Acoustic Emission Monitoring of Low Carbon Steel Corrosion inside and outside the Comparative Study

2013 ◽  
Vol 331 ◽  
pp. 246-249
Author(s):  
Wei Li ◽  
Shao Fan Wang ◽  
Xin Jia

This paper applied acoustic emission technology, monitoring low carbon steel uniform corrosion process, obtained low carbon steel corrosion acoustic emission signal in the process of uniform corrosion, And analyzed acoustic emission signal characteristics of the low carbon steel corrosion process applied the method combining characteristic parameters with wavelet packet transform, in the meantime combined the detection data of storage tank, Contrast acoustic emission signal characteristics of low carbon steel corrosion in experiment conditions and acoustic emission signal characteristics of storage tank corrosion in actual conditions, the result provides reference for acoustic emission research of low carbon steel uniform corrosion process and tanks online acoustic emission testing.

MRS Advances ◽  
2017 ◽  
Vol 2 (62) ◽  
pp. 3909-3915
Author(s):  
Héctor M. Barbosa Cásarez ◽  
Araceli Espinoza Vázquez ◽  
Francisco J. Rodríguez-Gomez

AbstractPhenylcoumarin glucoside (4-PC) is a compound extracted from the plant Hintona latiflora and was studied as inhibitor for AISI 1018 steel corrosion in 3% NaCl solution using potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) techniques, which may find application as eco-friendly corrosion inhibitors. The 4-PC provides inhibitor properties that protect AISI 1018 low carbon steel against corrosion at low concentrations (5 ppm) obtained by EIS. Polarization studies showed that the inhibitor was of mixed type. The inhibition efficiency by the two electrochemical techniques shows similar results. The inhibitor adsorption was demonstrated to be a combined process (physisorption and chemisorption) according to the Langmuir isotherm.


Author(s):  
Ya.G. Avdeev ◽  
◽  
A.V. Panova ◽  
T.E. Andreeva ◽  
Yu.I. Kuznetsov ◽  
...  

Corrosion of 08PS low-carbon steel was studied in a wide temperature range t = 25—100 °C in 1 M H2SO4 + 1 M H3PO4, 2 M H2SO4 и 2 M H3PO4, inhibited by the binary mixture IFKhAN-92 + KNCS (a molar ratio of components 9:1) and a three-component mixture IFKhAN-92 + KNCS + urotropine (9:1:400), in the presence of high concentrations of Fe(III) and Fe(II) salts, as well as in their joint presence. It is shown that under experimental conditions the corrosion inhibitors under study provide effective protection of steel in 1 M H2SO4 + 1 M H3PO4 even in the presence of Fe(III), Fe(II) salts or their mixtures. The highest protective effects are provided by a three-component inhibitor mixture. Under similar conditions in individual 2 M H3PO4 and, especially, 2 M H2SO4, the protective effects of inhibitors are lower. A stronger deceleration of steel corrosion by composite inhibitors based on IFKhAN-92 in H2SO4 + H3PO4 solutions containing Fe(III) salts in comparison with similar solutions of individual H2SO4, is largely due to the binding of Fe(III) cations by phosphate anions into complexes, that significantly reduces their chemical activity and, as a result the corrosion rate of steel.


2013 ◽  
Vol 373-375 ◽  
pp. 677-680
Author(s):  
Wei Li ◽  
Yu Li Gong ◽  
Yang Yu

Based on the characteristics of the acoustic emission (AE) signals from low carbon steel pitting corrosion, a new extraction method was proposed with wavelet transformation and independent component analysis. The experiment result shows that the new method can overcome the influence induced by the uncertainty of the independent source of low carbon steel pitting corrosion and good extraction result can be achieved.


2019 ◽  
Vol 3 (1) ◽  
pp. 263-276 ◽  
Author(s):  
Hameed B. Mahood ◽  
Asaad H. Sayer ◽  
Athraa H. Mekky ◽  
Anees A. Khadom

ROTOR ◽  
2017 ◽  
Vol 10 (1) ◽  
pp. 13
Author(s):  
Naufan Arviansyah ◽  
Sumarji Sumarji ◽  
Digdo Listyadi Setyawan

This research have a purpuse to know corrosion rate in pipe X52 and A53 at oil sludge media caused BS and W. Corrosion is a damage of metal that occurs because reaction between metal with environtment and produce unwanted of corrosion product. Pipe X52 and A53 is a type of low carbon steel that use for fluid transportation system in industry. Oil sludge is a sediment of crude oil from main gathering storage and containing variouses elements. Oil sludge have a one of element is Basic Sediment and Water that is can make corrosion happen to distribution pipes. Measuring Method used in this research is weight loss method. The result of corrosion rate in Oil Sludge media containing 30,17% BS and W for pipe A53 is 1,64 x 10-2 mmpy and the result for pipa X52 is 2,47 x 10-2 mmpy. The result of corrosion rate in Oil Sludge media containing 60,67% BS and W for pipe A53 is 2,12 x 10-2 mmpy and for pipe X52 the result is 3,13 x 10-2 mmpy. The result of this research showed pipe A53 have more resistance than pipe X52. The corrosion is classified as uniform corrosion. Keywords : A53, Weight Loss, Oil Sludge, X52.