scholarly journals Influence of Light Source, Thermocycling and Silane on the Shear Bond Strength of Metallic Brackets to Ceramic

2015 ◽  
Vol 26 (6) ◽  
pp. 685-688 ◽  
Author(s):  
Hugo Franco de Abreu Neto ◽  
Ana Rosa Costa ◽  
Américo Bortolazzo Correr ◽  
Silvia Amélia Vedovello ◽  
Heloísa Cristina Valdrighi ◽  
...  

The objective of this study was to evaluate the effects of different light sources, thermocycling and silane on the bond strength of metallic brackets to ceramic. Cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 60 s. Half of the cylinders (Groups 1 to 4) received two layers of silane. Metallic brackets were bonded to the cylinders using Transbond XT and divided into 8 groups (n=20), according to light source (Radii Plus LED - 40 s; Groups 1, 2, 5 and 6 and XL 2500 halogen light - 40 s; Groups 3, 4, 7 and 8) and experimental conditions with (Groups 2, 4, 6 and 8) without thermocycling (Groups 1, 3, 5 and 7). Shear bond testing was carried out after 24 h of deionized water storage (Groups 1, 3, 5 and 7) and thermocycling (Groups 2, 4, 6 and 8; 7,000 cycles - 5°/55 °C). Date were submitted to three-way ANOVA and Tukey's post hoc test (α=0.05). The Adhesive Remnamt Index (ARI) was evaluated at 8× magnification. The application of silane was effective in increasing the shear bond strength of the brackets to ceramic (p<0.05). Significant difference (p<0.05) on the bond strength was observed between light sources with or without thermocycling. The ARI showed a predominance of scores 0 for all groups, with an increase in scores 1, 2 and 3 for the silane groups. In conclusion, silane improved significantly the shear bond strength of the brackets to ceramic. The thermocycling and light sources influence on the bond strength.

2011 ◽  
Vol 22 (6) ◽  
pp. 486-489 ◽  
Author(s):  
Ana Rosa Costa ◽  
Américo Bortolazzo Correr ◽  
Regina Maria Puppin-Rontani ◽  
Silvia Amélia Scudeler Vedovello ◽  
Heloísa Cristina Valdrighi ◽  
...  

This study evaluated the effects of thermocycling and different light sources on the bond strength of metallic brackets to bovine tooth enamel using an adhesive resin. Bovine teeth were etched with 35% phosphoric acid gel for 20 s. After application of primer, metallic brackets were bonded to the buccal surface using Transbond XT, forming 8 groups (n=20), depending on the light source used for photoactivation (AccuCure 3000 argon laser - 20 s, Apollo 95E plasma arc - 12 s, UltraLume 5 LED - 40 s and XL2500 halogen light - 40 s) and experimental conditions without (Groups 1 to 4) or with thermocycling (Groups 5 to 8). Shear bond testing was carried out after 24 h of distilled water storage (Groups 1 to 4) or storage and thermocycling in distilled water (groups 5 to 8; 1,500 cycles - 5o/55oC). Data were subjected to two-way ANOVA and Tukey’s test (α=0.05). The Adhesive Remnant Index (ARI) was evaluated at ×8 magnification. No significant differences (p>0.05) in bond strength were found when the conditions without and with thermocycling were compared for any of the light sources. No significant differences (p>0.05) in bond strength were found among the light sources, irrespective of performing or not thermocycling. There was a predominance of ARI scores 1 in all groups. In conclusion, light sources and thermocycling had no influence on the bond strength of brackets to bovine enamel.


2011 ◽  
Vol 36 (5) ◽  
pp. 492-501 ◽  
Author(s):  
B Stawarczyk ◽  
R Hartmann ◽  
L Hartmann ◽  
M Roos ◽  
M Özcan ◽  
...  

