Preparation and characterization of La0.6Sr0.4Co0.2Fe0.8O3-δ thin-film membrane on porous support by dip-coating method

2011 ◽  
Vol 59 (3) ◽  
pp. 505-512
Author(s):  
Salwa Meredith Hashim ◽  
Abdul Rahman Mohamed ◽  
Subhash Bhatia
2006 ◽  
Vol 317-318 ◽  
pp. 807-810 ◽  
Author(s):  
Chang Yeoul Kim ◽  
Jin Wook Choi ◽  
Tae Yeoung Lim ◽  
Duck Kyun Choi

Electrochromic WO3 thin film was prepared by using tungsten metal solution in hydrogen peroxide as a starting solution and by sol-gel dip coating method. XRD pattern showed that tungsten oxide crystal phase formed at 400. In the view of electrochemical property, WO3 thin film which was heat-treated at 300 and was amorphous had better than that of the crystalline phase.


2007 ◽  
Vol 336-338 ◽  
pp. 585-588 ◽  
Author(s):  
Dao Qi Xue ◽  
Jun Ying Zhang ◽  
Hai Bing Feng ◽  
Tian Min Wang

ZnO:Eu3+ films were obtained by dip-coating method and influence of heat treatment on luminescent properties was investigated. Emission and excitation spectra revealed that the organic and nitrate molecules, which adhered on the surface of films when the samples were treated at lower temperatures (300oC-400oC), played an important role on the luminescent properties. At higher temperatures (500oC-800oC), the luminescence spectra of ZnO and Eu3+ were quite different with those treated at lower temperatures. Energy transferred from ZnO host to Eu3+ was obviously observed in the emission and excitation spectra. The luminescence mechanism was discussed briefly.


2019 ◽  
Vol 2 (3) ◽  
pp. 123
Author(s):  
Ervina Sandra Dewi ◽  
Siti Alaa ◽  
Dian Wijaya Kurniawidi ◽  
Susi Rahayu

A study has been conducted on the characterization of optical properties of thin films from lidah mertua (Sansevieria trifasciata) with dip coating method. The dip coating method was applied with different temperature and different time immersion treatments. The measuring variables in the manufacture of this thin film were tested based on the optical properties of their absorbance value of the extract and the thicknessof thin film. The absorbance spectral of extraction pigments were measured using UV-Vis in the wavelength range 350 nm to 700 nm. The results of the measurements showed that the extract of the S. trifasciata has high absorbance. Beside that, the minimum coating thickness is produced by a concentration of 12.5% with a 5 minute immersion time of 520 nm.


2002 ◽  
Vol 11 (02) ◽  
pp. 173-178
Author(s):  
SUDHIR KUMAR SHARMA ◽  
V. K. SHARMA ◽  
K. N. TRIPATHI

We report on our systematic and detailed study of fabrication and characterization of polyaniline (PA) prepared by vacuum deposition and polystyrene (PS) prepared by dip coating method thin film optical waveguides. The four-layer consisting of substrate (glass)/PA/PS/air has been used for demonstrating polarization filter action.


Author(s):  
Gözde Çelebi Efe ◽  
Elif Yenilmez ◽  
İbrahim Altinsoy ◽  
Serbülent Türk ◽  
Cuma Bindal

Langmuir ◽  
2014 ◽  
Vol 30 (30) ◽  
pp. 9028-9035 ◽  
Author(s):  
J. Dugay ◽  
R. P. Tan ◽  
A. Loubat ◽  
L.-M. Lacroix ◽  
J. Carrey ◽  
...  

2015 ◽  
Vol 1131 ◽  
pp. 237-241 ◽  
Author(s):  
Akkarat Wongkaew ◽  
Chanida Soontornkallapaki ◽  
Naritsara Amhae ◽  
Wichet Lamai

This work aims to study the effect of ZnO containing in TiO2/SiO2 film on the superhydrophilic property after exposed to different types of light. The metal solutions were prepared by sol-gel technique and the film was deposited on glass slides by dip coating method. The parameter studied was the amount of ZnO in the TiO2/SiO2 film. The contents of ZnO were 5-20% weight (increased by 5%). The amount of TiO2 was constant at 30% weight. The obtained films were analyzed for their roughness. The results indicated that film roughness changed according to the ZnO contents. With 5%ZnO in the thin film, the roughness was 0.726 nm while 20%ZnO obtained the roughness of 2.128 nm. UV-Vis spectrophotometer was used for measuring of transmittance of films. At wavelength of 550 nm, the transmittances of each film were greater than 90%. Band gap energy of each film was calculated from the transmittance data. It was found that the average band gap energy of the films was 2.47 eV. Then, the films contained various amount of ZnO were grouped into 2 sets. The first set was exposed to visible light while the other set was exposed to UV. The duration of exposure was 5 hr. Both sets of films after exposed to any light were kept in a black box controlled relative humidity of 85%. Each film was measured contact angle every day. It was found that the 30%TiO2/5%Zn/SiO2 film exposed to visible light showed the best superhydrophilic property. The contact angle was about 0-5° within 3 days. This may due to the reduction of band gap energy in the presence of ZnO in TiO2/SiO2 films to 2.41 eV and the roughness of the film.