NARIHIRO ◽  
Yasuo OTOGURO ◽  
Takashi ŌTSUBO ◽  
Noboru MIIDA
Keyword(s):  

1972 ◽  
Vol 58 (3) ◽  
pp. 411-422
Author(s):  
Kiyoshi NARIHIRO ◽  
Yasuo OTOGURO ◽  
Takashi OTSUBO ◽  
Noboru MIIDA
Keyword(s):  

2020 ◽  
Vol 790 ◽  
pp. 139717
Author(s):  
Wei Zhang ◽  
Tianyu Zhang ◽  
Xiaowei Wang ◽  
Yunnan Ji ◽  
Jianming Gong

Metals ◽  
2020 ◽  
Vol 10 (4) ◽  
pp. 522 ◽  
Author(s):  
Petro Loboda ◽  
Constantine Zvorykin ◽  
Volodymyr Zvorykin ◽  
Eduard Vrzhyzhevskyi ◽  
Tatjana Taranova ◽  
...  

In this article, structural features of Ti-TiB and (α+β) Ti alloys in the initial state, in the weld and in the heat-affected zone of electron beam welds were investigated. The influences of welding parameters, such as influence of the electron beam velocity, preheating of the welded alloys and the subsequent annealing of the welded joint on the its microstructure, and the mechanical strength and ductility of the critical elements of the joint were studied by scanning electron microscopy using microprobe Auger spectral and X-ray diffraction analysis and tensile tests. It has been shown that the conditions for rapid crystallization of the material from the melt of the weld contribute to refining of reinforcing fibers of TiB and its hardening in comparison with the starting material Ti-TiB. Besides that, influences of the preferential orientation of TiB reinforcing microfibers (along and across the welded butt joint) on the mechanical properties of the welded joint were investigated bz tensile testing. Using the methods of fractographic analysis, the effect of the boron-containing phase on the fracture character of Ti-TiB welded joints was established. It was shown that, along with the strengthening effect, TiB fibers cause embrittlement of the material.


2015 ◽  
Vol 3 (3) ◽  
pp. 49-54
Author(s):  
Devpriyo Ghosh ◽  
Sarthak Nangia ◽  
Sourav Chakravarty ◽  
Sharwin Maben ◽  
Satya Shankar Sharma

Metals ◽  
2020 ◽  
Vol 10 (6) ◽  
pp. 738
Author(s):  
Yuan Liu ◽  
Yan Han ◽  
Sheng Yin ◽  
Fei Zhao

In the present study, quenching and partitioning (Q & P) treatment of a medium-carbon silicon-rich steel was processed by a dilatometer. The volume fraction of the retained austenite at different partitioning times was determined by X-ray diffraction (XRD). The metastable austenite transformation process after different partitioning times was studied by a combination of dilatometry, XRD, and transmission electron microscopy (TEM). Analysis of the transformation kinetics of metastable austenite during partitioning by means of dilatometry and the Johnson–Mehl–Avrami–Kolmogorov (JMAK) equation was carried out. The results show that the volume fraction of retained austenite increases first and then decreases with the increase of the partitioning time. The transformation active energy Q = 141 kJ·mol−1 and the Avrami exponent n = 1. The transformation product of metastable austenite is needle-like bainite, which grows perpendicularly towards the boundary of the austenite. Finally, the blocky austenite was divided into lath-shaped forms.


Author(s):  
D.Q.Q. Wang ◽  
D.D. Yao ◽  
Z.B. Gao ◽  
Q. Wang ◽  
Z.F. Zhang ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document