Effects of Various Antioxidant Pretreatment Modalities on Adhesion to Sound and Caries-Affected Dentin: An In Vitro Study

2021 ◽  
pp. 232020682199798
Author(s):  
Beyza Unalan Degirmenci ◽  
Alperen Degirmenci ◽  
Emine Kara

Aim: Natural antioxidants were offered as the answer of dentin adhesion issue. The aim of this study is to investigate the effects of proanthocyanidin and lycopene as pretreatment agents on the sound and caries-affected dentin surface on microtensile bond strength and microleakage. Materials and Methods: This study was designed as in vitro because of that 84 mandibular molar teeth were collected. Forty-two of the included teeth were carious teeth, while the other 42 were without caries. Sixty of them were used for microleakage and 24 for microtensile bond strength testing and scanning electron microscopy analysis. The samples were divided into six subgroups randomly according to dentin pretreatments: 5% proanthocyanidin, 5% lycopene, and no antioxidant application. After the restorative procedures, samples were attached to the microtensile tester. Samples were subjected to tensile stress in the load cell until they broke at a speed of 0.5 mm per min. Microtensile bond strength (µTBS) and microleakage test data were analyzed with two-way analysis of variance, Bonferroni correction, and Tamhane’s T2 tests. Results: Two-way variance analysis showed that dentin pretreatment applications, dentin substrate, and the interaction between these two parameters had statistically significant effects on µTBS values ( P < .001). There was no difference between dentin pretreatment applications in terms of microleakage scores ( P > .05). Conclusion: The application of dentin pretreatment with proanthocyanidin is a successful procedure that increases the bond strength in both dentin substrate, while pretreatment with lycopene in caries-affected dentin reduces it.

2020 ◽  
Vol 8 (10) ◽  
pp. 454-459
Author(s):  
Bhalla V. ◽  
◽  
K. Goud M. ◽  
Chockattu S. ◽  
Khera A ◽  
...  

Background:Dentin bonding is an ever-evolving field in adhesive dentistry. With the introduction of newer systems into the market, there is a crucial need to test their efficiency in terms of bond strength. Dual-cured adhesives in theory may provide for a better degree of conversion as compared to conventional light-cured adhesives .Thus, the aim of this study was to compare the shear bond strength of three different self-etch adhesives namely ClearfilSE bond (Kuraray), Tetric N Bond Universal (IvoclarVivadent) and Futura Bond DC (Voco) to dentin. Materials & Methods: Ninety extracted non-carious, intact human mandibular molar teeth were selected for this study. Each tooth was decoronated using a double-sided diamond disc with water coolant to a depth of 2mm from the cusp tip .The cut dentin surface was then abraded against 600-grit wet silicon carbide papers for 60 seconds to produce a uniform smear layer. The root portion of each tooth was mounted on a plastic ring using cold cure acrylic resin. Specimens were then divided into three adhesive groups of 30 teeth each, Group A: ClearfilSE Bond (Kuraray), Group B: Tetric N Bond Universal (IvoclarVivadent), Group C :Futura Bond DC (Voco). All bonding agents were used according to the manufacturers’ instructions, in combination with the resin composite Tetric N Ceram (IvoclarVivadent). The samples were thermocycled, followed by shear bond strength testing using a Universal testing machine (Hounsfield). Data were subjected to statistical analysis using one-way analysis of variance (ANOVA) (P<0.05) and Post hoc Tukey’s test for inter- and intra- group analysis respectively. Results: Clearfil SE Bond yielded the highest shear bond strength values (30.9 ±4.66 MPa) which were statistically significant, followed byTetric N Bond Universal group (29.8 ±4.34) and the lowest shear bond strength values were recorded for Futura Bond DC (18.2 ±3.13). Conclusion: Clearfil SE bond and Tetric N bond Universal can be considered as better options than Futura Bond DC.


2014 ◽  
Vol 50 ◽  
pp. 228-234 ◽  
Author(s):  
Thiago Henrique Scarabello Stape ◽  
Murilo de Sousa Menezes ◽  
Flávio Henrique Baggio Aguiar ◽  
Paulo Sérgio Quagliatto ◽  
Carlos José Soares ◽  
...  

Author(s):  
Masoud Fallahinejad Ghajari ◽  
Mahsa Sheikholeslamian ◽  
Amir Ghasemi ◽  
Leila Simaei

Objectives: This study aimed to determine the microtensile bond strength (μTBS) of a bulk-fill composite to permanent and primary coronal dentin using a universal adhesive in self-etch and total-etch modes. Materials and Methods: This in-vitro study was performed on 52 occlusal dentinal surfaces of human primary and permanent teeth. The crowns were cut to the gingival level. The 48 prepared dentin sections were randomly assigned to the following groups (n=13): A: Primary/Total-etch, B: Primary/Self-etch, C: Permanent/Total-etch, and D: Permanent/Self-etch. In groups A and C, after etching for 15 seconds, two layers of a universal bonding (Futurabond U) were applied and cured for 10 seconds. All samples were filled with a bulk-fill composite (x-trafil; VOCO) and cured for 40 seconds. The samples were cut to a bar-shaped dentin block with the dimensions of 1×1×1 mm3, and after 10,000 thermocycles, the μTBS test was accomplished at a crosshead speed of 1 mm/minute. The mean and standard deviation (SD) of μTBS were calculated, and the data were analyzed using two-way analysis of variance (ANOVA) and Fisher's exact test. Results: The mean μTBS was as follows: A: 15.03±2.0279, B: 11.11±2.4423, C: 23.50±4.8165, and D: 16.26±6.3200 MPa. Futurabond U showed a higher μTBS in the total-etch mode (P<0.001). The permanent teeth had greater μTBS than the primary teeth (P<0.001). Similar percentages of failure modes were observed in the total-etch groups but in the self-etch groups, most failures were in the form of adhesive and mixed. Conclusion: Greater μTBS was observed in the permanent teeth with the total-etch technique.


2014 ◽  
Vol 02 (02) ◽  
pp. 091-095
Author(s):  
Veerendra Uppin ◽  
Priyanka Sarangi ◽  
Sukanta Satapathy

AbstractAn in-vitro evaluation was done to compare shear bond strength of four self etching primer adhesives to dentin. 75 human extracted molar teeth were selected. The occlusal surface of these teeth was ground to remove coronal enamel and expose dentin. The dentinal surface of each tooth was then abraded using series of silicon carbide (320, 400, 600 grit) abrasive paper. Teeth were divided into 5 groups of 15 teeth each and composite post were then built on the bonded surfaces using Z-100 hybrid composite. The teeth were then fractured applying shearing load through universal testing machine. Shear strength values were in the range of 15.96 to 22.64 Mpa. Clearfil S3 gave highest mean shear bond strength whereasAdhe SE gave lowest value of shear strength. Based on this study it could be concluded that contemporary self etching primer adhesives bond successfully to dentin and also their bonding ability seems to be comparable to conventional total etch system.