Mechanical properties and deformation behavior of Ti–5Cr–xFe alloys

2009 ◽  
Vol 472 (1-2) ◽  
pp. 546-550 ◽  
Author(s):  
Wen-Fu Ho ◽  
Chang-Hung Pan ◽  
Shih-Ching Wu ◽  
Hsueh-Chuan Hsu
2018 ◽  
Vol 1 (1) ◽  
pp. 77-90
Author(s):  
Walaa Abdelaziem ◽  
Atef Hamada ◽  
Mohsen A. Hassan

Severe plastic deformation is an effective method for improving the mechanical properties of metallic alloys through promoting the grain structure. In the present work, simple cyclic extrusion compression technique (SCEC) has been developed for producing a fine structure of cast Al-1 wt. % Cu alloy and consequently enhancing the mechanical properties of the studied alloy. It was found that the grain structure was significantly reduced from 1500 µm to 100 µm after two passes of cyclic extrusion. The ultimate tensile strength and elongation to failure of the as-cast alloy were 110 MPa and 12 %, respectively. However, the corresponding mechanical properties of the two pass CEC deformed alloy are 275 MPa and 35%, respectively. These findings ensure that a significant improvement in the grain structure has been achieved. Also, cyclic extrusion deformation increased the surface hardness of the alloy by 49 % after two passes. FE-simulation model was adopted to simulate the deformation behavior of the material during the cyclic extrusion process using DEFORMTM-3D Ver11.0. The FE-results revealed that SCEC technique was able to impose severe plastic strains with the number of passes. The model was able to predict the damage, punch load, back pressure, and deformation behavior.


2008 ◽  
Vol 584-586 ◽  
pp. 182-187
Author(s):  
Lilia Kurmanaeva ◽  
Yulia Ivanisenko ◽  
J. Markmann ◽  
Ruslan Valiev ◽  
Hans Jorg Fecht

Investigations of mechanical properties of nanocrystalline (nc) materials are still in interest of materials science, because they offer wide application as structural materials thanks to their outstanding mechanical properties. NC materials demonstrate superior hardness and strength as compared with their coarse grained counterparts, but very often they possess a limited ductility or show low uniform elongation due to poor strain hardening ability. Here, we present the results of investigation of the microstructure and mechanical properties of nc Pd and Pd-x%Ag (x=20, 60) alloys. The initially coarse grained Pd-x% Ag samples were processed by high pressure torsion, which resulted in formation of homogenous ultrafine grain structure. The increase of Ag contents led to the decrease of the resulted grain size and change in deformation behavior, because of decreasing of stacking fault energy (SFE). The samples with larger Ag contents demonstrated the higher values of hardness, yield stress and ultimate stress. Remarkably the uniform elongation had also increased with increase of strength.


2010 ◽  
Vol 667-669 ◽  
pp. 253-258
Author(s):  
Wei Ping Hu ◽  
Si Yuan Zhang ◽  
Xiao Yu He ◽  
Zhen Yang Liu ◽  
Rolf Berghammer ◽  
...  

An aged Al-5Zn-1.6Mg alloy with fine η' precipitates was grain refined to ~100 nm grain size by severe plastic deformation (SPD). Microstructure evolution during SPD and mechanical behaviour after SPD of the alloy were characterized by electron microscopy and tensile, compression as well as nanoindentation tests. The influence of η' precipitates on microstructure and mechanical properties of ultrafine grained Al-Zn-Mg alloy is discussed with respect to their effect on dislocation configurations and deformation mechanisms during processing of the alloy.


2007 ◽  
Vol 539-543 ◽  
pp. 1701-1706
Author(s):  
Rong Shi Chen ◽  
Wei Neng Tang ◽  
Dao Kui Xu ◽  
En Hou Han

The effects of Y addition to the Mg-Zn-Y-Zr alloy on the change of the microstructure and the mechanical properties (with the Y content range of 1 to 3 wt%) have been investigated. It shows that when Zn content is constant (5.65wt%), the alloys with Y content between 1.17 and 1.72wt% nearly reach its highest strength. With the composition near the optimums, the extruded Mg-6%Zn-1%Y-Zr alloy shows high strength and excellent ductility. The deformation behavior of this new alloy at high temperature has also been studied. Moreover, the super-long fatigue behavior of the Mg-6%Zn-1%Y-Zr alloy has also been tested, the results show the alloy with a high fatigue strength of about 85-90MPa in the super-long fatigue life regime of 1×109 cycles.


2015 ◽  
Vol 640 ◽  
pp. 118-128 ◽  
Author(s):  
Yunchang Xin ◽  
Xiaojun Zhou ◽  
Yang Wu ◽  
Huihui Yu ◽  
Qing Liu

Sign in / Sign up

Export Citation Format

Share Document