Influence of the sliding velocity and the applied potential on the corrosion and wear behavior of HC CoCrMo biomedical alloy in simulated body fluids

2011 ◽  
Vol 4 (8) ◽  
pp. 2090-2102 ◽  
Author(s):  
Roberto Alonso Gil ◽  
Anna Igual Muñoz
2016 ◽  
Vol 25 (9) ◽  
pp. 095024 ◽  
Author(s):  
F Stergioudi ◽  
C A Vogiatzis ◽  
E Pavlidou ◽  
S Skolianos ◽  
N Michailidis

2005 ◽  
Vol 475-479 ◽  
pp. 2333-2336 ◽  
Author(s):  
Kyosuke Ueda ◽  
Takayuki Narushima ◽  
Chiaki Ouchi ◽  
Yasutaka Iguchi

Wear behavior of titanium materials such as C.P.Ti, Ti-6Al-4V and Ti-6Al-7Nb, was studied in simulated body fluids by means of the pin-on-disk type wear testing. The mass loss in wear testing increased with increasing the sliding distance. The a+b type titanium alloys, Ti-6Al-4V and Ti-6Al-7Nb, exhibited higher wear resistance than the C.P.Ti. Average size of the wear debris was 4.5 µm and 3.7 µm for C.P.Ti and the a+b type titanium alloys, respectively. The elution of metallic constituents into 1 mass% lactic acid solution was detected after the wear test.


2016 ◽  
Vol 57 (12) ◽  
pp. 2054-2059
Author(s):  
Kyosuke Ueda ◽  
Motoka Kasamatsu ◽  
Masanori Tanno ◽  
Kosuke Ueki ◽  
Jean Geringer ◽  
...  

2020 ◽  
Vol 22 (4) ◽  
pp. 1031-1046
Author(s):  
X. Canute ◽  
M. C. Majumder

AbstractThe need for development of high temperature wear resistant composite materials with superior mechanical properties and tribological properties is increasing significantly. The high temperature wear properties of aluminium boron carbide composites was evaluated in this investigation. The effect of load, sliding velocity, temperature and reinforcement percentage on wear rate was determined by the pin heating method using pin heating arrangement. The size and structure of base alloy particles change considerably with an increase of boron carbide particles. The wettability and interface bonding between the matrix and reinforcement enhanced by the addition of potassium flurotitanate. ANOVA technique was used to study the effect of input parameters on wear rate. The investigation reveals that the load had higher significance than sliding velocity, temperature and weight fraction. The pin surface was studied with a high-resolution scanning electron microscope. Regression analysis revealed an extensive association between control parameters and response. The developed composites can be used in the production of automobile parts requiring high wear, frictional and thermal resistance.


2020 ◽  
Author(s):  
Eshani Hettiarachchi ◽  
◽  
Shaylene Paul ◽  
Shaylene Paul ◽  
Milton Das ◽  
...  

CrystEngComm ◽  
2021 ◽  
Author(s):  
Shuqin Jiang ◽  
Yuanyuan Cao ◽  
Chenxi Zong ◽  
Yuanfeng Pang ◽  
Zhiwen Sun

The regulation effect of Mg2+ on HAP crystallization is closely related to the adding time of Mg2+. The introduction of Mg2+ in the ACP unstable stage is unable to inhibit HAP crystallization.