SUMMARY This study tested the impact of Gluma Desensitizer on the shear bond strength (SBS) of two conventional (RelyX ARC, Panavia 21) and two self-adhesive (RelyX Unicem, G-Cem) resin luting cements after water storage and thermocycling. Human third molars (N=880) were embedded in acrylic resin. The buccal dentin was exposed. Teeth were randomly divided into four main groups, and the following cements were adhered: 1) RelyX ARC, 2) Panavia 21, 3) RelyX Unicem, and 4) G-Cem. In half of the teeth in each group, dentin was treated with Gluma Desensitizer. In the conventional cement groups, the corresponding etchant and adhesive systems were applied. SBS of the cements was tested after 1 hour (initial); at 1, 4, 9, 16, and 25 days of water storage; and at 1, 4, 9, 16, and 25 days of thermocycling. SBS data were analyzed by one-way analysis of variance (ANOVA); this was followed by the post hoc Scheffé test and a t-test. Overall, the highest mean SBS (MPa) was obtained by RelyX ARC (ranging from 14.6 ± 3.9 to 17.6 ± 5.2) and the lowest by Panavia 21 in combination with Gluma Desensitizer (ranging from 0.0 to 2.9 ± 1.0). All tested groups with and without desensitizer showed no significant decrease after aging conditions compared with baseline values (p&gt;0.05). Only the Panavia 21/Gluma Desensitizer combination showed a significant decrease after 4 days of thermocyling compared with initial values and 1 day thermocycling. Self-adhesive cements with Gluma Desensitizer showed increased SBS after aging conditions (ranging from 7.4 ± 1.4 to 15.2 ± 3) compared with groups without desensitizer (ranging from 2.6 ± 1.2 to 8.8 ± 2.9). No cohesive failures in dentin were observed in any of the test groups. Although self-adhesive cements with and without desensitizer presented mainly adhesive failures after water storage (95.8%) and thermocyling (100%), conventional cement (RelyX ARC) showed mainly mixed failures (90.8% and 89.2%, after water storage and thermocyling, respectively). Application of the Gluma Desensitizer to dentin before cementation had a positive effect on the SBS of self-adhesive cements.


2007 ◽  
Vol 77 (4) ◽  
pp. 701-706 ◽  
Author(s):  
Rodney G. Northrup ◽  
David W. Berzins ◽  
Thomas Gerard Bradley ◽  
William Schuckit

Abstract Objective: To evaluate and compare the shear bond strengths of two adhesives using two types of brackets: a conventional and a self-ligating bracket system. Materials and Methods: Sixty extracted human premolars were collected. The premolars were randomly divided into three groups of 20 teeth. All three groups were direct bonded. Groups 1 and 2 used light-cured adhesive and primer (Transbond XT) with a conventional (Orthos) and a self-ligating bracket (Damon 2), respectively. Group 3 used a light-cured primer (Orthosolo) and a light-cured adhesive (Blūgloo) with a self-ligating bracket (Damon 2). The specimens were stored in distilled water at 37°C for 40 ± 2 hours, after which they were debonded and inspected for Adhesive Remnant Index (ARI) scoring. Results: The mean shear bond strength was 15.2 MPa for group 1, 23.2 MPa for group 2, and 24.8 MPa for group 3. A one-way analysis of variance and post hoc Tukey test showed significant differences in bond strength (P &lt; .001) between group 1 and groups 2 and 3 but no significant difference (P &gt; .05) between groups 2 and 3. A Weibull analysis demonstrated that all three groups provided sufficient bond strength with over 90% survival rate at normal masticatory and orthodontic force levels. A Kruskal-Wallis test showed no significant difference (P &gt; .05) in ARI scores among all three groups. Conclusions: All three groups demonstrated clinically acceptable bond strength. The Damon 2 self-ligating bracket exhibited satisfactory in vitro bond strength with both adhesive systems used.


