scholarly journals WITHDRAWN: Preparation of nano α-Al2O3 particles with optimum conditions by the sol–gel method

Author(s):  
R.S. Dariani ◽  
S. Emami
2010 ◽  
Vol 150-151 ◽  
pp. 1325-1329
Author(s):  
Jian Fei Liu ◽  
Zhi Wang ◽  
Yin Sen Ding ◽  
Guo Pu Shi

The composites of Fe/Al2O3 gradient coatings on steel substrate were prepared by spraying and sol-gel method, and the microstructure and performances of the composites were analyzed. The results show that the adhesion strength of Fe/Al2O3 gradient coatings with FeAlNi transitional layers reaches 25.3MPa when the sintering temperature is 1220°C, and the surface hardness of coatings is four times higher than that of steel substrate. The coatings are mainly composed of α-Al2O3, AlFeO3 and NiFe2O4. There is no obvious hole or macro-interface, while some organization similar to the branch appears in the coatings. The bonding of Fe/Al2O3 gradient coatings and steel substrate mainly depends on adsorption, diffusion and chemical combination.


2015 ◽  
Vol 19 (sup2) ◽  
pp. S2-2-S2-9
Author(s):  
Z. Chen ◽  
B. X. Zhu ◽  
J. M. Li ◽  
J. H. Chen ◽  
J. Tao

2021 ◽  
Vol 4 (1) ◽  
pp. 65-73
Author(s):  
Siti Rodiah ◽  
Mifta Huljana ◽  
Jauharuddin Luthfi Al Jabbar ◽  
Chairul Ichsan ◽  
Hasan Marzuki

One of the heavy metals contained in the textile industry wastewater is chromium (Cr). Chromium hexavalent ions (Cr6+) are highly toxic and its accumulation in the human body will cause various negative impacts. This study aimed to determine the characteristics of silica synthesized by the sol-gel method to gain homogeneity and high purity. Synthesized silica was calcined at 700°C for 4 hours and its performance to adsorb Cr(VI) ions  in textile wastewater was investigated. The presence of -OH group from silanol (–Si-OH) was appeared at wavenumber 3367.70 cm-1, meanwhile siloxane functional groups were recorded at 1056.99 cm-1 and 784.38 cm-1 due to the O-Si-O asymmetric stretching and Si-O bending vibration. Optimum conditions of silica to adsorb Cr(VI) ions took place at pH 2 and contact time of 90 minutes by adsorption efficiency of 75,65% and followed the Freundlich isotherm.


NANO ◽  
2011 ◽  
Vol 06 (06) ◽  
pp. 575-581 ◽  
Author(s):  
FAEZEH NIKANJAM ◽  
RASOUL SARRAF-MAMOORY ◽  
NASTARAN RIAHI-NOORI

Lithium fluoride (LiF) nanopowders were prepared by trifluoroacetate-based sol–gel processing. In this work, lithium acetate dehydrate ( LiAc ⋅ 2H2O ) and trifluoroacetic acid (TFA) was used as lithium and fluorine sources. The thermal behavior of initial gel was examined using differential thermal analysis (DTA). Effects of solvent (glacial acetic acid, absolute ethanol, and ethylene glycol), Li+ concentration (0.5, 1, and 2 mol/l) and decomposition temperature (200, 250, and 300°C) on synthesis of LiF nanopowders by sol–gel method were investigated. The results of LPSA, FE-SEM, and XRD showed that the growth of particles and aggregation can be controlled by changing above parameters. However, it is indicated that optimum conditions are; solvent as ethanol, Li ion concentration (0.5 mol/l), and decomposition temperature (300°C), respectively. Also, the addition of oleic acid as an organic additive made the final LiF particles finer and about 70–90 nm.


2014 ◽  
Vol 29 (8) ◽  
pp. 807
Author(s):  
WANG Min ◽  
NIU Chao ◽  
DONG Zhan-Jun ◽  
CHE Yin-Sheng ◽  
DONG Duo ◽  
...  

2011 ◽  
Vol 10 (2) ◽  
pp. 187-192 ◽  
Author(s):  
Ramona-Crina Suciu ◽  
Marcela Corina Rosu ◽  
Teofil Danut Silipas ◽  
Emil Indrea ◽  
Violeta Popescu ◽  
...  

Author(s):  
Dong XU ◽  
Qi SONG ◽  
Ke ZHANG ◽  
Hong-Xing XU ◽  
Yong-Tao YANG ◽  
...  
Keyword(s):  
Sol Gel ◽  

Sign in / Sign up

Export Citation Format

Share Document