scholarly journals Experimental Investigation on the Ecofriendly External Wrapping of Glass Fiber Reinforced Polymer in Concrete Columns

2021 ◽  
Vol 2021 ◽  
pp. 1-12
Author(s):  
D. S. Vijayan ◽  
A. Mohan ◽  
J. Jebasingh Daniel ◽  
V. Gokulnath ◽  
B. Saravanan ◽  
...  

An ecofriendly fiber reinforced polymer (FRP) had been used in the last decade to enhance the short concrete column’s strength and deformation capacity. This study involves the wrapping of FRP sheets with a thickness of 3 mm and 5 mm on a short column, and then the compressive strength is determined. The rectangular columns of size 150 mm × 300 mm are used for this study, and cast under the grades of M20 and M40 are wrapped with GFRP sheets at the thickness of 3 mm and 5 mm. These results are clarified at a specific thickness of the FRP-wrapped columns. It provides a maximum axial compressive strength, and Young’s modulus gets enhanced rigorously when it is to be compared to the normal concrete. This thesis deals with experimental studies of different parameters associated with wrapped glass fiber reinforced polymer (GFRP). In M20 grade, when the 3 mm wrapped specimen and the 5 mm wrapped specimen are compared, the specimen wrapped with 5 mm increases 5.182% more than the specimen wrapped with 3 mm. In M40 grade, when the 0 mm, 3 mm, and 5 mm wrapped specimens are compared, the specimen wrapped with 5 mm increases 2.47% more than the specimen wrapped with 0 mm. The 5 mm wrapping attains the maximum strength.

Author(s):  
Ashkan Farazin ◽  
Afrasyab Khan

Fiber-reinforced polymer-based composites may experience various strain rates under different dynamic loads. As the mechanical behavior of these composites varies with strain rate, their response will be dependent on the strain rate. This paper presents a comprehensive review on glass fibers and composites reinforced with these fibers, as the most practical polymer-based composite, under dynamic loading. First, the properties of long glass fibers under different strain rates will be reviewed in detail. In the following, experimental studies on the effects of strain rate on various types of glass fiber-reinforced polymer-based composites will be categorized and presented. The behavior of thermoset polymers will be also addressed under different strain rates. Finally, various analytical and numerical macromechanical and micromechanical models will be comprehensively described for this type of composites.


2019 ◽  
Vol 10 (4) ◽  
pp. 510-538 ◽  
Author(s):  
Mohamed Abdel-Kader ◽  
Ahmed Fouda

In this article, the response of nine plain concrete panels to an impact of hard projectiles was examined in an experimental study. The tests were planned with an aim to observe the influence of compressive strength on the performance of concrete under impact loading. Concrete panels with compressive strengths within the range of 26 to 92 MPa subjected to impact by 23 mm hard projectile at velocities within the range of 270 to 348 m/s were studied. Also, using a glass fiber reinforced polymer sheet, as a liner on the rear face of the plain concrete panel, to strengthen the panel was examined. The experimental results indicate that strengthening concrete panel with a rear glass fiber reinforced polymer sheet showed more satisfactory performance under the impact load than increasing compressive strength of concrete. Also, the use of glass fiber reinforced polymer sheets as rear liners in addition to increasing the concrete strength showed superior performance of concrete panels against impact; it is recommended to be used in protective structures.


1994 ◽  
Vol 116 (3) ◽  
pp. 167-172 ◽  
Author(s):  
P. K. Dutta

Polymeric composites are relatively inexpensive materials of high strength, in which deformation of the matrix is used to transfer stress by means of shear traction at the fiber-matrix interface to the embedded high-strength fibers. At low temperatures, complex stresses are set up within the microstructure of the material as a result of matrix stiffening and mismatch of thermal expansion coefficients of the constituents of the composites. These stresses in turn affect the strength and deformation characteristics of the composites. This is demonstrated by compression testing of an unidirectional glass-fiber-reinforced polymer composite at room and low temperatures. The increase of compressive strength matched the analytical prediction of strength increase modeled from the consideration of increase in matrix stiffness and thermal residual stresses at low temperatures. Additional compression tests performed on a batch of low-temperature thermally cycled specimens confirmed the predictable reduction of brittleness due to suspected increase of microcrack density. The mode of failure characterized by definite pre-fracture yielding conforms more to Budiansky’s plastic microbuckling theory than to Rosen’s theory of elastic shear or extensional buckling.


2021 ◽  
Vol 68 (1) ◽  
Author(s):  
Mohamed S. Moawad ◽  
Ahmed Fawzi

AbstractOne of the major advantages of using glass fiber-reinforced polymer bars as a replacement to the traditional steel-reinforced bars is its lightweight and high-resistant to corrosion. This research focuses on the performance of concrete beams partially/fully reinforced with glass fiber-reinforced polymer bars with 50% of GFRP bars were used to reinforce partially concrete beams at flexural zone. While 100% of GFRP bars were used to reinforce fully concrete beams at flexural and compression zones with different concrete compressive strength.This study reported the test results of 6 reinforced concrete beams with dimensions 150 × 200mm and a 1700-mm clear span length subjected to a four-point loading system. The tested beams were divided into three groups; the first one refers to the glass fiber-reinforced polymer bar effect. The second group is referring to the effect of concrete compressive strength, while the third group is referring to the effect of the GFRP bar volume ratio.Using longitudinal GFRP bars as a full or partial replacement of longitudinal steel bar reinforcement led to an increase in the failure load capacity and the average crack width, while a decrease in ductility was reported with a lower number of cracks. Increasing the concrete compressive strength is more compatible with GFRP bar reinforcement and enhanced the failure performance of beams compared with normal compressive strength concrete.


Machines ◽  
2021 ◽  
Vol 9 (1) ◽  
pp. 16
Author(s):  
Gabriel Mansour ◽  
Panagiotis Kyratsis ◽  
Apostolos Korlos ◽  
Dimitrios Tzetzis

There are numerous engineering applications where Glass Fiber Reinforced Polymer (GFRP) composite tubes are utilized, such as desalination plants, power transmission systems, and paper mill, as well as marine, industries. Some type of machining is required for those various applications either for joining or fitting procedures. Machining of GFRP has certain difficulties that may damage the tube itself because of fiber delamination and pull out, as well as matrix deboning. Additionally, short machining tool life may be encountered while the formation of powder like chips maybe relatively hazardous. The present paper investigates the effect of process parameters for surface roughness of glass fiber-reinforced polymer composite pipes manufactured using the filament winding process. Experiments were conducted based on the high-speed turning Computer Numerical Control (CNC) machine using Poly-Crystalline Diamond (PCD) tool. The process parameters considered were cutting speed, feed, and depth of cut. Mathematical models for the surface roughness were developed based on the experimental results, and Analysis of Variance (ANOVA) has been performed with a confidence level of 95% for validation of the models.