The crystallization and dielectric properties of SrO–BaO–Nb2O5–GeO2 glass–ceramics were investigated. One- and two-stage heat-treatment methods were used to convert the parent glass to glass–ceramics. Strontium barium niobate (SBN) with a tetragonal tungsten-bronze structure formed as the major crystalline phase. When the crystallizing temperature/time was increased, the secondary crystalline BaGe2O5 phase coexisted with SBN. BaGe2O5 formed as a surface layer grown from the surface into the interior of the sample. The dendritic morphology of SBN crystals was examined. The glass–ceramics crystallized by two-stage heat treatment have higher dielectric constants than those crystallized by one-stage heat treatment. The highest dielectric constant that was obtained in the present glass–ceramics was 320. The glass–ceramics showed relaxor-type dielectric behavior.


2018 ◽  
Vol 43 (1-4) ◽  
pp. 10-19
Author(s):  
Lei Han ◽  
Jun Song ◽  
Taoyong Liu ◽  
Yu Tang ◽  
Zhiwei Luo ◽  
...  

2010 ◽  
Vol 92 ◽  
pp. 65-71 ◽  
Author(s):  
Pei Xin Zhang ◽  
Li Gao ◽  
Qiu Hua Yuan ◽  
Hai Lin Peng ◽  
Xiang Zhong Ren ◽  
...  

The glass-ceramics of MgO-Al2O3-SiO2 system were prepared by sintering technology. The crystallization process of MgO-Al2O3-SiO2 glass-ceramics was investigated with X-ray diffraction (XRD), scanning electron microscopy (SEM), and other techniques; the discussion of breaking strength, thermal expansion coefficient and relevant properties at different sintering temperatures was also presented. The results show that: (1) The main crystalline phase isα-cordierite at different sintering temperatures, and the samples show high flexural strength and low thermal expansion coefficient; (2) with the increase of sintering temperature, the content of crystal phase increases, while the thermal expansion coefficient decreases evidently, the flexural strength and tightness density rise up first, then go down.