Rail dark spot defect, also termed squat failure or shelling, which is a kind of rolling contact fatigue failure and occurs frequently on running surfaces of railway rails carrying high speed traffic, is one of the most dangerous rail failures. The dark spot crack is characterized by a principal crack propagating in the direction of traffic and a second crack growing in the direction opposite to traffic. By using a newly developed two-disk machine, the authors have succeeded in reproducing very similar dark spot cracks to those which appear in actual rails. It is found that the dark spot defects are caused by frequent repetitions of dry and wet runnings, and that the traction force plays an important role for the occurrence of the cracks. The principal crack may occur from a tiny pit formed a posteriori on the contacting surface and after that, the second crack is formed by cracks branched from the extended principal crack. It has also been proved experimentally that water is capable of entering the tip of the crack. Furthermore, a possible mechanism for the dark spot cracking has been proposed on the basis of the fracture mechanics approach.


2011 ◽  
Vol 217-218 ◽  
pp. 866-873 ◽  
Author(s):  
Katsuyuki Kida

Previous researchers investigated the failures of ball surfaces of silicon nitride bearings from the viewpoint of the ring crack model. They explained the process of flaking failures in terms of surface semi-circular cracks which grew by the stresses around the circumference of the contact circle. However, contrary to their explanation, we found that the ring crack model did not explain the process of the flaking failure of plates. In the present work we compare the growth directions of surface and subsurface cracks in order to find out which crack is more dominant in the process of the flaking failure. We carried out reciprocating-rolling contact fatigue (RCF) tests and concluded that the directions of arcs formed by the semi-circular surface cracks were dominated by subsurface crack growth direction.


Author(s):  
John W. Lucek

Rolling-contact fatigue test methods were used to measure the wear performance of several silicon nitride materials. Sintered, hot pressed and hot isostatically pressed materials exhibited wear rates ranging over three orders of magnitude. Hot isostatically pressed materials had the lowest wear rates. Despite the disparity in wear performance, all materials tested had useful rolling-contact fatigue lives compared to steel. Fatigue life estimates, failure modes, and rolling wear performance for theses ceramics are compared to M-50 steel. This work highlights the rapid contact stress reductions that occur due to conformal wear in rolling-contact fatigue testing. Candidate bearing materials with unacceptably high wear rates may exhibit useful fatigue lives. Rolling contact bearing materials must possess useful wear and fatigue resistance. Proper performance screening of candidate bearing materials must describe the failure mode, wear rate, and the fatigue life. Guidelines for fatigue testing methods are proposed.


Author(s):  
Gerald E. Arnold

Ball or roller bearings have much in common with a railway wheel running on a rail. Both have high Hertzian stresses and are subject to rolling contact fatigue. Silicone Nitride (Si3N4), a Technical Ceramic, has now firmly established itself in the engineering marketplace as part of a hybrid bearing, where the rolling elements are silicone nitride and the races are steel. The paper explores the possibility of a Silicon Nitride/steel wheel/rail combination and finds that, because Silicon Nitride has a higher Modulus of Elasticity, it is not suitable as a direct replacement on existing systems, because it would produce a smaller contact patch and greater contact stress. The low toughness of Silicon Nitride in comparison to steel could be an obstacle to its general railway use, however, it could made into a composite material in the same manner as Carbon Reinforced Silicon Carbide (C/SiC) is used in brake discs. There is a possibility that, under the right conditions, Silicon Nitride could return very low wear rates, because of its extreme hardness, and because it’s excellent resistance to rolling contact fatigue (noted in hybrid bearings). This could give a wheel high mileage, without the need to remove fatigued material by controlled wear or by turning. A promising future application for the material is a cable-hauled system, where the predicted lower adhesion between Silicon Nitride and a steel rail is not a problem and the wheels are not required to be conductive.