scholarly journals Impact of inter-metallic compound thickness on thermo-mechanical reliability of solder joints in solar cell assembly

2021 ◽  
Vol 116 ◽  
pp. 114008
Author(s):  
Musa T. Zarmai ◽  
Chike F. Oduoza
2013 ◽  
Vol 2013 (0) ◽  
pp. _J211021-1-_J211021-3
Author(s):  
Takahiro NAMAZU ◽  
Kohei OHTANI ◽  
Masayuki FUJII ◽  
Shozo INOUE

2021 ◽  
Vol 11 (1) ◽  
Author(s):  
Jianguo Cui ◽  
Keke Zhang ◽  
Di Zhao ◽  
Yibo Pan

AbstractThrough ultrasonic wave assisted Sn2.5Ag0.7Cu0.1RExNi/Cu (x = 0, 0.05, 0.1) soldering test and − 40 to 125 °C thermal shock test, the microstructure and shear properties of Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints under thermal cycling were studied by the SEM, EDS and XRD. The results show that the Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints with high quality and high reliability can be obtained by ultrasonic assistance. When the ultrasonic vibration power is 88 W, the ultrasonic-assisted Sn2.5Ag0.7Cu0.1RE0.05Ni/Cu solder joints exhibits the optimized performance. During the thermal cycling process, the shear strength of ultrasonic-assisted Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints had a linear relationship with the thickness of interfacial intermetallic compound (IMC). Under the thermal cycling, the interfacial IMC layer of ultrasonic-assisted Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints consisted of (Cu,Ni)6Sn5 and Cu3Sn. The thickness of interfacial IMC of ultrasonic-assisted Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints was linearly related to the square root of equivalent time. The growth of interfacial IMC of ultrasonic-assisted Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints had an incubation period, and the growth of IMC was slow within 300 cycles. And after 300 cycles, the IMC grew rapidly, the granular IMC began to merge, and the thickness and roughness of IMC increased obviously, which led to a sharp decrease in the shear strength of the solder joints. The 0.05 wt% Ni could inhibit the excessive growth of IMC, improve the shear strength of solder joints and improve the reliability of solder joints. The fracture mechanism of ultrasonic-assisted Sn2.5Ag0.7Cu0.1RExNi/Cu solder joints changed from the ductile–brittle mixed fracture in the solder/IMC transition zone to the brittle fracture in the interfacial IMC.


RSC Advances ◽  
2020 ◽  
Vol 10 (66) ◽  
pp. 40215-40224
Author(s):  
Angela De Rose ◽  
Gabriele Mikolasch ◽  
Mathias Kamp ◽  
Achim Kraft ◽  
Mathias Nowottnick

High mechanical reliability of tin-based solder joints processed by joining copper and nickel-coated aluminium with short soldering times in ambient air.


2018 ◽  
Vol 47 (7) ◽  
pp. 4165-4169 ◽  
Author(s):  
Yong-Gue Sung ◽  
Woo-Ram Myung ◽  
Haksan Jeong ◽  
Min-Kwan Ko ◽  
Jeonghoon Moon ◽  
...  

2017 ◽  
Vol 2017 (1) ◽  
pp. 000641-000645
Author(s):  
Tim Jensen ◽  
Sunny Neoh ◽  
Adam Murling

Abstract The reliability of solder joints have been studied for many years. The selection of a solder for a particular application is often limited based on melting point requirements. This limits the number of options that are available for use. When alloy selection options are limited, people look to process changes to try and improve the reliability. Two such areas that have been identified that can impact reliability are bondline control and void reduction. This paper analyzes a new reinforced solder technology to maintain a consistent solder joint bondline. Experiments were also conducted to determine how best to design these preforms to minimize voiding.


Sign in / Sign up

Export Citation Format

Share Document