ABSTRACTWe have previously shown that 25nm thick gold stripes on 1mm thick silicone membrane retain electrical conduction when stretched up to 100% along their long dimension. To function as electrical interconnects in conformable integrated circuits, the metallization must be stretchable in arbitrary directions. Therefore we have made and tested the mechanical and electrical properties of complex conductor patterns including X and Y oriented lines and cross junctions. We find that the metal patterns continue to conduct under uniaxial stretching in the X or Y direction and under radial, biaxial stretching.


2011 ◽  
Vol 31 (1) ◽  
Author(s):  
Masao Takashige ◽  
Toshitaka Kanai

Abstract There are two different stretching processes that produce the biaxially oriented film, namely the tenter process and double bubble tubular film process. Furthermore, there are two tenter processes, i.e., the sequential biaxial stretching process and simultaneous biaxial stretching process. There is no report describing the difference among film physical properties of the three different processes. The biaxially oriented polyamide film using the double bubble tubular process has good balanced physical property and high impact strength, thus it is used for proper applications utilizing their advantage properties. In this report, the influence of each biaxial stretching process on film physical properties of polyamide, which has hydrogen bond, was studied in detail. As a result, the tentering process film has anisotropic tensile properties between machine direction (MD) and transverse direction (TD). This result was influenced by a later stretching process, namely TD stretching. On the contrary, the double bubble tubular film has good balanced properties, especially thermal shrinkage and impact strength. Tentering simultaneous stretching film has much larger shrinkage in MD than in TD. The sequential stretching film has larger shrinkage in TD than in MD. The double bubble tubular film has high impact strength, because it corresponds to the balanced molecular orientation.


Materials ◽  
2018 ◽  
Vol 11 (11) ◽  
pp. 2292 ◽  
Author(s):  
Yoshinori Hashimoto ◽  
Shotaro Nishitsuji ◽  
Takashi Kurose ◽  
Hiroshi Ito

This work reports on an experimental study of the stretching of ultra-high molecular weight polyethylene (UHMWPE) film in various uniaxial/biaxial stretching modes at various temperatures and stretching speeds. We examined the stress-birefringence relationship as a stress-optical rule (SOR) under uniaxial stretching and evaluated the stress-optical coefficient (SOC). Wide-angle X-ray diffraction (WAXD) measurements were applied to evaluate the contribution to birefringence of the crystalline and amorphous phases and to characterize stretching modes. In simultaneous biaxial stretching, the melting temperature (Tm) proved critical to structural formation. We applied thermal analysis techniques and tensile testing to evaluate higher order structures after each stretching mode.