Microstructure and Mechanical Properties of Low-Si Spring Steels Produced by Quenching- Isothermal-Quenching-Tempering Process

2014 ◽  
Vol 716-717 ◽  
pp. 74-78
Author(s):  
Fei Zhao ◽  
Huan Zhang ◽  
Yi Long Liang

An investigation of low Si spring steels (50CrVA) subjected to quenching-isothermal-quenching-tempering (Q-I-Q-T) process is presented. The results indicated that Q-I-Q-T process lead to the excellent mechanical properties compare to those treated by traditional heat-treatment, quenching and tempering, owing to the multiphase structure. The Q-I-Q-T treated microstructure consists of martensite, retained austensite, bainite and fine distributed carbides.

2013 ◽  
Vol 58 (1) ◽  
pp. 25-30 ◽  
Author(s):  
G. Golanski ◽  
J. Słania

The paper presents a research on the influence of multistage heat treatment with the assumed parameters of temperature and time on the microstructure and mechanical properties of high-chromium martensitic GX12CrMoVNbN9-1 (GP91) cast steel. In the as-cast state GP91 cast steel was characterized by a microstructure of lath martensite with numerous precipitations of carbides of the M23C6, M3C and NbC type, with its properties higher than the required minimum. Hardening of the examined cast steel contributes to obtaining a microstructure of partly auto-tempered martensite of very high strength properties and impact strength KV on the level of 9-15 J. Quenching and tempering with subsequent stress relief annealing of GP91 cast steel contributed to obtaining the microstructure of high-tempered lath martensite with numerous precipitations of the M23C6 and MX type of diverse size. The microstructure of GP91 cast steel received after heat treatment was characterized by strength properties (yield strength, tensile strength) higher than the required minimum and a very high impact energy KV. It has been proved that GP91 cast steel subject to heat treatment No. 2 as a result of two-time heating above the Ac3 temperature is characterized by the highest impact energy.


2013 ◽  
Vol 774-776 ◽  
pp. 1059-1067 ◽  
Author(s):  
Wichan Chuaiphan ◽  
Loeshpahn Srijaroenpramong ◽  
Dumrongrit Pinpradub

The effects of heat treatment on microstructure and mechanical properties of AISI 4140 for base cutter cane harvester were studied. The effect of heat treatment - i.e. the different quenching medium (water, oil and air mediums) and the different heat treatment condition (quenching, quenching+tempering, cover scrap cast iron+ quenching and cover scrap cast iron+ quenching+tempering) on the on microstructure and mechanical properties (hardness, impact toughness and bend test). The material AISI 4140 was purchased from local market in Thailand and an emission spectroscopy was applied to quantify the amount of elements in steel. The specimens were heat treated in an induction furnace. The resultant microstructure of materials AISI 4140 consists of martensite and retained austenite after quenching all mediums, which quenching in water it have more than in oil and air medium respectively. The microstructure of materials AISI 4140 after tempering process consists of bainitic structure (ferrite and epsilon carbide) and retained austenite, which tempering in water quenching condition it have more than in oil and air quenching condition respectively. The hardness, impact toughness and bended test are according to behavior heat transfer of quenching mediums. The material alloy steel grade AISI 4140 is the good candidates to promote the quenching in water ,oil and air medium and must be continuous to tempering process. The technique heating by cover scrape cast iron it was good for protected surface and decreased decarburization on surface of steels. But it is not necessary for control microstructure and mechanical properties.


