Effects of thickness and cycle parameters on fretting wear behavior of CVD diamond coatings on steel substrates

2010 ◽  
Vol 205 (1) ◽  
pp. 158-167 ◽  
Author(s):  
Qiuping Wei ◽  
Z.M. Yu ◽  
Michael N.R. Ashfold ◽  
Z. Chen ◽  
L. Wang ◽  
...  
2009 ◽  
Vol 47 (9-12) ◽  
pp. 919-922 ◽  
Author(s):  
Eckart Uhlmann ◽  
Stefan Rosiwal ◽  
Katharina Bayerlein ◽  
Markus Röhner

2018 ◽  
Vol 190 ◽  
pp. 14008 ◽  
Author(s):  
Markus Prieske ◽  
Richard Börner ◽  
Andreas Schubert

forming tool coating. Most of the forming tools are made of steel, so that especially the coatability of steel by a polycrystalline diamond coating would rise the range of fields of application. The polycrystalline CVD-diamond coatings are deposited by a laser induced plasma CVD process, without a vacuum chamber. Various surface microstructures were investigated regarding their influence on the residual stresses to prevent a flaking of the coating: on the one hand, deterministic structures generated by ultrasonic vibration assisted milling (UVAM) and on the other hand, stochastic structures manufactured by blasting and polishing processes. For the UVAM, a surface prediction tool was used to design the surface microstructure beforehand. All steel substrates (material no. 1.2379) were coated in one batch by high-power impulse magnetron sputtering with a chromium nitride coating with a thickness of 2.4 μm. The specimens were analysed by laser microscopy, scanning electron microscopy, energy-dispersive X-ray spectroscopy and Raman spectroscopy. None of the microstructures investigated in this study was able to prevent delamination of the coating entirely. It could be shown that a roughness higher than Sa 0.1μm supports the interlocking between coating and surface as well as that sharp peaks inhibit a homogenous diamond coating deposition.


Materials ◽  
2021 ◽  
Vol 14 (9) ◽  
pp. 2153
Author(s):  
Tengfei Zhang ◽  
Jie Su ◽  
Yuanjie Shu ◽  
Fei Shen ◽  
Liaoliang Ke

Rubbers are widely used in various fields as the important sealing materials, such as window seal, door seal, valve, pump seal, etc. The fretting wear behavior of rubbers has an important effect on their sealing performance. This paper presents an experimental study on the fretting wear behavior of rubbers against the steel ball under air conditions (room temperature at 20 ± 2 °C and humidity at 40%). Three kinds of rubbers, including EPDM (ethylene propylene diene monomer), FPM (fluororubber), and NBR (nitrile–butadiene rubber), are considered in experiments. The sphere-on-flat contact pattern is used as the contact model. The influences of the displacement amplitude, normal force, frequency, and rubber hardness on the fretting wear behavior are discussed in detail. White light profiler and scanning electron microscope (SEM) are used to analyze the wear mechanism of the rubber surface. The fretting wear performances of three rubbers are compared by considering the effect of the displacement amplitude, normal force, frequency, and rubber hardness. The results show that NBR has the most stable friction coefficient and the best wear resistance among the three rubbers.


2002 ◽  
Vol 11 (3) ◽  
pp. 288-293 ◽  
Author(s):  
Gui-Zhen Xu ◽  
Jia-Jun Liu ◽  
Zhong-Rong Zhou

1996 ◽  
Vol 47 (7) ◽  
pp. 611-615
Author(s):  
Hiroyuki TANAKA ◽  
Toshiaki TANAKA ◽  
Hideaki SOHMA ◽  
Masato YOSHIDA ◽  
Akira SAKAI ◽  
...  

Wear ◽  
2015 ◽  
Vol 338-339 ◽  
pp. 252-257 ◽  
Author(s):  
Jae Yong Yun ◽  
Gyeong Su Shin ◽  
Dae Il Kim ◽  
Ho Sik Lee ◽  
Woong Soon Kang ◽  
...  

2012 ◽  
Vol 48 ◽  
pp. 162-171 ◽  
Author(s):  
M.X. Shen ◽  
M.H. Zhu ◽  
Z.B. Cai ◽  
X.Y. Xie ◽  
K.C. Zuo

2019 ◽  
Vol 141 (10) ◽  
Author(s):  
Mengjiao Wang ◽  
Yunxia Wang ◽  
Jianzhang Wang ◽  
Na Fan ◽  
Fengyuan Yan

Super duplex stainless steel (SDSS) has excellent mechanical properties and corrosion resistance. However, currently, there are few researches conducted on its fretting wear performance. This paper studies the influence of different heat treatment temperatures and medium environment on the fretting wear performance of SAF 2507 SDSS. Results show that the combined effect of the sigma phase and seawater lubrication can significantly improve the wear resistance of SAF 2507 SDSS. After treated with different heat treatment temperatures, different contents of sigma phases are precipitated out of SAF 2507 SDSS, which improves the wear resistance of the material to different degrees. In addition, the fretting wear performance of SAF 2507 SDSS also relates to the lubrication medium. In air, the friction and wear performance of SAF 2507 SDSS is poor, while in seawater, solution and corrosion products that acted as a lubricant dramatically improve the wear resistance of the material. Under the combined action of heat treatment and seawater lubrication medium, the friction coefficient and wear reduce by 70% and 91%, respectively.