SCC growth direction and SCC characteristics in Ni base weld metal (DNiCrFe-1J) in high temperature oxygenated water have been studied. The following results were obtained. (1) Strong direction dependence was observed in which SCC propagated preferentially along the growth direction of columnar crystals, (2) Conventional average SCC length which can be calculated from the equation in which SCC area is divided by the entire CT specimen thickness was about 1/2–3/4 times the average individual SCC length on individual columnar crystals. This was because SCC does not go through the entire thickness of the CT specimen. On the other hand, maximum SCC length was almost equal to the average individual SCC length produced on individual columnar crystals. Thus, the average individual SCC length and/or maximum SCC length were judged to be appropriate lengths for obtaining the SCC growth rate of Ni base weld metal (DNiCrFe-1J).


Alloy Digest ◽  
2002 ◽  
Vol 51 (5) ◽  

Abstract Nimrod 617KS is an Inconel-type consumable with a nominal composition of nickel, 24% Cr,12% Co, and 9% Mo and is used to join UNS N06617 and Nicrofer 6023 to themselves. The alloy is designed for high-temperature service and is often used as the weld metal in dissimilar cases to ensure the weld is as strong as the base metal. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating and joining. Filing Code: Ni-583. Producer or source: Metrode Products Ltd.


Sign in / Sign up

Export Citation Format

Share Document