scholarly journals A Review of Thiosulfate Leaching of Gold: Focus on Thiosulfate Consumption and Gold Recovery from Pregnant Solution

Metals ◽  
2017 ◽  
Vol 7 (6) ◽  
pp. 222 ◽  
Author(s):  
Bin Xu ◽  
Wenhao Kong ◽  
Qian Li ◽  
Yongbin Yang ◽  
Tao Jiang ◽  
...  
2018 ◽  
Vol 77 ◽  
pp. 195-202 ◽  
Author(s):  
Sanghee Jeon ◽  
Mayumi Ito ◽  
Carlito Baltazar Tabelin ◽  
Rongrit Pongsumrankul ◽  
Naho Kitajima ◽  
...  

Minerals ◽  
2021 ◽  
Vol 11 (9) ◽  
pp. 1021
Author(s):  
Sugyeong Lee ◽  
Charlotte E. Gibson ◽  
Ahmad Ghahreman

The use of alkaline pressure oxidation to pretreat refractory gold ore often results in insufficient gold recovery (<60%) in downstream thiosulfate leaching. To improve gold recovery, flotation was considered for the separation of carbonaceous matter (C-matter). In this study, the effect of MIBC on C-matter flotation was investigated to understand the role of the frother in bubble and froth formation and on flotation kinetics. MIBC dosages between 30 and 150 g/t were used in combination with 500 g/t of kerosene as a collector. The results showed that the recovery and selectivity of C-matter were improved with increasing MIBC dosages. Improved selectivity at higher MIBC dosages was attributed to faster C-matter recovery as bubble size decreased to the critical coalescence concentration (CCC) and to changes to the foam structure. Analysis of flotation kinetics showed that the flotation rate increased as the MIBC dosage increased due to the decreasing bubble size and the reduced induction time caused by the interaction between the collector and the frother. The results of this study explain the role of MIBC in C-matter flotation and can be used as a design basis for scavenger-cleaner flotation testing. Overall, the results show the potential for flotation as a means to improve gold recovery in thiosulfate leaching through the removal of C-matter.


2013 ◽  
Vol 734-737 ◽  
pp. 977-981 ◽  
Author(s):  
Qi Meng ◽  
Yi Qi Cui ◽  
Xiong Tong ◽  
Peng Dong ◽  
Kai Wang

The main recovery methods of gold from thiosulfate leaching solution are introduced, such as replacement precipitation, carbon adsorption, ionexchange resin adsorption, and solvent extraction. Research status of different process and their advantages/disadvantages are reviewed briefly. The research prospects on the methods are also given.


Toxics ◽  
2021 ◽  
Vol 9 (5) ◽  
pp. 111
Author(s):  
Maria Mihăilescu ◽  
Adina Negrea ◽  
Mihaela Ciopec ◽  
Petru Negrea ◽  
Narcis Duțeanu ◽  
...  

Gold is one of the precious metals with multiple uses, whose deposits are much smaller than the global production needs. Therefore, extracting maximum gold quantities from industrial diluted solutions is a must. Am-L-GA is a new material, obtained by an Amberlite XAD7-type commercial resin, functionalized through saturation with L-glutamic acid, whose adsorption capacity has been proved to be higher than those of other materials utilized for gold adsorption. In this context, this article presents the results of a factorial design experiment for optimizing the gold recovery from residual solutions resulting from the electronics industry using Am-L-GA. Firstly, the material was characterized using atomic force microscopy (AFM), to emphasize the material’s characteristics, essential for the adsorption quality. Then, the study showed that among the parameters taken into account in the analysis (pH, temperature, initial gold concentration, and contact time), the initial gold concentration in the solution plays a determinant role in the removal process and the contact time has a slightly positive effect, whereas the pH and temperature do not influence the adsorption capacity. The maximum adsorption capacity of 29.27 mg/L was obtained by optimizing the adsorption process, with the control factors having the following values: contact time ~106 min, initial Au(III) concentration of ~164 mg/L, pH = 4, and temperature of 25 °C. It is highlighted that the factorial design method is an excellent instrument to determine the effects of different factors influencing the adsorption process. The method can be applied for any adsorption process if it is necessary to reduce the number of experiments, to diminish the resources or time consumption, or for expanding the investigation domain above the experimental limits.


Author(s):  
Ivan Korolev ◽  
Kirsi Yliniemi ◽  
Mari Lindgren ◽  
Leena Carpén ◽  
Mari Lundström

AbstractRecently, an emerging electrodeposition-redox replacement (EDRR) method was demonstrated to provide exceptionally efficient gold recovery from cyanide-free hydrometallurgical solutions. However, the effect of electrode material and its corrosion resistance in this process was overlooked, even though the EDRR process is carried out in extremely corrosive, acidic chloride solution that also contains significant amounts of strong oxidants, i.e., cupric ions. In the current study, nickel alloy C-2000, stainless steels 316L and 654SMO, and grade 2 titanium were for the first time critically evaluated as potential cathode materials for EDRR. The particular emphasis was placed on better understanding of the effect of cathode substrate on the overall efficiency of the gold recovery process. The use of a multiple attribute decision-making method of material selection allowed reaching of a well-founded compromise between the corrosion properties of the electrodes and process efficiency of gold extraction. The 654SMO steel demonstrated outstanding performance among the examined materials, as it enabled gold recovery of 28.1 pct after 3000 EDRR cycles, while its corrosion rate (CR) was only 0.02 mm/year.


Sign in / Sign up

Export Citation Format

Share Document