Influence of welding process on Type IV cracking behavior of P91 steel

2014 ◽  
Vol 613 ◽  
pp. 148-158 ◽  
Author(s):  
M. Divya ◽  
C.R. Das ◽  
S.K. Albert ◽  
Sunil Goyal ◽  
P. Ganesh ◽  
...  
Author(s):  
Nick Bagshaw ◽  
Chris Punshon ◽  
John Rothwell

Boiler and steam piping components in power plants are fabricated using creep strength enhanced ferritic (CSEF) steels, which often operate at temperatures above 550°C. Modification of alloy content within these steels has produced better creep performance and higher operating temperatures, which increases the process efficiency of power plants. The improved materials, however, are susceptible to type IV cracking at the welded regions. A better understanding of type IV cracking in these materials is required and is the basis of the Technology Strategy Board (TSB) UK funded VALID (Verified Approaches to Life Management & Improved Design of High Temperature Steels for Advanced Steam Plants) project. In order to study the relationship between creep performance and heat input during welding, several welds with varying amounts of heat input and resultant HAZ widths were produced using the electron beam welding process. The welding parameters were developed with the aid of weld process modeling using the finite element (FE) method, in which the welding parameters were optimized to produce low, medium and high heat input welds. In this paper, the modeling approach and the development of electron beam welds in ASTM A387 grade P92 pipe material are presented. Creep specimens were extracted from the welded pipes and testing is ongoing. The authors acknowledge the VALID project partners, contributors and funding body: Air Liquide, Metrode, Polysoude, E.ON New Build & Technology Ltd, UKE.ON, Doosan, Centrica Energy, SSE, Tenaris, TU Chemnitz, The University of Nottingham, The Open University and UK TSB. Paper published with permission.


2005 ◽  
Vol 10 (2) ◽  
pp. 149-157 ◽  
Author(s):  
S. K. Albert ◽  
M. Tabuchi ◽  
H. Hongo ◽  
T. Watanabe ◽  
K. Kubo ◽  
...  

2012 ◽  
Vol 552 ◽  
pp. 493-501 ◽  
Author(s):  
Wang Xue ◽  
Qian-gang Pan ◽  
Yao-yao Ren ◽  
Wei Shang ◽  
Hui-qiang Zeng ◽  
...  

Author(s):  
N. Yoneyama ◽  
K. Kubushiro ◽  
H. Yoshizawa

9Cr steel weldments are concerned with evaluation of creep life time and creep rupture mechanism. In fine grain HAZ (FG-HAZ) of weldments, TYPE IV cracking and creep voids occurred at lower stress than rupture stress level of base metal. In the crept specimen, FG-HAZ sometime has large coarsening grains near creep voids. These recovery phenomena are localized in FG-HAZ, and recovered microstructures are dependent on heat input of welding. In this study, creep tests are examined in two types of weldments, and relations between creep life time and coarsened sub-grains or grains have been studied by microstructural changing with EBSP analysis. In crept specimens, boundaries are moved and boundary density is decreasing in the fine-grained HAZ. Maximum grain size and creep life time have linear function, and EBSP can evaluate creep life time of 9Cr weldments. These microstructural changing are considered by morphology of precipitates in the several crept specimens.


Metals ◽  
2020 ◽  
Vol 10 (10) ◽  
pp. 1285 ◽  
Author(s):  
Kai Yang ◽  
Yingjie Zhang ◽  
Jianping Zhao

P91 steel is a typical steel used in the manufacture of boilers in ultra-supercritical power plants and heat exchangers in nuclear power plants. For the long-term serviced P91 steel pressurized structures, the main failure mode is the welded joint failure, especially the heat affected zone (HAZ) failure. Repair welding technique is an effective method for repairing such local defects. However, the thermal shock composed of high temperature and thermal stress in the repair welding process will pose a critical loading condition for the existing defects near the heat source which cannot be detected by conventional means. So, the evaluation of structural integrity for the welded joint in the thermal-mechanical coupling field is necessary. In this work, the crack propagation law in the HAZ for the P91 steel welded joint was investigated under repair welding thermal loads. The weld repair model of the P91 steel welded joint was established by ABAQUS. The transient temperature field and stress field in repair welding process were calculated by relevant user subroutines and sequential coupling simulation method. The residual stress was determined by the impact indentation strain method to verify the feasibility of the finite element (FE) model and simulation method. In order to obtain the crack propagation path, the elastoplastic fracture analysis of the welded joint with initial crack was performed based on the extended finite element method (XFEM). The influence of different welding linear energy on the crack propagation was analyzed. The results show that the cracks in the HAZ propagate perpendicular to the surface and tend to deflect to the welding seam under repair welding thermal loads. The crack propagation occurs in the early stage of cooling. Higher welding linear energy leads to larger HAZ and higher overall temperature. With the increase of welding linear energy, the length and critical distance of the crack propagation increase. Therefore, low welding linear energy can effectively inhibit the crack propagation in the HAZ. The above calculation and analysis provide a reference for the thermal shock damage analysis of repair welding process, which is of great significance to improving the safety and reliability of weld repaired components.


2019 ◽  
Vol 795 ◽  
pp. 416-423
Author(s):  
Ze Xun Hu ◽  
Jian Ping Zhao ◽  
Ying Jie Zhang

The type IV cracking is one of the main reasons for service failure. The repair welding is implemented to solve this problem. The residual stress in P91 repair welding incorporating martensitic transformation (MT) is acquired through finite element simulation. In the simulation, the ABAQUS and the user subroutines FILM, DFLUX, HETVAL, USDFLD, UEXPAN and UHARD are adopted. The effect of MT latent heat on temperature and the effects of the volume expansion, the yield strength change and the transformation plasticity on stress are considered. The results show that there is full MT in the repair welding area and the old welding area. The MT latent heat makes the temperature of the repair welding area increase. The residual stress of the repair welding area decreases because MT relieves the thermal stress. Before repair welding, the residual stress distribution is M-shape, which is consistent with the experimental results. After repair welding, the residual stress of repair welding area decreases and the residual stress of old welding area increases.