Effect of structure on second harmonic generation in molecularly doped poly(ethylene oxide)/ atactic -poly(methylmethacrylate) blends

Polymer ◽  
2001 ◽  
Vol 42 (11) ◽  
pp. 4837-4844 ◽  
Author(s):  
A.D. Grishina ◽  
L.Y.A. Pereshivko ◽  
T.V. Krivenko ◽  
V.V. Savel'ev ◽  
J. Vernel ◽  
...  
Author(s):  
C. E. Cluthe ◽  
G. G. Cocks

Aqueous solutions of a 1 weight-per cent poly (ethylene oxide) (PEO) were degassed under vacuum, transferred to a parallel plate viscometer under a nitrogen gas blanket, and exposed to Co60 gamma radiation. The Co60 source was rated at 4000 curies, and the dose ratewas 3.8x105 rads/hr. The poly (ethylene oxide) employed in the irradiations had an initial viscosity average molecular weight of 2.1 x 106.The solutions were gelled by a free radical reaction with dosages ranging from 5x104 rads to 4.8x106 rads.