The effect of two-frequency low-cycle loading on the fatigue life of steels and welded joints

1995 ◽  
Vol 27 (1-2) ◽  
pp. 82-87
Author(s):  
K. Kálna
Materials ◽  
2021 ◽  
Vol 14 (9) ◽  
pp. 2331
Author(s):  
Yixun Wang ◽  
Yuxiao Luo ◽  
Yuki Kotani ◽  
Seiichiro Tsutsumi

The authors wish to revise in the text of Appendix A, pages 19–21 [...]


Materials ◽  
2021 ◽  
Vol 14 (5) ◽  
pp. 1249
Author(s):  
Yixun Wang ◽  
Yuxiao Luo ◽  
Yuki Kotani ◽  
Seiichiro Tsutsumi

The existing S-N curves by effective notch stress to assess the fatigue life of gusset welded joints can result in reduced accuracy due to the oversimplification of bead geometries. The present work proposes the parametric formulae of stress concentration factor (SCF) for as-welded gusset joints based on the spline model, by which the effective notch stress can be accurately calculated for fatigue resistance assessment. The spline model is also modified to make it applicable to the additional weld. The fatigue resistance of as-welded and additional-welded specimens is assessed considering the geometric effects and weld profiles. The results show that the error of SCFs by the proposed formulae is proven to be smaller than 5%. The additional weld can increase the fatigue life by as great as 9.4 times, mainly because the increasing weld toe radius and weld leg length lead to the smaller SCF. The proposed series of S-N curves, considering different SCFs, can be used to assess the welded joints with various geometric parameters and weld profiles.


2014 ◽  
Vol 49 (3) ◽  
pp. 290-301 ◽  
Author(s):  
I. A. Volkov ◽  
Yu. G. Korotkikh
Keyword(s):  

2017 ◽  
Vol 743 ◽  
pp. 264-268 ◽  
Author(s):  
Anastasia Smirnova ◽  
Yury Pochivalov ◽  
Victor Panin ◽  
Anatoly Orishich ◽  
Aleksandr Malikov ◽  
...  

The structure and mechanical properties of welded joints of VT23 titanium alloy received by method of laser welding after modifying the surface layers by ultrasonic mechanical forging (Treatment 1 and Treatment 2) were investigated. The experimental tests have revealed that the Treatment 2 provides a multiple increase in the relaxation property in fatigue life test. The formation of nonuniform distribution of vanadium, chromium and molybdenum in the welded joint increases the strength and, at the same time, the brittleness of β-phase. Mechanical treatment of the surface layers in the second mode provides a multiple increase in ductility up to 13%, in the as-received condition up to 9.9%. In consequence of plastic deformation, the β-phase intensity reduces twice with Treatment 2 which is related to its clustering. As follows from a presented data, the fatigue life of the VT23 titanium alloy has increased more than threefold.


2018 ◽  
Vol 157 ◽  
pp. 05013 ◽  
Author(s):  
Peter Kopas ◽  
Milan Sága ◽  
František Nový ◽  
Bohuš Leitner

The article presents the results of research on low cycle fatigue strength of laser welded joints vs. non-welded material of high-strength steel DOMEX 700 MC. The tests were performed under load controlled using the total strain amplitude ɛac. The operating principle of the special electro-mechanic fatigue testing equipment with a suitable clamping system was working on 35 Hz frequency. Fatigue life analysis was conducted based on the Manson-Coffin-Basquin equation, which made it possible to determine fatigue parameters. Studies have shown differences in the fatigue life of original specimens and laser welded joints analysed, where laser welded joints showed lower fatigue resistance. In this article a numerical analysis of stresses generated in bending fatigue specimens has been performed employing the commercially available FEM-program ADINA.


2003 ◽  
Author(s):  
Tomohiro Hirata ◽  
Toshiaki Nakamaru ◽  
Keisuke Toyama ◽  
Shuichi Magara ◽  
Hiroshi Watanabe ◽  
...  