Electrical Properties BaTiO3 Thick Films with an Interlayer SrTiO3 Thin Films

2007 ◽  
Vol 124-126 ◽  
pp. 659-662
Author(s):  
Sung Pill Nam ◽  
Sung Gap Lee ◽  
Seong Gi Bae ◽  
Young Hie Lee

The BaTiO3/SrTiO3 heterolayered thick films were fabricated by two different methods – thick films of BaTiO3 by screen printing method on alumina substrates electrodes with Pt, thin films of SrTiO3 by the spin-coating method on BaTiO3 thick films and once more thick films of BaTiO3 by the screen printing method on SrTiO3 layer. The leakage current and the dielectric properties were investigated for effect of various stacking sequence of sol-gel-prepared SrTiO3 layer at interface of BaTiO3 thick films. The insertion of SrTiO3 interlayer yielded BaTiO3 thick films with homogeneous and dense grain structure with the number of SrTiO3 layers. The leakage current density of the BaTiO3/SrTiO3-7 film is less that 1.5 10-9 A/cm2 at 5 V.

2007 ◽  
Vol 124-126 ◽  
pp. 663-666 ◽  
Author(s):  
Sung Gap Lee ◽  
Sang Man Park ◽  
Young Jae Shim ◽  
Young Chul Rhee

PZT(70/30) powder was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The coating and drying procedure was repeated 4 times. And then the PZT(30/70) precusor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5 mol/L and the number of coating was varied from 0 to 6. The porosity decreased and the grain size increased with increasing the number of coatings. The thickness of the PZT-6(6: number of coatings) films was about 60~65μm. All PZT thick films showed the typical XRD patterns of a typical perovskite polycrystalline structure. The relative dielectric constant of the PZT-6 thick film was 540. The remanent polarization and coercive field of the PZT-6 film were 23.6 μC /cm2, 12.0 kV/cm, respectively.


2007 ◽  
Vol 336-338 ◽  
pp. 381-383
Author(s):  
Sung Gap Lee ◽  
Young Jae Shim ◽  
Cheol Jin Kim ◽  
Won Tae Bae ◽  
Kyu Hong Hwang ◽  
...  

Ferroelectric PZT heterolayered thick films were fabricated by the alkoxide-based sol-gel method. PZT(20/80) and PZT(80/20) paste were made and alternately screen-printed on the alumina substrates. The coating and drying procedure was repeated 4 times to form the heterolayered thick films. The thickness of the PZT heterolayered thick films was approximately 60 μm. All PZT thick films showed the typical XRD patterns of a perovskite polycrystalline structure. The relative dielectric constant and the dielectric loss of the PZT thick films sintered at 1050oC were 283 and 1.90%, respectively.


2007 ◽  
Vol 544-545 ◽  
pp. 633-636
Author(s):  
Sung Gap Lee ◽  
Sang Man Park

Ferroelectric Pb(Zr0.6Ti0.4)O3 (PZT(60/40)) powder was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The Pt bottom electrodes were screen-printed on the alumina substrate. The PZT(60/40) thick films were annealed at 1050°C for 10min in PbO atmosphere. Pb(Zr0.4Ti0.6)O3 (PZT(40/60)) precursor solution, which prepared by sol-gel method, was spin-coated on the PZT thick films to obtain a densification. These PZT multilayered thick films were annealed at 650°C for 2 h in PbO atmosphere. The upper electrodes were fabricated by screen printing the Ag paste and then firing at 590°C for 10min. Its structural and electrical properties of the PZT thick films with the treatment of PZT(40/60) precursor solution coating were investigated. The coating and drying procedure was repeated 4 times. And then the PZT(40/60) precursor solution was spin-coated on the multilayered thick films. A concentration of a coating solution was 1.5 mol/L and the number of coating was repeated from 0~15. The porosity of the thick films was decreased with increasing the number of coatings. All PZT multilayered thick films showed the XRD patterns of typical peroveskite polycrystalline structure. The relative dielectric constant of the PZT-15 (15: number of solution coatings) thick film were 370. And the PZT-15 thick film shows the remanent polarization of 23.5 μC/cm2 and coercive field of 18.0 kV/cm, respectively.


Author(s):  
Ibrahim Mohd Yazid ◽  
Muhammad Hazim Raselan ◽  
Shafinaz Sobihana Shariffudin ◽  
Puteri Sarah Mohamad Saad ◽  
Sukreen Hana ◽  
...  

2020 ◽  
Author(s):  
A. Amali Roselin ◽  
N. Anandhan ◽  
I. Joseph Paneer Doss ◽  
G. Gopu ◽  
K. P. Ganesan ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document