Optimization of sulfurization time and temperature for fabrication of Cu2ZnSnS4 (CZTS) thin films

2019 ◽  
Vol 126 ◽  
pp. 32-41 ◽  
Author(s):  
M.A. Olgar
2011 ◽  
Vol 418-420 ◽  
pp. 67-71 ◽  
Author(s):  
Xin Yi Li ◽  
Da Chen Wang ◽  
Qin Yang Du ◽  
Wei Feng Liu ◽  
Guo Shun Jiang ◽  
...  

CZTS thin films are fabricated by sulfurizing co-sputtered metallic precursor CuZnSn layers under H2S atmosphere. The precursor layers are Cu-poor, Zn-rich deposited and the fabricated films are about 2 µm in thickness. A closed-tube process is preferred with regard to its producing large closely pack grains with smooth surface. XRD and Raman confirm the CZTS structure and the impurities on the surface are removed after suitable chemistry treatments. The band gap of the CZTS is determined to be 1.48 eV by extrapolation. Some more CZTS films are product with slightly changed parameters, sulfurization time, temperature and concentration of H2S, respectively. It is supposed that beside sulfurization time, the temperature could be more significant than concentration of H2S in the closed system.


2013 ◽  
Vol 818 ◽  
pp. 3-8 ◽  
Author(s):  
Min Xie ◽  
Da Ming Zhuang ◽  
Ming Zhao ◽  
Bo Jian Li ◽  
Jun Song

CZTS thin films were fabricated through sulfurization of sputtered alloy precursors. The properties of CZTS films obtained at sulfurization time of less than 2 hours and at H2S concentrations of higher than 15% were investigated. Sulfurization time of 30 min, 60 min and 90 min and H2S concentrations of 20%, 40% and 60% have been chosen for the sulfurization process. It has been found that Cu poor and slightly Zn rich CZTS films can be obtained at all of those sulfurization time and H2S concentrations. Changing the sulfurization time or H2S concentrations wont change the compositions of sulfurized films. Minor SnS coexist with the dominate CZTS although the films are Zn rich and the distributions of Sn and S along the depth of the films are uniform. The films sulfurized at H2S concentration of 20% have the biggest grain size of exceeding 2 μm and obvious columnar CZTS grains can be observed across the whole cross-section.


Author(s):  
Wenbin Hao ◽  
Jinze Li ◽  
Wei Li ◽  
Jiansheng Zhao ◽  
Jianfeng Chen

2021 ◽  
Vol 134 ◽  
pp. 105943
Author(s):  
Jiao Wang ◽  
Yanping Wang ◽  
Haoran Li ◽  
Aimei Zhao ◽  
Bing Li ◽  
...  

2020 ◽  
Vol 146 ◽  
pp. 106669 ◽  
Author(s):  
M.A. Olgar ◽  
A. Seyhan ◽  
A.O. Sarp ◽  
R. Zan
Keyword(s):  

2013 ◽  
Vol 24 (8) ◽  
pp. 2667-2671 ◽  
Author(s):  
Hao Guan ◽  
Honglie Shen ◽  
Chao Gao ◽  
Xiancong He