2016 ◽  
Vol 27 (6) ◽  
pp. 734-738 ◽  
Author(s):  
Natália Regina Santos de Matos ◽  
Ana Rosa Costa ◽  
Heloísa Cristina Valdrighi ◽  
Américo Bortolazzo Correr ◽  
Silvia Amélia Vedovello ◽  
...  

Abstract The aim of this study was to evaluate the effect of silanes, thermal cycling and acid etching on the shear bond strength (SBS) of metallic brackets to feldspathic ceramic. Feldspathic ceramic cylinders (Groups 1, 2, 5 and 6) were etched for 60 s with 10% hydrofluoric acid and Groups 3, 4, 7 and 8, without acid etching. Two layers of silane Clearfil Ceramic Primer (CCP, Groups 1 to 4) and two layers of RelyX Ceramic Primer (RCP, groups 5 to 8) were applied and dried for 60 s. Brackets were bonded to the cylinders with Transbond XT and light-activated for 40 s with Bluephase G2. All specimens were stored in deionized water at 37 °C for 24 h, and the specimens of groups 1, 3, 5 and 7 were submitted to 7,000 thermal cycles (5 °C/55 °C). After storage, the SBS test was performed at a crosshead speed of 1 mm/min. Data were subjected to three-way ANOVA and Tukey's post hoc test (α=0.05). The adhesive remnant index (ARI) was evaluated at 8x magnification. The SBS of CCP was significantly greater than of RCP (p<0.05), with or without thermal cycling. Thermal cycling significantly reduced the SBS (p<0.05). The groups submitted to acid etching showed significantly higher SBS than those without acid etching (p<0.05). In conclusion, thermal cycling reduced SBS for all groups. The best ceramic surface treatment for bracket bonding was achieved by acid etching and CCP silane. The ARI results showed predominance of score 0 for all groups.


2013 ◽  
Vol 18 (6) ◽  
pp. 112-116
Author(s):  
Sergio Luiz Mota Júnior ◽  
Márcio José da Silva Campos ◽  
Marco Abdo Gravina ◽  
Marcelo Reis Fraga ◽  
Robert Willer Farinazzo Vitral

OBJECTIVE: development of a new device to be coupled to light-curing units for bonding orthodontic brackets and accessories, and test its efficacy in an in vitro mechanical trial. The inner surface of the device is mirrored and is based on physical concepts of light refraction and reflection. The main advantage of such device is the reduced clinical time needed for bonding and the low possibility of contamination during the process. METHODS: One hundred and twenty specimens were used for testing the shear bond strength of brackets bonded with the device. The Adhesive Remnant Index (ARI) was also determined. The sample was divided into 2 groups. In group 1 a halogen light-curing unit was used while in group 2 a led light-curing unit was used. Each group was then subdivided. In subgroups H1 and L1, a conventional light guide rod was used while in subgroups H2 and L2 bonding was performed with the mirrored device coupled to the tip of the guide light rod. RESULTS: The values obtained for the shear bond strength and the ARI in the subgroups were compared. Results showed that there was no statistically significant difference for the shear strength (p > 0.05) and the ARI (p > 0.05) between the subgroups. CONCLUSION: The tests of mechanical trials and the ARI analysis showed that the new device fulfilled the requirements for bonding orthodontic accessories, and that the time for bonding was reduced to half, being necessary only one light exposure.


2017 ◽  
Vol 46 (3) ◽  
pp. 179-183
Author(s):  
Fernando Guerra SÁEZ ◽  
Ana Rosa COSTA ◽  
Adriana Simoni LUCATO ◽  
Ana Paula Terossi de GODOI ◽  
Lourenço CORRER-SOBRINHO ◽  
...  

