scholarly journals Effects of silicon doping on low-friction and high-hardness diamond-like carbon coating via filtered cathodic vacuum arc deposition

2021 ◽  
Vol 11 (1) ◽  
Author(s):  
Jae-Il Kim ◽  
Young-Jun Jang ◽  
Jisoo Kim ◽  
Jongkuk Kim

AbstractIn this study, silicon (Si) was doped on a tetrahedral amorphous carbon (ta-C) coating and the tribological characteristics of the resulting Si-doped diamond-like carbon (DLC; a-C:Si:H) were investigated against a SUJ2 ball. The Si fraction in the coating was varied from 0 to ~ 20 at.% by increasing the trimethylsilane gas flow rate during filtered cathodic vacuum arc deposition. The coefficient of friction (CoF) showed no obvious change when the Si fraction was less than ~ 7 at.%. However, after Si doping, it significantly decreased when the Si fraction was greater than ~ 8 at.%. The running-in period also decreased to less than 1000 cycles after Si doping. The rapid formation of Si-rich debris and transfer layer led to the fabrication of a low-friction tribofilm, which was induced by the tribochemical reaction with moisture under ambient conditions. When the Si fraction was ~ 17 at.%, the lowest CoF of less than 0.05 was obtained. Further Si doping beyond the critical point led to the destruction of the film because of reduced hardness.

2014 ◽  
Vol 31 (2) ◽  
pp. 85-89 ◽  
Author(s):  
A. Wasy ◽  
G. Balakrishnan ◽  
S. Lee ◽  
J.-K. Kim ◽  
T. G. Kim ◽  
...  

2008 ◽  
Vol 47-50 ◽  
pp. 1415-1418
Author(s):  
Lan Xin Xu ◽  
Peng Li ◽  
Jin Wang ◽  
Yong Xiang Leng ◽  
Hong Sun ◽  
...  

In order to improve the abrasion property of polyoxymethylene (POM),diamond like carbon (DLC) film was deposited on POM substrate by the method of magnetic filtered cathodic vacuum arc deposition (MFCVAD). X-ray photoelectron spectroscopy (XPS) showed that the sp3 fraction decreased with the negative bias voltages increased. According to the result of the nano-indenter, the hardness of POM plates coated with DLC films was significantly harder than POM substrate. The results of ball-on-disc tribological testing demonstrated that the hardest DLC film had the lowest friction coefficient (0.11). The evaluation of in vitro platelet adhesion test indicates that the numbers of adhered and activated platelet on the DLC film deposited under the condition of 0V and 9min were remarkably decreased compared with that of the untreated POM.


Procedia CIRP ◽  
2020 ◽  
Vol 95 ◽  
pp. 999-1003
Author(s):  
Alexey Vereschaka ◽  
Marina Volosova ◽  
Nikolay Sitnikov ◽  
Nikolay Andreev ◽  
Filipp Milovich ◽  
...  

Vacuum ◽  
2013 ◽  
Vol 89 ◽  
pp. 220-224 ◽  
Author(s):  
Zhanyun Huang ◽  
Ping Luo ◽  
Wanzong Chen ◽  
Shirong Pan ◽  
Dihu Chen

2001 ◽  
Vol 398-399 ◽  
pp. 539-543 ◽  
Author(s):  
S.P Lau ◽  
Y.H Cheng ◽  
J.R Shi ◽  
P Cao ◽  
B.K Tay ◽  
...  

Sign in / Sign up