Co3O4/MCM-41 adsorbent with high surface area and more active sites was successfully prepared by ultrasonic assisted impregnation (UAI) technology and it has been found that the sulfur capacity was improved by 33.2% because of ultrasonication.


2014 ◽  
Vol 20 (1) ◽  
pp. 97-107 ◽  
Author(s):  
Mohammad Behnajady ◽  
Shahrzad Yavari ◽  
Nasser Modirshahla

In this work TiO2-P25 nanoparticles with high surface area have been used as adsorbent for the removal of C.I Acid Red 27 (AR27), as an organic contaminant from aqueous solution. Characteristics of phases and crystallite size of TiO2-P25 nanoparticles were achieved from XRD and the surface area and pore size distribution were obtained from BET and BJH techniques. TiO2-P25 nanoparticles with almost 80% anatase and 20% rutile phases, the average crystallite size of 18 nm, have specific surface area of 56.82 m2 g-1. The effect of various parameters like initial AR27 concentration, pH, contact time and adsorbent dosage has been carried out in order to find desired adsorption conditions. The desired pH for adsorption of AR27 onto TiO2-P25 nanoparticles was 3. The equilibrium data were analyzed with various 2-, 3- and 4-parameter isotherm models. Equilibrium data fitted very well by the 4-parameter Fritz-Schluender model. Results of adsorption kinetics study indicated that the pseudo-second order kinetics provided the best fit with correlation coefficients close to unity.


2003 ◽  
Vol 788 ◽  
Author(s):  
A. Akash ◽  
B. Nair ◽  
K. Minnick ◽  
M. Wilson ◽  
J. Hartvigsen

ABSTRACTA novel nano-ceramic material, called HSA-CERCANAM®, which has a very high surface area with a nanopore network has been developed. HSA-CERCANAM® can be casted in various shapes and forms resulting in a monolithic piece that has surface area as high as 80–100 m2/g. The surface area and the nanopore network of HSA-CERCANAM® remains stable at temperatures as high as 1000°C. Furthermore, the unique nature of HSA-CERCANAM® allows it to be casted on and around features, either sacrificial or permanent. Using sacrificial features, microchannels can be incorporated internally into the monolithic HSA-CERCANAM® piece in a simple, one-step process. Further, this monolithic ceramic component, which has an intrinsically high surface area and a nanopore network, can be infiltrated with a desired catalyst. This could offer clear technological advantages over currently available microreactors. The surface area, porosity, catalyst type and infiltration levels are some of the ways in which tailored microstructures can be realized in components such as mixers, heat exchangers, extractors, filters or reaction chambers thereby leading to highly efficient, multi-functional ceramic micro-devices.


NANO ◽  
2015 ◽  
Vol 10 (01) ◽  
pp. 1550005 ◽  
Author(s):  
Yaling Xie ◽  
Aidong Tang ◽  
Huaming Yang

Nanoporous materials Al -MCM-41 with varying Si / Al molar ratios have been successfully synthesized from natural clay mineral halloysite nanotubes (HNTs). Hydrothermal treatment of acid-pretreated HNTs and NaOH solution resulted in the one-step synthesis of final nanoporous products by using surfactant. The effects of Si / Al molar ratios (7.7, 61.0 and 176.5) on the surface area, porosity and degree of structural order of Al -MCM-41 materials have been investigated by X-ray diffraction (XRD), transmission electron microscopy (TEM), N 2 adsorption–desorption measurements and Fourier transform infrared (FTIR) spectra techniques. The results indicated that Si / Al molar ratio had important effect on the characteristics of nanoporous materials, and Al -MCM-41 with an intermediate Si / Al molar ratio of 61.0 exhibited excellent characteristics with high degree of order, high surface area (S BET ) of 1033 m2/g and pore volume of 0.92 mL/g.


2007 ◽  
Vol 19 (17) ◽  
pp. 4367-4372 ◽  
Author(s):  
Ajayan Vinu ◽  
Pavuluri Srinivasu ◽  
Dhanashri P. Sawant ◽  
Toshiyuki Mori ◽  
Katsuhiko Ariga ◽  
...  

1999 ◽  
Vol 15 (1) ◽  
pp. 79-90 ◽  
Author(s):  
Yasushi Takeuchi ◽  
Mitsuharu Hino ◽  
Yukihiro Yoshimura ◽  
Toshiro Otowa ◽  
Hisatsugu Izuhara ◽  
...  

2016 ◽  
Vol 852 ◽  
pp. 1349-1355
Author(s):  
Jia Yi Zhu ◽  
Xi Yang ◽  
Zhi Bing Fu ◽  
Chao Yang Wang ◽  
Wei Dong Wu ◽  
...  

The ultra-low density carbon aerogel, as low as 20 mg/cm3, was fabricated by pyrolysis of the organic aerogel formed by aqueous condensation of resorcinol and formaldehyde. Its surface area was as high as 1783 m2/g and it was used for investigation of electrochemical capacitive behaviours. The ultra-low density carbon aerogel displayed capacitive performance (110 F/g at 0.2 A/g) in 6 M KOH aqueous solution. Additionally, over 98% of the initial capacitance was retained after repeating the cyclic voltammetry test for 1000 cycles. The electrochemical performance might be attributed to the combination of three dimensional “opened” structure and high surface area of the carbon aerogel.