scholarly journals Relationships between properties and rapid gas decompression (RGD) resistance of various filled nitrile butadiene rubber vulcanizates under high-pressure hydrogen

2021 ◽  
pp. 103038
Author(s):  
Sang Koo Jeon ◽  
Oh Heon Kwon ◽  
Nae Hyung Tak ◽  
Nak Kwan Chung ◽  
Un Bong Baek ◽  
...  
2019 ◽  
Vol 9 (1) ◽  
Author(s):  
Jae Kap Jung ◽  
Sang Koo Jeon ◽  
Kyu-Tae Kim ◽  
Chang Hoon Lee ◽  
Un Bong Baek ◽  
...  

Abstract Nondestructive impedance spectroscopy (IS) was developed and demonstrated to detect the effects of hydrogen on nitrile butadiene rubber exposed to hydrogen gas (H2) at high pressures up to 10 MPa. IS was applied to obtain an in situ and real-time quantification of H2 penetration into and its desorption out of rubber under high pressure. The diffusion coefficients of H2 were also obtained from the time evolution of the capacitance, which were compared with those obtained by thermal desorption gas analysis. The in situ measurements of the capacitance and the dissipation factor under various pressures during cyclic stepwise pressurization and decompression demonstrated the diffusion behaviour of H2, the phase of the rubber under high pressure, the transport properties of H2 gas, and the physicochemical interaction between H2 and the rubber. These phenomena were supported by a COMSOL simulation based on the electric current conservation equation and scanning electron microscopy (SEM) observations.


2020 ◽  
Vol 35 (2) ◽  
pp. 221-228
Author(s):  
S.-B. Chen ◽  
T.-X. Li ◽  
S.-H. Wan ◽  
X. Huang ◽  
S.-W. Cai ◽  
...  

2020 ◽  
Vol 26 (2) ◽  
pp. 62-69
Author(s):  
Farida Ali ◽  
Tuti I. Sari ◽  
Andi A. Siahaan ◽  
Al-Kautsar D. Arya ◽  
Tri Susanto

Penelitian ini untuk mengetahui pengaruh penambahan Natural Rubber (NR) dan Epoxidation Natural Rubber (ENR-46) dengan kompatibiliser Chlorprene Rubber (CR) pada aplikasi kompon termoplastik Poly Vinyl Chloride (PVC) dan Nitrile Butadiene Rubber (NBR), variabel penelitian meliputi ENR-46/PVC/NBR/CR, NR/PVC/NBR/CR dan CR-NR/PVC/NBR, CR-ENR-46/PVC/NBR. Parameter pengujian sifat fisik-mekanik : Hardness (Shore A), Tensile Strength (Mpa), Elongation at Break (%) dan ketahanan terhadap pelarut minyak (n-Pentane, Toluene, Hexane dan Pertalite). Hasil penelitian didapatkan untuk sifat fisik-mekanik, semakin banyak penambahan NR Kekerasan kompon termoplastik akan menurun, Tensile Strength dan Elongation at Break kompon akan meningkat begitu juga dengan CR-NR. Tetapi berbanding terbalik hasilnya untuk ENR-46 dan CR-ENR-46. Pengujian Ketahanan terhadap pelarut minyak semakin banyak penambahan ENR-46 Ketahanan kompon termoplastik terhadap pelarut akan meningkat, hasil yang sama juga pada CR-ENR-46. Tetapi berbanding terbalik hasilnya dengan penambahan NR dan CR-NR pada kompon termoplastik.