Author(s):  
L. Malinov ◽  
V. Malinov ◽  
D. Burova

The relevance. Improving the mechanical properties of steels makes it possible to increase the service life of machine parts, which is an important task in materials science. One of the promising directions in its solution is to obtain in steel a multiphase structure, one of the main components of which is metastable austenite, which undergoes a dynamic deformation martensitic transformation (DDMT) - self-hardening effect under loading (SHL). Methods providing the required structure are isothermal and step quenching. However, at present, when they are carried out for cooling from the austenitizing temperature and holding at the constant temperature used non-environmentally friendly substances: heated oil, molten salts or alkalis. In this regard the actual problem is the exclusion of them from the technological process. The possibility of solving this problem on several steels has shown. Purpose is to show the possibility of increasing the mechanical properties of the studied steels 30ХГСА, 38ХС, 45Г, 40ХН, 10Г12, 60Х18 by using rational modes of an environmentally friendly method of steels quenching (isothermal - for low-alloyed and step - for high-alloyed) due to obtaining in their structure along with other components of metastable residual austenite and the implementation of the SHL effect. Research methods. Samples of the investigated steels after austenitization (in some cases with holding in IСIT) were cooled in water to the temperature of lower bainite formation (isothermal quenching) or stabilization of supercooled austenite to martensitic transformation upon cooling (step quenching), after which they were kept in a furnace and cooled in air to room temperature. Durometric, metallographic and X-ray research methods were used. The tensile properties and impact strength were determined. These properties were compared with those obtained for the studied steels after a typical heat treatment, including quenching in oil and tempering. Results. It is shown that isothermal and step quenching of the investigated steels without the use of non-environmentally friendly substances, carried out according to rational modes, makes it possible to increase the mechanical properties in comparison with their level after the commonly used quenching in oil (fire hazard, the vapors are cancerogenic) and tempering. This is achieved by obtaining a multiphase structure with metastable austenite. Scientific novelty. It is proposed to obtain a multiphase structure with metastable austenite in them to improve the mechanical properties of the studied steels by conducting isothermal and step quenching in an environmentally friendly way without using heated oil, molten salts or alkalis. Practical value. For the studied steels the modes of isothermal and step quenching are determined in an environmentally friendly way, which make it possible to increase the mechanical properties in comparison with the level achieved by quenching and tempering. Wherein in contrast to a similar typical quenching method are excluded the costs of purchasing salts or alkalis, their disposal and washing of products from them. Compared to quenching and tempering, the new method does not require the use of oil and tempering. The latter improves ecology and reduces energy consumption during heat treatment.


2015 ◽  
Vol 817 ◽  
pp. 472-478
Author(s):  
Jun Ru Li ◽  
Chen Gong ◽  
Le Yu Zhou ◽  
Lie Chen ◽  
Hui Zuo ◽  
...  

In this work, the effects of final heat treatment including quenching and tempering process on mechanical properties of 10Cr12Ni3Mo2VN steel were investigated by orthogonal experimental. It is shown that, the quenching process had a small effect on the strength properties. But the impact property obviously decreased with the increase of quenching temperature, that is due to the grain coarsening. It can be found that tempering temperature is the major factor which affects the mechanical properties. Tempering process had a large effect on the precipitation of carbides and that affected the strength, toughness and plastic greatly. The impact toughness had a minimum after tempered at 650°C between 600°C~700°C. The experimental results show that the M23C6 type carbides precipitated at the grain and martensite lath boundary were the main reason which decreased the impact toughness when tempering temperature increased from 600°C to 650°C.


2018 ◽  
Vol 18 (1) ◽  
pp. 125-135
Author(s):  
Sattar H A Alfatlawi

One of ways to improve properties of materials without changing the product shape toobtain the desired engineering applications is heating and cooling under effect of controlledsequence of heat treatment. The main aim of this study was to investigate the effect ofheating and cooling on the surface roughness, microstructure and some selected propertiessuch as the hardness and impact strength of Medium Carbon Steel which treated at differenttypes of heat treatment processes. Heat treatment achieved in this work was respectively,heating, quenching and tempering. The specimens were heated to 850°C and left for 45minutes inside the furnace as a holding time at that temperature, then quenching process wasperformed in four types of quenching media (still air, cold water (2°C), oil and polymersolution), respectively. Thereafter, the samples were tempered at 200°C, 400°C, and 600°Cwith one hour as a soaking time for each temperature, then were all cooled by still air. Whenthe heat treatment process was completed, the surface roughness, hardness, impact strengthand microstructure tests were performed. The results showed a change and clearimprovement of surface roughness, mechanical properties and microstructure afterquenching was achieved, as well as the change that took place due to the increasingtoughness and ductility by reducing of brittleness of samples.


2021 ◽  
Vol 64 ◽  
pp. 620-632
Author(s):  
Alexander Malikov ◽  
Anatoly Orishich ◽  
Igor Vitoshkin ◽  
Evgeniy Karpov ◽  
Alexei Ancharov