Effect of High-Temperature Treatment on Carbon-Carbon Composite Material X-Ray Structural Properties and Thermal Conductivity

2013 ◽  
Vol 54 (4) ◽  
pp. 319-323 ◽  
Author(s):  
M. Yu. Bamborin ◽  
D. V. Yartsev ◽  
S. A. Kolesnikov
1998 ◽  
Vol 547 ◽  
Author(s):  
J.-H. Park ◽  
P.M. Woodward ◽  
J.B. Parise ◽  
I. Lubomirsky ◽  
O. Stafsudd

AbstractA new perovskite was recovered from the high pressure-high temperature treatment of the α-TlSbO3 form of Na2SnTeO6 at 7 GPa and 950 °C for 30 minutes. Synchrotron x-ray powder diffraction data show the space group is P21/n with a=5.40361 (5), b=5.46152(5), c=7.69288(7) Å and ß=90.034(3)°. Using disk samples of both polymorphs, the dielectric properties were measured as a function of temperature. At ambient conditions, the perovskite form has a more than 1.5 fold enhancement in dielectric constant compared to the α-TlSbO3 form while the molar volume and the molecular polarizability decrease.


RSC Advances ◽  
2019 ◽  
Vol 9 (32) ◽  
pp. 18333-18343 ◽  
Author(s):  
Fei Ma ◽  
Shaolan Ding ◽  
Huijun Ren ◽  
Piaolin Peng

A chromium oxide-carbon composite material was formed by the high-temperature carbonization of chromium-tanned leather shavings, followed by the leaching of chrome oxide and activation by KOH.