Laboratory Research on Fatty Acid Based Biobinder as an Addition for Crumb Rubber Modified Asphalt

Author(s):  
Jiayun Zhang ◽  
Gang Xu ◽  
Minghui Gong ◽  
Jun Yang
Environments ◽  
2021 ◽  
Vol 8 (6) ◽  
pp. 47
Author(s):  
Lim Min Khiong ◽  
Md. Safiuddin ◽  
Mohammad Abdul Mannan ◽  
Resdiansyah

This paper presents the results of a laboratory-based experimental investigation on the properties of asphalt binder and hot-mix asphalt (HMA) mixes modified by locally available crumb rubber, which was used as a partial replacement of asphalt by weight. In this study, fine crumb rubber with a particle size in the range of 0.3–0.6 mm, obtained from scrap tires, was added to the asphalt binder through the wet process. Crumb rubber contents of 5%, 10%, 15%, and 19% by weight of asphalt were added to the virgin binder in order to prepare the modified asphalt binder samples, while the unmodified asphalt binder was used as the control sample. The crumb rubber modified binder samples were examined for measuring viscosity indirectly using the penetration test, and temperature resistance using the softening point test. Later, both the modified and unmodified asphalt binders were used to produce HMA mixes. Two categories of HMA mix commonly used in Malaysia—namely, AC 14 (dense-graded) and SMA 14 (gap-graded)—were produced using the modified asphalt binders containing 5%, 10%, 15%, and 19% crumb rubber. Two AC 14 and SMA 14 control mixes were also produced, incorporating the unmodified asphalt binder (0% crumb rubber). All of the AC 14 and SMA 14 asphalt mixes were examined in order to determine their volumetric properties, such as bulk density, voids in total mix (VTM), voids in mineral aggregate (VMA), and voids filled with asphalt (VFA). In addition, the Marshall stability, Marshall flow, and stiffness of all of the AC 14 and SMA 14 mixes were determined. Test results indicated that the modified asphalt binders possessed higher viscosity and temperature resistance than the unmodified asphalt binder. The viscosity and temperature resistance of the asphalt binders increased with the increase in their crumb rubber content. The increased crumb rubber content also led to improvements in the volumetric properties (bulk density, VTM, VMA, and VFA) of the AC 14 and SMA 14 mixes. In addition, the performance characteristics of the AC 14 and SMA 14 mixes—such as Marshall stability, Marshall flow, and stiffness—increased with the increase in crumb rubber content. However, the AC 14 mixes performed much better than the SMA 14 mixes. The overall research findings suggest that crumb rubber can be used to produce durable and sustainable HMA mixes, with manifold environmental benefits, for use in flexible pavements carrying the heavy traffic load of highways.


2020 ◽  
Vol 259 ◽  
pp. 119662 ◽  
Author(s):  
Israel Rodríguez-Fernández ◽  
Farrokh Tarpoudi Baheri ◽  
Maria Chiara Cavalli ◽  
Lily D. Poulikakos ◽  
Moises Bueno

2004 ◽  
Vol 16 (1) ◽  
pp. 45-53 ◽  
Author(s):  
S. K. Palit ◽  
K. Sudhakar Reddy ◽  
B. B. Pandey

2012 ◽  
Vol 204-208 ◽  
pp. 3899-3904
Author(s):  
Lan Yun Chen ◽  
Qing Long You ◽  
Xin Qiu

In order to study the effects of different factors on the performance of crumb rubber modified asphalt, on the basis of many laboratory tests, this article analyzed such factors as types of crumb rubber, fineness, content, mixing temperature and matrix asphalt. Results show that mixed with the crumb rubber, pavement performance of the asphalt has been improved to varying degree. In the engineering application of rubber asphalt, it is suggested that the 20 mesh crumb rubber modified asphalt of truck tire be adopted, with about 16% to 18% of crumb rubber content at about 175°C. As for matrix asphalt, it should be selected according to the different climatic conditions and the mechanical characteristics of the pavement.