Abstract Objective To evaluate in vitro the effect of different treatments of the ceramic surface and thermal cycling on the shear bond strength (SBS) of metallic brackets bonded to feldspathic ceramic. Material and method Ceramic cylinders were divided into four groups (n=4) according to the treatment of ceramic surface: G1-Clearfil Ceramic Primer silane and Transbond XT (CCPT); G2-etched with 10% hydrofluoric acid (HFA) for 60 s, CCP and Transbond XT (ACCPT); G3-etched with 10% HFA for 60 s, Ambar Adhesive and Transbond XT (AAAT); and, G4 - etched with 10% HFA for 60 s, RelyX Ceramic Primer silane -RCP, adhesive primer Transbond and Transbond XT (ACPPT). Brackets were bonded to the cylinders with Transbond XT and light-activated for 40 s with LED Radii Plus. All specimens were stored in deionized water at 37 °C for 24 h, and two cylinders from each group were subject to 7,000 thermal cycles in a thermal cycler (5 °C/55 °C). After storage and thermal cycling, the SBS test was performed at a crosshead speed of 1 mm/min. Data were subjected to two-way ANOVA and Tukey’s post hoc test (α=0.05). Result The SBS of ACCPT was significantly higher than the other groups (p<0.05). The specimens submitted to thermal cycling showed significantly lower SBS than those without thermal cycling (p<0.05), regardless the ceramic surface treatment. The ARI showed predominance of score 0 for all groups. Conclusion Acid etching, CCP silane and Transbond XT method obtained the best results for bracket bonding. Thermal cycling reduced SBS for all groups. Score 0 was predominant for ARI in all groups.


2020 ◽  
Vol 31 (1) ◽  
pp. 52-56
Author(s):  
Gustavo Vallandro Lopes ◽  
Lourenço Correr-Sobrinho ◽  
Américo Bortolazzo Correr ◽  
Ana Paula Terossi de Godoi ◽  
Silvia Amélia Scudeler Vedovello ◽  
...  

Abstract The present study was evaluated the effect of different light activation and thermocycling methods on the shear bond strength (SBS) and on the adhesive remnant index (ARI) of metal brackets bonded to feldspathic ceramic. Hundred metal brackets were bonded to 20 porcelain cylinders, divided into four groups (n=25) based on light activation and thermocycling processes. The cylinders were etched with 10% hydrofluoric acid for 60 s and coated with two layers of silane. The brackets were bonded with Transbond XT composite resin. Light activation in Groups 1 and 3 was performed during 3 s using the VALO Ortho Cordless appliance with irradiance 3,200 mW/cm2 and in Groups 2 and 4 for 40 s using Optilight Max appliance with irradiance 1,200 mW/cm². The samples were stored in deionized water at 37°C for 24 h and the samples from Groups 1 and 2 were submitted to the SBS test at a rate of 1 mm/min, whereas the samples from Groups 3 and 4 were submitted to 7,000 thermal cycles (5°/55°C) before to the SBS test. The data were assessed by two-way analysis of variance and by Tukey’s test (a=0.05). No significant difference was observed between SBS means in the different light activation devices used. The samples subjected to thermocycling revealed lower SBS values (p≤0.05). There was predominance of score 0 for ARI in all groups. Therefore, the different light activation methods did not interfere in SBS, but thermocycling reduced SBS.


2017 ◽  
Vol 16 ◽  
pp. 1-7
Author(s):  
Bruna Lorena dos Santos Oliveira ◽  
Ana Rosa Costa ◽  
Américo Bortolazzo Correr ◽  
Marcus Vinicius Crepaldi ◽  
Lourenço Correr-Sobrinho ◽  
...  

