Helium-bubble formation and void swelling in nimonic PE16 alloy under dual-ion (He+, Ni+) irradiation
1983 ◽
Vol 209-210
◽
pp. 381-386
◽
2019 ◽
Vol 467-468
◽
pp. 1134-1139
◽
2016 ◽
Vol 474
◽
pp. 65-75
◽
Helium bubble formation in ultrafine and nanocrystalline tungsten under different extreme conditions
2015 ◽
Vol 458
◽
pp. 216-223
◽
1984 ◽
Vol 120
(2-3)
◽
pp. 342-344
◽
2013 ◽
Vol 438
(1-3)
◽
pp. 178-182
◽
2011 ◽
Vol 417
(1-3)
◽
pp. 499-503
◽