scholarly journals Use of fly ash from fluidized bed boilers in clinker-slag-ash based binders

2018 ◽  
Vol 174 ◽  
pp. 02002
Author(s):  
Elżbieta Janowska-Renkas ◽  
Jolanta Kowalska

The study presents the state of knowledge regarding physical and chemical properties, as well as trends for application of fly ashes from combustion in fluidized bed boilers in building materials. Clinker - slag - ash based binders were tested that contained up to 40 mass % of fly ashes from combustion in fluidized bed boilers. It was demonstrated that fluidized bed combustion fly ashes (FBC fly ash), apart from granular blast furnace slag, could be the ingredient of low clinker Portland cements (ca. 20% by mass). These cements, compared to CEM I Portland cement, have higher water demand and durability in the corrosive environment, and a lower compressive strength value. Based on test results of binders with various content of blast furnace slag and fly ash, the clinker - slag - ash based binder was singled out, which demonstrated the higher durability in the corrosive environment. It was found that production of clinker - slag - ash based binders was possible in the strength class 32.5 even with 30% by mass of FBC fly ash content.

2019 ◽  
Vol 25 (3) ◽  
pp. 340-347
Author(s):  
Ting WANG ◽  
Xiaojian GAO ◽  
Jian WANG

As a byproduct of phosphoric acid industry, phosphogypsum has many environmental problems. In order to recycle phosphogypsum to manufacture lightweight building materials, cementitious additives including fly ash, ground granulate blast-furnace slag and Portland cement were added to improve strength and water-resistance and different volume of foam was added to reduce the bulk density. The results show that hydrated lime can improve mechanical strength and water resistance of PG paste and the optimal dosage of hydrated lime is 6 %. Higher addition of fly ash or ground granulated blast-furnace slag improves the fluidity and delays the setting time of PG paste. The addition of 10 ~ 20 % fly ash results in a little reducing influence and 10 % ground granulated blast-furnace slag leads to an increase of 20.7 % for 28 days compressive strength of hardened PG specimen. The higher addition of Portland cement results in the better mechanical strength and water resistance of PG specimens. The 28day compressive and flexural strength reaches 25.9 MPa and 8.9 MPa respectively for the 25 % Portland cement mixture. PG based lightweight building materials can prepared by the addition of 60 % volume of air foam, with compressive strength of 1.7 MPa, bulk density of 521.7 kg/m3 and thermal conductivity of 0.0724 W/(m·K). DOI: http://dx.doi.org/10.5755/j01.ms.25.3.19910


Crystals ◽  
2021 ◽  
Vol 11 (6) ◽  
pp. 596
Author(s):  
Yasuhiro Dosho

To improve the application of low-quality aggregates in structural concrete, this study investigated the effect of multi-purpose mineral admixtures, such as fly ash and ground granulated blast-furnace slag, on the performance of concrete. Accordingly, the primary performance of low-quality recycled aggregate concrete could be improved by varying the replacement ratio of the recycled aggregate and using appropriate mineral admixtures such as fly ash and ground granulated blast-furnace slag. The results show the potential for the use of low-quality aggregate in structural concrete.


2014 ◽  
Vol 1052 ◽  
pp. 392-395 ◽  
Author(s):  
Li Xia He

High Ti-bearing blast furnace (BF) slag is the smelting waste of vanadium titano-magnetite. It has great production but low utilization. The high Ti-bearing BF slag is used in building materials industry, which recycles waste material, saves resources and energy, benefiting environmental protection and achieving sustainable development of resources. Study on the recycling of high Ti-bearing BF slag will be an important subject of our researches in future.


2014 ◽  
Vol 629-630 ◽  
pp. 371-375
Author(s):  
Ji Wei Cai ◽  
Si Jia Yan ◽  
Gong Lei Wei ◽  
Lu Wang ◽  
Jin Jin Zhou

Fly ash (FA) and granular blast-furnace slag (GBFS) are usual mineral admixtures to conventional concrete, and their contents substituted for Portland cement definitely affect development rate of strength of concrete. C30 and C60 concrete samples with FA and/or GBFS were prepared to study the influence of substitution content of the mineral admixtures on 3 d, 7 d and 28 d strength. The results reveal that the development rate of strength in period from 3 d to 7 d gets slow with increasing content of mineral admixtures except for concrete with only GBFS less than 20%. In the case of substituting FA as the only mineral admixture for part of cement, the development rate of strength of C30 concrete in period from 7 d to 28 d keeps roughly constant even that of C60 concrete increases. When substituting mineral admixtures in the presence of GBFS for cement within experimental range, the development rate of strength in period from 7 d to 28 d gets fast with increasing substitution content. The enhancing effect of combining FA and GBFS occurs in period from 7 d to 28 d for both C30 and C60 concretes (FA+GBFS≤40%), even occurs in period from 3 d to 7 d for C60 concrete. Based on 7 d strength and the development rate, 28 d strength of concrete can be predicted accurately.


2017 ◽  
Vol 865 ◽  
pp. 282-288 ◽  
Author(s):  
Jul Endawati ◽  
Rochaeti ◽  
R. Utami

In recent years, sustainability and environmental effect of concrete became the main concern. Substituting cement with the other cementitious material without decreasing mechanical properties of a mixture could save energy, reduce greenhouse effect due to mining, calcination and limestone refining. Therefore, some industrial by-products such as fly ash, silica fume, and Ground Iron Blast Furnace Slag (GIBFS) would be used in this study to substitute cement and aggregate. This substitution would be applied on the porous concrete mixture to minimize the environmental effect. Slag performance will be optimized by trying out variations of fly ash, silica fume, and slag as cement substitution material in mortar mixture. The result is narrowed into two types of substitution. First, reviewed from the fly ash substitution effect on binder material, highest compressive strength 16.2 MPa was obtained from mixture composition 6% fly ash, 3% silica fume and 17% grinding granular blast-furnace slag. Second, reviewed from slag types as cement substitution and silica fume substitution, highest compressive strength 15.2 MPa was obtained from mortar specimens with air-cooled blast furnace slag. It composed with binder material 56% Portland composite cement, 15% fly ash, 3% silica fume and 26% air-cooled blast furnace slag. Considering the cement substitution, the latter mixture was chosen.