Aim: To evaluate, in vitro, the effect of adhesive and bonding materials on the shear bond strength (SBS) of metallic brackets bonded to bovine teeth. Methods: Bovine teeth were embedded with acrylic resin, etched with 35% phosphoric acid for 20 s, rinsed, dried for 20 s and divided into 8 groups (n=20), according to the bonding materials and adhesive: Groups 1 and 5 – Transbond XT; Groups 2 and 6 – Fill Magic; Groups 3 and 7 – Biofix; and, Groups 4 and 8 – Orthocem. One layer of adhesive 3 M Unitek (Group 1), and one layer of Single Bond Universal Adhesive (Groups 2, 3 and 4) were applied and light-cured with LED for 10 s. Brackets were bonded to the buccal surface with four bonding materials and light-cured with LED for 40 s. SBS was carried out after 24 h and thermocycling (7,000 cycles - 5°/55 °C). Data were submitted to two way ANOVA and Tukey’s post hoc test (α=0.05). The Adhesive Remaining Index (ARI) was evaluated at 8×. Results: The adhesive was effective in increasing the SBS for all bonding materials (p<0.05). Significant difference (p<0.05) on the SBS was observed between bonding materials with or without adhesive. The ARI showed a predominance of scores 0 for all groups. Conclusions: The adhesive improved significantly the SBS of the brackets to teeth. Different SBS values occurred among the bonding materials. ARI index showed predominance of score 0 for all groups.


2011 ◽  
Vol 22 (3) ◽  
pp. 245-248 ◽  
Author(s):  
Paulo Roberto Amaral Gonçalves ◽  
Rafael Ratto de Moraes ◽  
Ana Rosa Costa ◽  
Américo Bortolazzo Correr ◽  
Paulo Roberto Aranha Nouer ◽  
...  

This study evaluated the bond strength of brackets to ceramic testing different etching times and light sources for photo-activation of the bonding agent. Cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 20 or 60 s. After application of silane on the ceramic surface, metallic brackets were bonded to the cylinders using Transbond XT (3M Unitek). The specimens for each etching time were assigned to 4 groups (n=15), according to the light source: XL2500 halogen light, UltraLume 5 LED, AccuCure 3000 argon laser, and Apollo 95E plasma arc. Light-activation was carried out with total exposure times of 40, 40, 20 and 12 s, respectively. Shear strength testing was carried out after 24 h. The adhesive remnant index (ARI) was evaluated under magnification. Data were subjected to two-way ANOVA and Tukey's test (α=0.05). Specimens etched for 20 s presented significantly lower bond strength (p<0.05) compared with those etched for 60 s. No significant differences (p>0.05) were detected among the light sources. The ARI showed a predominance of scores 0 in all groups, with an increase in scores 1, 2 and 3 for the 60 s time. In conclusion, only the etching time had significant influence on the bond strength of brackets to ceramic.


2020 ◽  
Vol 2020 ◽  
pp. 1-7
Author(s):  
Ruba M. Mustafa ◽  
Suhad J. Al-Nasrawi ◽  
Abtesam I. Aljdaimi

Biodentine is a calcium silicate cement (CSC) that has been broadly applied in vital pulp therapy. The quality of the Biodentine-composite bond has a significant effect on the longevity of the definitive restoration. The aim of this study is to investigate the shear bond strength (SBS) between Biodentine and composite restoration at different maturation times of Biodentine aged in artificial saliva. Fifteen Biodentine discs were allocated into three groups (n = 5) based on the timeframe of performance of composite restoration: immediate (after 12  min), after 14 days, and after 28 days of Biodentine maturation. Total etch and rinse adhesive system and bulk-fill regular resin composite were used. The shear bond strength and the failure pattern were assessed. One-way ANOVA with the Bonferroni post hoc test was applied for statistical analysis at p < 0.05 . The highest (32.47 ± 8.18 MPa) and the lowest (4.08 ± 0.81 MPa) SBS values were recorded for 14 days and 12 min groups, respectively. Significant statistical differences were reported among the groups, and a high statistically significant difference was found between the immediate group and the other groups. Adhesive failure patterns were evident in all groups. More clinically acceptable bond strength between the Biodentine and overlaid composite restoration is at 14 days after Biodentine maturation. Delaying the coverage of Biodentine later than 14 days may significantly reduce the SBS. Using the artificial saliva as an aging medium may affect the SBS between Biodentine and composite material.